Y 2 O 3 :Bi 3+ thin films prepared by radio frequency magnetron sputtering: Structural and optical studies
Source abstract
Abstract
Abstract Y2O3:Bi3+ thin films of various microstructures were deposited using different deposition times by means of a radio frequency magnetron sputtering system. The deposition time affects the surface morphology, crystalline phase and the optical properties of the Y2O3:Bi3+ thin films. The films with the shorter and longer deposition time were amorphous and cubic in structure, respectively. The Bi3+ ions in the cubic structure emitted in the broad blue band centered at 410 nm, while the amorphous structure also emitted in the green region.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Luminescence Properties of Advanced Materials · Ga2O3 and related materials · Glass properties and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (11)
Show source-provided references
1. Metal-ion doped luminescent thin films for optoelectronic applications10.1039/c3tc31024h ↗
2. Structural and photoluminescence characters of SnO2: Sb films deposited by RF magnetron sputtering10.1016/j.jlumin.2004.12.003 ↗
3. Investigation of CaTiO3:Pr3+ thin films deposited by radio frequency reactive magnetron sputtering for electroluminescence application
4. Thin film RF magnetron sputtering of gadolinium-doped yttrium aluminum garnet ultraviolet emitting materials10.1016/j.optmat.2005.08.024 ↗
5. Comparison of Y2O3:Bi3+ phosphor thin films fabricated by the spin coating and radio frequency magnetron techniques10.1016/j.physb.2016.06.007 ↗
6. A new high temperature modification of face-centered cubic Y2O310.1017/S0885715600017760 ↗
7. K. Brandenburg, DIAMOND-2.0 Visual Crystal Structure Information System, Crystal Impact Distribution, Bonn, Germany, 1998.
8. Refinement of the Y2O3 structure at 77 K10.1107/S0567740880011351 ↗
9. The effect of different annealing temperatures on the structure and luminescence properties of Y2O3:Bi3+ thin film fabricated by RF magnetron sputtering10.1016/j.apsusc.2017.01.001 ↗
10. Effect of deposition time on structural, electrical, and optical properties of SnS thin films deposited by chemical bath deposition10.1016/j.apsusc.2010.07.104 ↗
11. Conversion of Y3(Al, Ga)5O12:Tb3+ to Y2Si2O7: Tb3+ thin film by annealing at higher temperatures10.1016/j.apsusc.2013.01.025 ↗