Abstract
Abstract Fused silica surface machined using continuous-wave CO2 laser beams with an energy density of 0.5 J/mm2 presented U-shaped grooves (approximately 47 μm-deep and 250 μm-wide) and asymmetrical craters (2–5 μm high). The fully reacted valley in the groove center exhibited porous microstructures and agglomerated silica nanoparticles in the size of 33–118 nm; whereas, the less reacted peak in the groove edge only presented uneven solidified films from silica ablations. Distinct morphologies in the valley and peak areas were supposed to result from the Gaussian energy distribution of laser beams. The selected area electron diffraction pattern suggested that the laser-reacted silica nanostructures were still amorphous with no obvious composition change. The x-ray photoelectron spectrometric results showed that both Si 2p and O 1s peaks shifted to higher energy sides, implying a more oxidized state of Si4+ and absorbed oxygen or hydroxides on nanostructured silica after CO2 laser machining.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Laser Material Processing Techniques · Diamond and Carbon-based Materials Research · Laser-Ablation Synthesis of Nanoparticles
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (9)
Show source-provided references
1. Removal of scratches on fused silica optics by using a CO2 laser10.1364/OE.21.028272 ↗
2. Laser recrystallization and inscription of compositional microstructures in crystalline SiGe-core fibres10.1038/ncomms13265 ↗
3. Morphological changes in ultrafast laser ablation plumes with varying spot size10.1364/OE.23.015608 ↗
4. M.A. Norton, J.J. Adams, C.W. Carr, E.E. Donohue, M.D. Feit, R.P. Hackel, W.G. Hollingsworth, J.A. Jarboe, M.J. Matthews, A.M. Rubenchik, M.L. Spaeth, 2007, Growth of laser damage in fused silica: diameter to depth ratio, Proc. SPIE 6720, Laser-Induced Damage in Optical Materials: 2007, 67200H. https://doi.org/10.1117/12.748441.10.1117/12.748441 ↗
5. Scan speed and fluence effects in femtosecond laser induced micro/nano-structures on the surface of fused silica10.1016/j.jnoncrysol.2018.04.018 ↗
6. Evaluation of the fused silica thermal conductivity by comparing infrared thermometry measurements with two-dimensional simulations10.1063/1.4764904 ↗
7. Wetting of grain boundaries in hard-magnetic Nd-Fe-B alloys10.3103/S106782121206003X ↗
8. Size dependence of Si 2p core-level shift at Si nanocrystal/SiO2 interfaces10.1063/1.2776014 ↗
9. Periodic silver nanocluster arrays over large-area silica nanosphere template as highly sensitive SERS substrate10.1016/j.apsusc.2017.12.157 ↗