journal article·2023-08-01Open access

The effect of heat input in multi-pass GMAW of S960QL UHSS based on weaving and stringer bead procedure on microstructure and mechanical properties of HAZ

Tolga Mert, Ugur Gurol, Mustafa Tumer

Materials Research Express· Volume 10· Issue 8

Abstract

Abstract Quenched and tempered S960QL (yield strength ≥ 960 MPa) ultra-high strength steel (UHSS) thick plates were joined by multi-pass robotic gas metal arc welding (GMAW) using weaving and stringer bead techniques. The effects of microstructural changes in heat-affected zone (HAZ) of the joint on toughness and hardness were examined. Weaving and stringer bead techniques applied for the multi-pass welding procedure altered average peak temperatures and exposure time to those temperatures. Mechanical properties of HAZs were evaluated by utilizing notch impact and hardness tests, and these results were correlated with microstructural characterizations using optical (OM) and scanning electron microscopes (SEM). Prior austenite grain (PAG) coarsening occurred because of increased exposure time to peak temperature in coarse-grained HAZ (CGHAZ) of the W-5 (weaving pass) joint. CGHAZs at the face pass, which have not been subjected to a second thermal cycle, have the highest hardness in both joints. Hardness of SCHAZ and CGHAZ of S-12 joint was 7% and 1% higher compared with W-5 joint, respectively. Weld metal hardness of W-5 joint was 15% lower than that of S-12 joint. Both joints not only fulfilled the requirements of minimum 50 J per EN ISO 10025-6 at −20 °C but exceeded this limit by 50% (W-5) and 200% (S-12). Lateral expansions for impact toughness specimens were around 17.5% for S-12 joint, whereas it was 4% for W-5 joint. Since HAZ in the S-12 (stringer bead) joint is narrow compared with the one in the W-5 joint, impact toughness values were higher with the S-12 joint due to the locations of the notches of the impact specimens.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Welding Techniques and Residual Stresses · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Effect of welding heat input on simulated HAZ areas in S960QL high strength steel10.3390/met9111226 ↗
2. Evaluation of the factors influencing the strength of HSLA steel weld joint with softened HAZ10.1007/s40194-015-0262-z ↗
3. Fusion welding of ultra-high strength structural steels—A review10.1016/j.jmapro.2022.07.049 ↗
4. An approach to assessing S960QL steel welded joints using EBW and GMAW10.3390/met12040678 ↗
5. Electron beam and metal active gas welding of ultra-high-strength steel S1100MC: influence of heat input10.1007/s00170-021-08055-6 ↗
6. Mechanical and microstructural characterization of solid wire undermatched multilayer welded S1100MC in different positions10.1016/j.jmapro.2021.11.021 ↗
7. Mechanical and microstructural properties of S1100 UHSS welds obtained by EBW and MAG welding10.1007/s40194-022-01276-7 ↗
8. Microstructure, toughness and hardness of a simulated HAZ in Steel S1100QL and of the HAZ of an actual MAG welded joint made using a metallic flux-cored wire10.17729/ebis.2021.5/5 ↗
9. Cold cracking of S460N steel welded in water environment10.2478/pomr-2018-0104 ↗
10. Temper bead welding of S460N steel in wet welding conditions10.1515/adms-2017-0036 ↗
11. Dissimilar underwater wet welding of HSLA steels10.1007/s00170-020-05617-y ↗
12. Underwater wet welding of S1300 ultra-high strength steel10.1016/j.marstruc.2021.103120 ↗
13. Underwater local cavity welding of S460N steel10.3390/ma13235535 ↗
14. Application possibilities of the S960 steel in underwater welded structures10.22190/FUME210722066T ↗
15. Improving the HAZ toughness of Q+T high strength steels by post weld heat treatment10.1088/1757-899X/426/1/012012 ↗
16. Fatigue crack growth behavior of the simulated HAZ of 800 MPa grade10.1016/j.msea.2010.11.089 ↗
17. Effect of the t8/5 cooling time on the properties of S960MC steel in the HAZ of welded joints evaluated by thermal physical simulation10.3390/met10020229 ↗
18. The contribution of intragranular acicular ferrite microstructural constituent on impact toughness and impeding crack initiation and propagation in the heat-affected zone (HAZ) of low-carbon steels10.1016/j.msea.2015.03.090 ↗
19. A comparison of as-welded and simulated heat affected zone (HAZ) microstructures10.17222/mit.2016.006 ↗
20. Physical simulation aided process optimisation aimed sufficient HAZ toughness for quenched and tempered AHSS
21. Mechanical properties and microstructural evaluation of the heat-affected zone in ultra-high strength steels10.1016/j.tws.2020.107072 ↗
22. Effect of single and multiple thermal cycles on microstructure and mechanical properties of simulated HAZ in low carbon bainitic steel10.1520/MPC20150007 ↗
23. Physical simulation-based characterization of HAZ properties in steels. part 1. high-strength steels and their hardness profiling10.1007/s11223-019-00094-5 ↗
24. Effects of martensite-austenite constituent on crack initiation and propagation in inter-critical heat-affected zone of high-strength low-alloy (HSLA) steel10.1016/j.msea.2018.01.021 ↗
25. Investigation of physically simulated weld HAZ and CCT diagram of HSLA armour steel10.1007/s40194-017-0511-4 ↗
26. Physical simulation-based characterization of HAZ properties in steels. Part 2. dual-phase steels10.1007/s11223-019-00128-y ↗
27. Influence of prior austenite grain size on martensite-austenite constituent and toughness in the heat affected zone of 700MPa high strength linepipe steel10.1016/j.msea.2014.07.100 ↗
28. Role of bainitic microstructures with M-A constituent on the toughness of an HSLA steel for seismic resistant structural applications10.1016/j.msea.2020.140390 ↗
29. Effect of thermo-mechanical cycling on the microstructure and strength of lath martensite in the weld CGHAZ of HSLA steel10.1016/j.msea.2011.06.067 ↗
30. Fracture behaviour of welded joints fabricated in HSLA steels of different strength level10.1016/S0013-7944(99)00085-5 ↗
31. MAG Welding tests of modern high strength steels with minimum yield strength of 700 MPa10.3390/app9051031 ↗
32. TS EN 10025-6 + A1: hot rolled products of structural steels - Part 6: Technical delivery conditions for flat products of high yield strength structural steels in the quenched and tempered condition
33. EN ISO 16834:2012: welding consumables - Wire electrodes, wires, rods and deposits for gas shielded arc welding of high strength steels - Classification
34. EN ISO 14175:2008: welding consumables - Gases and gas mixtures for fusion welding and allied processes
35. Strenx ® 960 E/F data sheet
36. Böhler X 90-IG data sheet
37. ISO 148-1:2016: metallic materials - Charpy pendulum impact test - Part 1: Test method
38. ISO 9016:2012: destructive tests on welds in metallic materials - Impact tests - Test specimen location, notch orientation and examination
39. ISO 6507-1:2018: metallic materials - Vickers hardness test - Part 1: Test method
40. ISO 9015-2:2016: destructive tests on welds in metallic materials - Hardness testing - Part 2: Microhardness testing of welded joints
41. Characterization of armour steel welds using austenitic and ferritic filler metals10.1007/s12666-021-02464-7 ↗
42. Microstructure and mechanical properties of high-strength steel welding consumables with a minimum yield strength of 1100 MPa10.1007/s10853-018-2042-9 ↗
43. Effect of secondary peak temperature on microstructure and toughness in ICCGHAZ of laser-arc hybrid welded X100 pipeline steel joints10.1016/j.jmrt.2020.05.016 ↗
44. Undermatched welding of ultra-high-strength steel S1100 with metal-cored wire: influence of welding positions on mechanical properties10.1007/s11665-022-06876-4 ↗
45. Investigation of mechanism of cleavage fracture initiation in intercritically coarse grained heat affected zone of HSLA steel10.1179/1743284712Y.0000000056 ↗
46. Influence of cooling rate on microstructure and properties of high strength steel weld metal10.1179/136217110X12665048207692 ↗
47. Effect of post-weld tempering on the microstructure and mechanical properties in the simulated HAZs of a high-strength–high-toughness combination marine engineering steel10.1007/s40195-019-00954-8 ↗