Abstract This work aims to study the effect of pre-strain on the fracture behavior of X80 pipeline girth weld joint, a comprehensive analysis was conducted on the microstructure and mechanical properties of the girth weld before and after pre-strain treatment. The mechanical properties were evaluated through tensile testing, Charpy impact testing, and digital image correlation (DIC) strain analysis. Furthermore, the microstructure and fracture morphology of the girth weld were observed using optical electron microscopy (OM) and scanning electron microscopy (SEM). The results show that the application of pre-strain treatment leads to dislocation accumulation at the grain boundary of X80 pipeline girth weld, resulting in stress concentration and subsequent formation of damage holes. This process disrupts the continuity of chain M-A island and initiates small cracks at the grain boundary, ultimately causing a significant decrease in impact toughness and impact work from 177 J to about 10 J.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Fatigue and fracture mechanics · Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Failure analysis of a crude oil pipeline10.1016/j.engfailanal.2006.12.001 ↗
2. Research of strain aging in pipeline steel with a ferrite/martensite dual-phase microstructure10.1002/srin.201300465 ↗
3. The influence of heat treatment on the behavior of fatigue crack growth in welded joints made of S355 under bending loading10.1016/j.ijfatigue.2019.105328 ↗
4. Fracture response of X80 pipe girth welds under combined internal pressure and bending moment10.3390/ma16093588 ↗
5. Failure analysis of a natural gas pipeline rupture10.1007/s11668-013-9745-7 ↗
6. A review on pipeline integrity management utilizing in-line inspection data10.1016/j.engfailanal.2018.05.010 ↗
7. Failure analysis of girth weld cracking of mechanically lined pipe used in gas field gathering system10.1016/j.engfailanal.2016.05.034 ↗
8. Fracture toughness of the materials in welded joint of X80 pipeline steel10.1016/j.engfracmech.2015.07.061 ↗
9. A comparison between fracture toughness at different locations of longitudinal submerged arc welded and spiral submerged arc welded joints of API X80 pipeline steels10.1016/j.engfracmech.2015.09.003 ↗
10. Experimental characterization of dynamic fracture toughness behavior of X80 pipeline steel welded joints for different heat inputs10.1007/s40194-022-01391-5 ↗
11. The analysis of low temperature toughness on X80 pipeline steel welded joint10.1007/s12666-018-1382-0 ↗
12. Cold cracking susceptibility of X100 pipeline steel10.12073/j.cw.20190607001 ↗
13. Key points of safety lifting design for girth weld of high grade and large diameter natural gas pipeline
14. Main characteristics and safety evaluation of girth weld of high grade steel pipeline
15. Effect of strain aging on fracture toughness of welded joints of high-strain pipeline steel10.12073/j.hjxb.20210328001 ↗
16. Study on the effect of loading conditions on the fracture behavior of pipeline with girth weld10.1016/j.ijpvp.2023.104940 ↗
17. Study of tensile deformation and damage law in undermatching X80 pipeline steel welded joints10.3390/met13020226 ↗
18. Strain ageing embrittlement behaviour of X80 self-shielded flux-cored girth weld metal10.1080/10667857.2023.2164978 ↗
19. Correlation of local strain with microstructures around fusion zone of a Cr-Ni-Mo-V steel welded joint10.1016/j.msea.2017.01.015 ↗
20. In situ near-tip normal strain evolution of a growing fatigue crack10.1111/ffe.12391 ↗
21. All about speckles: speckle size measurement10.1111/ext.12110 ↗
22. Kou · 2002
23. Mechanical and metallurgical investigation of martensite–austenite constituents in simulated welding conditions10.1016/j.jmatprotec.2004.04.021 ↗
24. Effect of cyclic plastic deformation on microstructure and mechanical properties of weld metals used for reel-lay pipeline steels10.1016/j.msea.2018.09.036 ↗
25. Effect of plastic deformation on the electrochemical and stress corrosion cracking behavior of X70 steel in near-neutral pH environment10.1016/j.msea.2016.09.033 ↗
26. A comparison of EBSD based strain indicators for the study of Fe-3Si steel subjected to cyclic loading10.1016/j.matchar.2016.03.020 ↗
27. Effect of heat input and heat treatment on the microstructure and toughness of pipeline girth friction welded API 5L X65 steel10.1016/j.msea.2021.142588 ↗