Abstract
Slow strain rate tests have been used to evaluate the effect of heat treatment on the susceptibility to stress corrosion cracking (SCC) of type AISI 403 martensitic stainless steel in 20% NaCl at 95°C. Heat-treated specimens included water quenched, quenched and tempered at 200°C, 400°C and 600°C, respectively, and annealed at 850°C. When tested in an inert environment, the lowest elongation to failure and percentage reduction in area was shown by the quenched specimen, and the highest by the annealed specimen, and between these two specimens, there were the specimens tempered at 200°C, 400°C and 600°C, respectively. When tested in 20% NaCl (wt.%), pH 7, without exception, all the specimens were embrittled by the environment, showing, at least, 50% of the elongation exhibited in the inert environment, indicating a cracking-induced environmentally. The fracture morphology presented completely intergranular cracks along the prior austenite for the quenched specimen to completely transgranular cracking for the annealed specimen. The percentage of intergranular cracks decreased as the tempering temperature increased from 200°C to 600°C. The fracture mechanism is thought to occur in terms of a hydrogen embrittlement.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · High Temperature Alloys and Creep · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. Experience with stress corrosion cracking in large steam turbines
2. Stress corrosion cracking in turbine-generators
3. The effect of turbine steam impurities on caustic stress corrosion cracking of NiCrMoV steels
4. Stress corrosion cracking and corrosion fatigue of martensitic, ferritic and ferritic–austenitic (duplex) stainless steels
5. El-Sayed · Surf. Technol. · 1981 · 16 · 24510.1016/0376-4583(81)90087-X ↗
6. Gouda · Surf. Technol. · 1983 · 18 · 32710.1016/0376-4583(83)90123-1 ↗
7. El-Sayed · Corros. Prev. Control · 1986 · 12 · 142
8. de Santa-Maria · Corros. Sci. · 1989 · 29 · 6910.1016/0010-938X(89)90081-4 ↗
9. Maier · Corrosion · 1980 · 36 · 6010.5006/0010-9312-36.2.60 ↗
10. Stress corrosion cracking and hydrogen embrittlement of iron base alloys
11. Knutsen · Corrosion · 1991 · 47 · 35910.5006/1.3585266 ↗
12. Pourbaix · 1966
13. Wilde · Corrosion · 1971 · 27 · 32610.5006/0010-9312-27.8.326 ↗
14. Doig · Met. Trans. · 1982 · 13A · 91310.1007/BF02642406 ↗