Segregation study and segregation modeling of Ti in Pb[(Mg1/3Nb2/3)0.60Ti0.40]O3 single crystal grown by Bridgman method
Source abstract
Abstract
Relaxor ferroelectric 0.60Pb(Mg{sub 1/3}Nb{sub 2/3})O{sub 3}-0.40PbTiO{sub 3} single crystal was synthesized by Bridgman method. The segregation along the length of this crystal was observed by various physico-chemical characterization techniques. First, we note the evolution of the crystalline structure along the length of the as-grown crystals. The tetragonality factor c/a increases from 1.013 to 1.020. This evolution has been correlated with the Ti content determination by flame atomic absorption spectrometry, and it is shown that this is due to the evolution of Ti concentration along the crucible. Furthermore, a continuous increase of the fraction of tetragonal phase with increasing Ti content was observed. Hence, we could compare the experimental data with a standard segregation model and therefore calculate the effective segregation coefficient k {sub eff} for this composition. This coefficient was found to be equal to 0.849. The variation of the titanium content along the ingot causes an inevitable fluctuation of the dielectric and piezoelectric properties of the single crystal. Due to the increase of Ti concentration, the Curie point was 186 deg. C at the bottom of the ingot and 222 deg. C at the top. The piezoelectric coefficient of oriented and poled samples varies from 1500more » to 250 pC/N.« less
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Acoustic Wave Resonator Technologies · Microwave Dielectric Ceramics Synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (10)
Show source-provided references
1. Park · IEEE Trans. Ultrason. Ferroelectrics Freq. Con. · 1997 · 44 · 114010.1109/58.655639 ↗
2. Noheda · Curr. Opin. Solid State Mater. Sci. · 2002 · 6 · 2710.1016/S1359-0286(02)00015-3 ↗
3. Swartz · Mater. Res. Bull. · 1982 · 17 · 124510.1016/0025-5408(82)90159-3 ↗
4. Shrout · Am. Ceram. Soc. Bull. · 1987 · 66 · 704
5. Benayad · J. Cryst. Growth · 2004 · 270 · 13710.1016/j.jcrysgro.2004.06.017 ↗
6. Noheda · Phys. Rev. B · 2002 · 66 · 05410410.1103/PhysRevB.66.054104 ↗
7. Luo · Jpn. J. Appl. Phys. · 2000 · 39 · 558110.1143/JJAP.39.5581 ↗
8. Suh · J. Eur. Ceram. Soc. · 2002 · 22 · 21910.1016/S0955-2219(01)00278-3 ↗
9. J.C. Brice, North Holland Publishing Company, Amsterdam, 1965, p. 192.
10. Zawilski · J. Cryst. Growth · 2003 · 258 · 35310.1016/S0022-0248(03)01552-5 ↗