Grain refinement in Fe-rich FeSiB(P)NbCu nanocomposite alloys through P compositional modulation
Source abstract
Abstract
Abstract The progressive addition of P in Fe-rich FeSiB(P)NbCu nanocomposite alloy leads to grain refinement of α-Fe nanocrystals i.e, dense nucleation and grain growth inhibition. The P addition leads to linear reduction of α-Fe nanocrystallite size (D) and increases nucleation density (Nd) from ~ 30 nm and 2.5 × 1022 (0 at% P) to ~ 15 nm and 0.9 × 1023 for (8 at% P). The refined microstructure leads to coercivity reduction from 74 A/m (0 at% P) to 9.4 A/m (8 at% P), in agreement with Random-Anisotropy Model. The P assisted synergistic grain refinement mechanism is explained in the context of crystallization activation energy, selective solute re-distribution and enhanced stabilization of intergranular amorphous matrix. The 4 at% P alloy shows optimal soft-magnetic properties of 10.2 A/m and 1.64 T.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · Microstructure and mechanical properties · Magnetic properties of thin films
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. Modern soft magnets: Amorphous and nanocrystalline materials10.1016/j.actamat.2012.10.040 ↗
2. Effect of intergranular magnetic coupling on soft magnetic and magnetotransport properties in nanocrystalline materials10.1016/S1359-6462(02)00442-6 ↗
3. Composition design for Fe-based soft magnetic amorphous and nanocrystalline alloys with high Fe content10.1016/j.matdes.2020.108511 ↗
4. New Fe-metalloids based nanocrystalline alloys with high Bs of 1.9 T and excellent magnetic softness10.1063/1.3058624 ↗
5. The effect of introduction of carbon on the glass forming ability and magnetic properties of melt-spun FeSiBCuC alloys10.1016/j.jnoncrysol.2016.06.011 ↗
6. Nb-poor Fe-Nb-B nanocrystalline soft magnetic alloys with small amount of P and Cu prepared by melt-spinning in air10.1016/S1359-6462(02)00612-7 ↗
7. Relaxation studies of amorphous alloys with creep induced magnetic and structural anisotropy10.1016/j.scriptamat.2012.07.025 ↗
8. Effect of heating rate during primary crystallization on soft magnetic properties of melt-spun Fe-B alloys10.1016/j.scriptamat.2017.01.030 ↗
9. Competition driven nanocrystallization in high B s and low coreloss FeSiBPCu soft magnetic alloys10.1016/j.scriptamat.2014.08.023 ↗
10. Effect of Cu and P on the Crystallization Behavior of Fe-Rich Hetero-Amorphous FeSiB Alloy10.2320/matertrans.M2009206 ↗
11. Role of P on amorphization, microstructure, thermo-physical and soft magnetic properties of Fe-rich FeB(P)SiNbCu melt-spun alloys10.1016/j.jmmm.2019.165723 ↗
12. Crystallisation kinetics and microstructure development in metallic systems10.1016/S0079-6425(00)00021-9 ↗
13. Crystallization and magnetic hardening behaviour of Fe-rich FeSiBNb(Cu) melt-spun alloys10.1016/j.jmmm.2020.166528 ↗
14. Grain refinement mechanism of soft-magnetic alloys with nanocrystals embedded in amorphous matrix10.1016/j.jmrt.2020.01.093 ↗