Abstract The diffusion bonding of a Ni 3 Al intermetallic alloy to an austenitic stainless steel has been carried out at temperatures 950, 1000 and 1050 °C. The influence of bonding temperature on the microstructural development and hardness across the joint region has been determined. The microvoids in the interface have been found to decrease with increasing bonding temperature. The intermetallic phase Al 3 Ni has been detected at the Ni 3 Al side of the diffusion couple. Diffusion of Cr and Fe from the stainless steel to the Ni 3 Al alloy has been observed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Advanced Welding Techniques Analysis · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. Diffusion welding and brazing
2. Fundamentals of diffusion bonding
3. Diffusion bonding between Ti-6Al-4V alloy and ferritic stainless steel10.1016/j.matlet.2006.07.123 ↗
4. Phase relation and microstructure in multi-phase intermetallic alloys based on Ni3Al–Ni3Ti–Ni3V pseudo-ternary alloy system10.1016/j.intermet.2003.12.011 ↗
5. Interfacial chemical stability during diffusion bonding of Al2O3-fibres with Ni3Al- and NiAl-matrices10.1016/1359-6454(95)00337-1 ↗
6. Thermal stability of an Al/Ni3Al composite processed by powder metallurgy10.1016/S0966-9795(97)00027-7 ↗
7. Fracture mechanism of Ni3Al alloys and their composites with ceramic particles at elevated temperatures10.1016/S0966-9795(99)00095-3 ↗
8. Some observations on the high temperature oxidation behaviour of plasma sprayed Ni3Al coatings
9. A study of Ni3Al coating on carbon steel surface via the SHS casting route10.1016/S0257-8972(98)00820-2 ↗
10. Evaluation of the corrosion behaviour of plasma-sprayed Ni3Al coatings on steel in oxidation and molten salt environments at 900°C10.1016/S0257-8972(02)00772-7 ↗
11. Cavitation erosion resistance of AISI 420 martensitic stainless steel laser-clad with nickel aluminide intermetallic composites and matrix composites with TiC reinforcement10.1016/j.surfcoat.2006.01.054 ↗
12. Liquid impact erosion characteristics of martensitic stainless steel laser clad with Ni-based intermetallic composites and matrix composites10.1016/j.wear.2006.03.024 ↗
13. A study on the solid-state welding of boron-doped Ni3Al–AISI 304 stainless steel couple10.1016/j.matlet.2004.08.042 ↗
14. Processing, properties and applications of nickel and iron aluminides10.1016/S0079-6425(97)00014-5 ↗
15. Interface structure of diffusion bonded duplex stainless steel and medium carbon steel couple10.1016/j.matchar.2009.04.011 ↗
16. Trethewey · 1995
17. Interfacial reaction of infrared brazed NiAl/Al/NiAl and Ni3Al/Al/Ni3Al joints10.1016/S0966-9795(01)00011-5 ↗
18. Effect of heat treatments at 520°C on an aluminium alloy matrix composite reinforced with Ni3Al powder particles10.1016/j.scriptamat.2005.12.052 ↗