Role of interfacial microstructure on mechanical properties of cold metal transfer welded dissimilar A6061-T6 and A6082-T6 joints
Source abstract
Abstract
Abstract A6061-T6 and A6082-T6 dissimilar aluminium alloys are welded using CMT (Cold metal transfer) process and the interface microstructure of the individual alloys is correlated with mechanical properties. Microstructures indicate that dendrites next to the PMZ (Partially melted zone) of A6082-T6 side are finer than the dendrites next to the PMZ of A6061-T6 side. Liquation at grain boundaries and within the grains is clearly visible in the PMZ of A6061-T6 interface, whereas the PMZ of A6082-T6 interface does not reveal liquation phenomenon at grain boundaries and grain interiors. Among the interface regions, the A6082-T6 side shows superior mechanical properties as compared to the A6061-T6 side.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Welding Techniques Analysis · Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (12)
Show source-provided references
1. Materia ls and Design Welding of aluminum alloy to zinc coated steel by cold metal transfer10.1016/j.matdes.2013.01.045 ↗
2. Aluminium in Innovative Light-Weight Car Design10.2320/matertrans.L-MZ201132 ↗
3. Cold metal transfer welding – brazing of pure titanium TA2 to magnesium alloy AZ31B10.1016/j.jallcom.2014.03.051 ↗
4. Mechanical and microstructural properties of robotic Cold Metal Transfer (CMT) welded 5083–H111 and 6082–T651 aluminum alloys10.1016/j.matdes.2013.08.018 ↗
5. Materials Science & Engineering A Cold Metal Transfer joining of magnesium AZ31B-to-aluminum A6061–T610.1016/j.msea.2012.09.065 ↗
6. The wetting transition in high and low energy grain boundaries in the Cu (In) system10.1016/0956-7151(92)90070-U ↗
7. Wetting transition on grain boundaries in Al contacting with a Sn-rich melt10.1007/BF00207014 ↗
8. A thermal model of friction stir welding in aluminum alloys10.1016/j.ijmachtools.2008.02.001 ↗
9. Determination of optimum Sr level for eutectic Si modification in Al–Si cast alloys using thermal analysis and tensile properties
10. F.M. Ghaini, M. Sheikhi, M.J. Torkamany, J. Sabbaghzadeh, The relation between liquation and solidification cracks in pulsed laser welding of 2024 aluminium alloy, Mater. Sci. Eng. A. 519 (2009) 167–171.10.1016/j.msea.2009.04.056 ↗
11. Study on porosity formation in laser welds of aluminium alloys (Report 2). Mechanism of porosity formation by hydrogen and magnetism10.1080/09507119909447420 ↗
12. Marioara, Modelling of the microstructure and strength evolution in al-mg-si alloys during multistage thermal processing10.1016/j.actamat.2004.07.002 ↗