Preparation of alumina–high zirconia microcomposite by combined gel-precipitation
Source abstract
Abstract
Abstract Microcomposites of alumina and zirconia containing equal volume fractions of the two are prepared by a combined gel-precipitation route using aluminium chloride and zirconium oxychloride as precursors. Dried gel powders calcined between 375 and 800 °C show cubic phase as the only crystalline phase. Zirconia gets converted to tetragonal phase above 900 °C and is retained mostly in this form upto 1000 °C. At the higher temperatures, it converts to the monoclinic phase. Alumina starts to crystallize into δ-form at 900 °C and is converted to α-form at 1250 °C. Pressed pellets sintered at 1400 °C achieve densities close to theoretical in 4 h. Microstructures show evidence of segregation and coarsening in a composite matrix of alumina and zirconia mixed at a submicron level.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Nuclear materials and radiation effects · Ferroelectric and Piezoelectric Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (9)
Show source-provided references
1. Claussen · J. Am. Ceram. Soc. · 1976 · 59 · 4910.1111/j.1151-2916.1976.tb09386.x ↗
2. Yuan · J. Am. Ceram. Soc. · 1990 · 75 · 257610.1111/j.1151-2916.1992.tb05614.x ↗
3. Matsumoto · J. Am. Ceram. Soc. · 1993 · 76 · 267710.1111/j.1151-2916.1993.tb04000.x ↗
4. Sproson · J. Am. Ceram. Soc. · 1984 · 67 · C-9210.1111/j.1151-2916.1984.tb19523.x ↗
5. Balmer · J. Am. Ceram Soc. · 1995 · 78 · 48910.1111/j.1151-2916.1995.tb08842.x ↗
6. Smyser · Ceram. Eng. Sci. Proc. · 1997 · 18 · 20510.1002/9780470294437.ch22 ↗
7. Singh · Mater. Lett. · 1994 · 18 · 20110.1016/0167-577X(94)90231-3 ↗
8. Singh · Mater. Lett. · 1997 · 31 · 28110.1016/S0167-577X(96)00286-8 ↗
9. V. K. Singh, PhD thesis, Department of Ceramic Engineering, IT, Banaras Hindu University, India.