journal article·2024-12

Cryogenic fracture toughness of high manganese steel joint and 7 %Ni steel joint welded with nickel-based filler metal

Xiaotao Cai, Yanchang Qi, Haiyang Zhu, Liu Yao, Jinshan Wei, Chengyong Ma, Qilu Ge

Materials Letters· Volume 377
Publisher page

Abstract

The high manganese steel (HMS) joint and 7%Ni steel joint were fabricated using ENiCrMo-6 nickel-based electrodes. The cryogenic fracture toughness of both joints was investigated by Crack Tip Opening Displacement (CTOD) tests at 77K. The results showed that the fracture toughness of both joints satisfied DNV requirements of 0.15mm. The CTOD values of weld metal (WM) and heat affected zone (HAZ) in HMS joint were approximately 36.5% and 33.5% lower than those of corresponding areas in 7%Ni steel joint, respectively. In the HMS joint, the presence of more large-sized precipitates in WM and segregations in HAZ had negative effects on the fracture toughness. Compared to other test locations, the HAZ of 7%Ni steel joint contained local hard-brittle zones, resulting in more discrete CTOD values.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Fatigue and fracture mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (11)

Show source-provided references
1. Improvement of cryogenic toughness for 9% Ni steel keyhole TIG butt-welded joints with a Ni interlayer10.1016/j.msea.2022.142661 ↗
2. Investigation of fatigue and fracture characteristics for low-temperature metals considering the effects of various alloying components10.1007/s40194-020-00947-7 ↗
3. Mechanical properties of cryogenic high manganese steel joints filled with nickel-based materials by SMAW and SAW10.1016/j.matlet.2021.130596 ↗
4. Effect of Si content on microstructure and cryogenic toughness of heat affected zone of low nickel steel10.1016/j.msea.2019.138621 ↗
5. Effect of microstructure synergism on cryogenic toughness for CGHAZ of low-carbon martensitic steel containing nickel10.1016/j.msea.2021.142240 ↗
6. Investigation of fatigue performance of low temperature alloys for liquefied natural gas storage tanks10.1177/0954406215569255 ↗
7. Cryogenic fracture toughness of 9%Ni steel flux cored arc welds10.1016/j.jmatprotec.2017.10.026 ↗
8. The influence of microstructure evolution in thick 9late 9%Ni steel submerged arc welding joint on fracture toughness properties
9. Grain boundary wetting transition in the Mg-based ZEK 100 alloy10.3390/cryst13111538 ↗
10. Microstructural effects on J-integral fracture toughness of welded high-Mn steels at 298 and 77 K10.1002/srin.202200259 ↗
11. Effect of morphologies of martensite-austenite constituents on impact toughness in intercritically reheated coarse-grained heat-affected zone of HSLA steel10.1016/j.msea.2017.10.079 ↗