Microstructural evolution resulting from different deformation mechanisms of a high-Nb-containing TiAl alloy with harmonic structure during elevated-temperature deformation
Source abstract
Abstract
Abstract A Ti-42.5Al-8Nb-0.2W-0.2B-0.1Y (at%) alloy with a harmonic structure was deformed via compression (temperature: 950 °C–1050 °C, strain rate: 10−2 s−1–10−4 s−1) and the resulting microstructure was characterized. The results revealed that at certain temperatures and strain rates the alloy undergoes compression deformation via intragranular deformation. However, with increasing temperatures and decreasing strain rates, this mechanism changed to grain boundary sliding (GBS) of β/B2 grains and γ grains in the enlarged shell area and the accommodated intragranular deformation of γ grains in the core area.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Titanium Alloys Microstructure and Properties · High-Velocity Impact and Material Behavior
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (11)
Show source-provided references
1. Imayev · Scr. Mater. · 1999 · 40 · 18310.1016/S1359-6462(98)00419-9 ↗
2. Niu · J. Alloys Compd. · 2012 · 543 · 1910.1016/j.jallcom.2012.07.127 ↗
3. Cheng · Mater. Lett. · 2017 · 194 · 5810.1016/j.matlet.2017.01.127 ↗
4. Chu · Mater. Sci. Eng. A · 2018 · 725 · 46610.1016/j.msea.2018.04.055 ↗
5. Cheng · J. Alloys Compd. · 2017 · 693 · 74910.1016/j.jallcom.2016.09.170 ↗
6. Vajpai · Mater. Trans. · 2016 · 57 · 142410.2320/matertrans.MH201509 ↗
7. Wang · Mater. Sci. Eng. A · 2011 · 528 · 675410.1016/j.msea.2011.05.071 ↗
8. Wang · Mater. Sci. Eng. A · 2008 · 486 · 32110.1016/j.msea.2007.09.008 ↗
9. Chu · Metals · 2018 · 8 · 91610.3390/met8110916 ↗
10. Zherebtsov · Acta Mater. · 2016 · 121 · 15210.1016/j.actamat.2016.09.003 ↗
11. Straumal · Scr. Mater. · 2014 · 70 · 5910.1016/j.scriptamat.2013.09.019 ↗