MDOxidation behavior in wet oxygen environment of Al2O3 modified SiCf/(SiC + B4C) at 1200 °C
Source abstract
Abstract
Abstract The influence of Al 2 O 3 on the oxidation behavior of SiC f /(SiC + B 4 C) composite materials at 1200 °C in O 2 /H 2 O (40/60) atmosphere was studied employing Scanning Electron Microscope, X-ray Diffraction and Material Universal Testing Machine. Results showed that Al 2 O 3 could impede the crystallization of oxide (cristobalite) during cooling, and lead to a dense and smooth oxidized layer. Furthermore, the strength retention rate increases from 70.44 to 85.94% with Al 2 O 3 after oxidization for 200 h. The above results are attributed to high viscosity and low reaction activity with steam of the aluminosilicates melt. Therefore, Al 2 O 3 can significantly improve the oxidation resistance of SiC f /(SiC + B 4 C) composites in O 2 /H 2 O atmosphere.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Magnesium Oxide Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (9)
Show source-provided references
1. Ceramic Matrix Composites10.1098/rsta.1995.0048 ↗
2. Boron-bearing species in ceramic matrix composites for long-term aerospace applications10.1016/j.jssc.2003.03.005 ↗
3. Fatigue behavior of a Hi-NicalonTM/SiC-B4C composite at 1200 °C in air and steam10.1016/j.msea.2011.11.049 ↗
4. Effect of Al2O3 content on BaO-Al2O3-B2O3-SiO2 glass sealant for solid oxide fuel cell10.1016/j.ceramint.2009.09.045 ↗
5. Wuhan Institute of Building Materials, East China Institute of Chemical Technology, Zhejiang University, Glass Process Principle, China Building Industry Press, 1981, pp. 71–76.
6. The effect of Al2O3 on the high-temperature oxidation resistance of Si-B-C ceramic under air atmosphere
7. Oxidation behavior in wet oxygen environment of Al2O3 added reaction-sintered Si-B-C ceramics10.1016/j.ceramint.2017.11.196 ↗
8. Molecular mechanisms for corrosion of silica and silicate glasses10.1016/0022-3093(94)90708-0 ↗
9. Water dissolution in albite melts: constrains from ab initio NMR calculations10.1016/S0016-7037(02)01000-1 ↗