Thermal stability of intermetallic compounds at Sn-0.7Cu-10Bi-xNi/Co interface during reflows
Source abstract
Abstract
Abstract In this paper, thermal stability of Sn-0.7Cu-10B-xNi/Co (SCB-xNi/Co, x = 0.05, 0.10 and 0.15, in wt.%) interface during multiple reflows was investigated. Both (Ni,Co)Sn3 and (Cu,Ni)6Sn5 phases were formed at the SCB-xNi/Co interface after the initial reflow. With the increase of reflow number, the thermal stability of intermetallic compounds (IMCs) layer at high temperature was significantly different. The content of Ni atoms determined the thermal stability of IMCs layer in the interface reaction process. At the IMCs layer at the SCB-0.15Ni/Co interface, Ni atoms were enriched excessively, but they were present in a dispersive distribution at SCB-0.05Ni/Co and SCB-0.10Ni/Co interfaces. Ni atoms occupied sublattice sites of Co atoms in CoSn3 phase, which could improve the high-temperature stability of IMCs layer, so the IMCs layer had the strongest thermal stability at the SCB-0.15Ni/Co interface.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Metallurgical Processes and Thermodynamics · Silicon and Solar Cell Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. Ma · Nat. Commun. · 2017 · 8 · 191610.1038/s41467-017-01727-6 ↗
2. Gao · Mater. Lett. · 2019 · 252 · 9210.1016/j.matlet.2019.05.100 ↗
3. Gao · J. Qi. Mater. Des. · 2019 · 174
4. Zhao · Mater. Lett. · 2017 · 186 · 28310.1016/j.matlet.2016.10.017 ↗
5. Ma · J. Alloys Compd. · 2017 · 706 · 59610.1016/j.jallcom.2017.02.243 ↗
6. Wang · J. Alloys Compd. · 2015 · 619 · 47410.1016/j.jallcom.2014.09.017 ↗
7. Laurila · Mater. Sci. Eng. R · 2006 · 37 · 1
8. Gao · J. Mater. Sci. Mater. Electron. · 2019 · 30 · 218610.1007/s10854-018-0490-2 ↗
9. Li · Acta Mater. · 2006 · 54 · 290710.1016/j.actamat.2006.02.030 ↗
10. Kogtenkova · Phys. Solid State · 2016 · 58 · 74210.1134/S1063783416040107 ↗
11. Straumal · Mater. Sci. Forum · 1999 · 294–296 · 411
12. Wang · Mater. Chem. Phys. · 2011 · 130 · 65110.1016/j.matchemphys.2011.07.042 ↗
13. Huang · J. Electron. Mater. · 2010 · 39 · 240310.1007/s11664-010-1346-6 ↗
14. Gao · Mater. Lett. · 2008 · 62 · 225710.1016/j.matlet.2007.11.060 ↗