journal article·2020-04-01Open access

Effect of hydrogen embrittlement and non-metallic inclusions on tensile fracture properties of 55CrSi spring steel

Na Li, Wei Wang, Qimin Liang

Materials Research Express· Volume 7· Issue 4

Abstract

Abstract The tensile fracture behavior of 55CrSi spring steels were investigated. The results demonstrate that interior inclusion and hydrogen level has a significant effect on ductility and a minimal effect on tensile strength of the spring steel. It was due to the effect of cracking from MgO-Al2O3 spinel inclusion or the inclusions with a mixture of CaO, SiO2 and part of Al2O3 due to hydrogen. The results of SEM showed that the ductility reduction is connected with the formation of ‘fisheye’ which formed under the influence of mobile hydrogen. For the specimen containing MgO-Al2O3 spinel inclusion, the fracture surface in the ‘fisheye’ area is mainly composed of three regions including typical quasi-cleavage mixed intergranular fracture, dimple mixed transgranular fractures and ductile fracture from the interior to the edge, whereas there is no obvious transition zone from brittle fracture to dimple fracture in the ‘fisheye’ area of the specimen containing inclusions with a mixture of CaO, SiO2 and part of Al2O3.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Fatigue and fracture mechanics · Material Properties and Failure Mechanisms

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Effect of deoxidation process on inclusion and fatigue performance of spring steel for automobile suspension10.1007/s11663-018-1187-x ↗
2. Effects of stress relief tempering on microstructure and tensile/impact behavior of quenched and partitioned commercial spring steel10.1016/j.msea.2018.12.106 ↗
3. Relationship among fatigue life, inclusion size and hydrogen concentration for high-strength steel in the VHCF regime10.1016/j.msea.2009.10.056 ↗
4. Influence of multiphase on the strain hardening behavior of 60Si2CrVAT spring steel treated by a Q–P–T process10.1007/s10853-018-2294-4 ↗
5. Analysis of inclusions in spring steel using scanning electron microscopy and Auger spectroscopy10.1016/j.vacuum.2011.09.015 ↗
6. The influence of hydrogen on very high cycle fatigue properties of high strength spring steel10.1016/j.msea.2008.01.089 ↗
7. Inclusion initiated fracture under cyclic torsion very high cycle fatigue at different load ratios10.1016/j.ijfatigue.2019.01.015 ↗
8. The influence of nonmetallic inclusions on the mechanical properties of steel: a review10.1007/PL00020378 ↗
9. Effect of oxide inclusions on fatigue failure10.1179/imtr.1977.22.1.221 ↗
10. Characterization of inclusions in clean steels: a review including the statistics of extremes methods10.1016/S0079-6425(02)00014-2 ↗
11. Effects of defects, inclusions and inhomogeneities on fatigue strength10.1016/0142-1123(94)90001-9 ↗
12. Fatigue limit model for hardened steels10.1111/j.1460-2695.1992.tb00064.x ↗
13. Inclusion-controlled fatigue properties of 1800 MPA-class spring syeels10.1007/s11661-004-0279-1 ↗
14. Understanding the corrosion mechanism of spring steel induced by MnS inclusions with different sizes10.1007/s11837-018-3026-6 ↗
15. Hydrogen embrittlement in different materials: A review10.1016/j.ijhydene.2018.09.201 ↗
16. The influence of microstructure on the hydrogen embrittlement susceptibility of martensitic advanced high strength steels10.1016/j.mtcomm.2018.07.011 ↗
17. Ultra-long cycle fatigue of high-strength carbon steels:I. Review and analysis of the mechanism of failure10.1016/s0921-5093(03)00135-7 ↗
18. Hydrogen embrittlement of automotive advanced high-strength steels10.1007/s11661-012-1280-8 ↗
19. Effects of hydrogen on behaviour of low cycle fatigue of 2.25Cr-1Mo steel
20. Effect of hydrogen absorption on strain-induced low-cycle fatigue of low carbon steel10.1016/j.proeng.2010.03.060 ↗
21. A new nonmetallic inclusion rating method by positive use of hydrogen embrittlement phenomenon10.1007/s11661-012-1376-1 ↗
22. Internal hydrogen embrittlement of ultrahigh-strength AERMET 100 steel10.1007/s11661-003-0334-3 ↗
23. The role of hydrogen in hydrogen embrittlement fracture of lath martensitic steel10.1016/j.actamat.2012.06.040 ↗
24. State of the art in evaluation and control of steel cleanliness10.2355/isijinternational.43.271 ↗
25. A study on the susceptibility of high strength tempered martensite steels to hydrogen embrittlement (HE) based on incremental step load (ISL) testing methodology10.1016/j.msea.2018.01.032 ↗
26. Microstructural evolution of a low-carbon steel during application of quenching and partitioning heat treatments after partial austenitization10.1007/s11661-008-9701-4 ↗
27. Effect of plastic strain damage on the hydrogen embrittlement of a dual-phase (DP) and a quenching and partitioning (Q&P) advanced high-strength steel10.1016/j.msea.2020.139343 ↗
28. Effect of ferrite on the hydrogen embrittlement in quenched-partitioned tempered low carbon steel10.1016/j.msea.2017.12.032 ↗
29. Effect of bainitic microstructure on the susceptibility of pipeline steels to hydrogen induced cracking10.1016/j.msea.2011.03.036 ↗
30. The influence of hydrogen on the mechanical and fracture properties of some martensitic advanced high strength steels studied using the linearly increasing stress test10.1016/j.corsci.2015.06.038 ↗
31. Comparison of hydrogen embrittlement in three pipeline steels in high pressure gaseous hydrogen environments10.1016/j.corsci.2012.01.028 ↗
32. The mechanism of hydrogen embrittlement in intercritically annealed medium Mn TRIP steel10.1016/j.actamat.2016.04.038 ↗
33. First-principles study on the interaction of H interstitials with grain boundaries in a- and g-Fe10.1103/PhysRevB.84.144121 ↗
34. Effect of overaging and particle size on tensile deformation and fracture of particle-reinforced aluminum matrix composites10.1007/s11661-002-0258-3 ↗
35. Hydrogen embrittlement of steels10.1146/annurev.ms.08.080178.001551 ↗
36. A study on stress corrosion cracking and hydrogen embrittlement of Jethete M152 martensitic stainless steel10.1016/j.msea.2018.10.091 ↗