journal article·2021-07

Effect of chrome on the magnetic and structural properties of Mn57-xAl43Crx (x = 0.51, 0.91, 1.51) and Mn53.3-XAl45C1.7Crx (x = 0.0, 0.5, 1.0, 1.5, 2.0, 2.5) alloy systems

Marisela Benitez, J. Sebastián Trujillo, German A. Pérez Alcázar

Materials Letters· Volume 295
Publisher page

Abstract

Abstract The effect of Cr doping, in melted and heat treated (HT) at different temperatures of Mn57-xAl43Crx with x = 0.51, 0.91, 1.51 and Mn53.3-xAl45C1.7Crx with x = 0.0, 0.5, 1.0, 1.5, 2.0, 2.5 alloys were studied. In samples with C and Cr (0 and 1.0 at.%) a paramagnetic epsilon phase (e), and ferromagnetic tau phase (τ), with hard magnetic behavior, with coercive field Hc of 2.67 and 2.32 kOe, saturation magnetization Ms of 68 and 66 emu/g, remanent magnetization Mr of 39.6 and 33.6 emu/g, and product (BH)max of 0.91 and 0.69 MGOe, respectively, were observed. But for samples doped with Cr ≠ 1.0 at.% the metastable τ-phase partially decomposes into gamma (γ2) and beta (β) phases. The samples have particle sizes between 108 and 127 µm.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic Properties of Alloys · Metallic Glasses and Amorphous Alloys · Magnetic Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (11)

Show source-provided references
1. New permanent magnets; manganese compounds10.1088/0953-8984/26/6/064211 ↗
2. Influence of processing on structure property correlations in τ-MnAl rare-earth free permanent magnet material10.1016/j.jallcom.2015.02.041 ↗
3. Rapid quenching and properties of hard magnetic materials in MnAl-X (x= Ti, Cu, Ni, C,) systems10.1007/BF00544507 ↗
4. An overview of MnAl permanent magnets with a study on their potential in electrical machines10.3390/en13215549 ↗
5. L10 rare-earth-free permanent magnets: The effects of twinning versus dislocations in Mn-Al magnets10.1103/PhysRevMaterials.4.094402 ↗
6. Twin-like defects in L10 ordered τ-MnAl-C studied by EBSD10.1016/j.actamat.2015.08.044 ↗
7. Preparation of nanocrystalline Mn-Al-C magnets by melt spinning and subsequent heat treatments10.1016/j.jallcom.2006.08.313 ↗
8. Phase transitions and hard magnetic properties for rapidly solidified MnAl alloys doped with C, B, and rare earth elements10.1007/s10853-011-6049-8 ↗
9. Atomic and ionic radii of elements 1–9610.1002/chem.201602949 ↗
10. Rapid quenching and properties of hard magnetic materials in MnAI-X (X = Ti, Cu, Ni, C, B) systems10.1007/BF00544507 ↗
11. Magnetism-structure correlations during the ε→τ transformation in rapidly-solidified MnAl nanostructured alloys10.3390/met4010008 ↗