The growth kinetic behaviors of the intermetallics at W/Co interface under the current of spark plasma sintering

Jianan Li, Shenghua Deng, Ruidi Li, Tiechui Yuan

Materials Research Express· Volume 8· Issue 10

Abstract

The interdiffusion behaviors of elements at the W/Co interface under the application of current during SPS were investigated. It is found that Co _7 W _6 and Co _3 W are formed at the W/Co bonding interface. The growth of the Co _3 W layer is apparently improved by the high current during SPS. The growth rate constant of the Co _3 W layer undercurrent is 1.73–3.03 times faster than that without current. The research shows that the growth rate is increased with the current density. The growth activation energy of the Co _3 W layer is calculated to be 229.51 ± 27 kJ mol ^−1 undercurrent, which is smaller than that without current (279.38 ± 11 kJ mol ^−1 ). Moreover, the growth activation energy of the Co _3 W layer is decreased with the increase of the current density. The mechanism of current-improved growth of the Co _3 W layer is suggested to be the fact that the current lowers the nucleation barrier of intermetallic layer, which accordingly promotes chemical reactions.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. A review of multi-physical fields induced phenomena and effects in spark plasma sintering: Fundamentals and applications10.1016/j.matdes.2020.108662 ↗
2. The effect of electric field and pressure on the synthesis and consolidation of materials: A review of the spark plasma sintering method10.1007/s10853-006-6555-2 ↗
3. Reaction diffusion rate coefficient derivation by isothermal heat treatment in spark plasma sintering system10.1016/j.scriptamat.2017.03.005 ↗
4. Direct current-enhanced densification kinetics during spark plasma sintering of tungsten powder10.1016/j.scriptamat.2017.09.009 ↗
5. Enhanced atomic diffusion of Fe–Al diffusion couple during spark plasma sintering10.1016/j.scriptamat.2015.08.012 ↗
6. Fundamental investigations on the spark plasma sintering/synthesis process III. Current effect on reactivity10.1016/j.msea.2005.06.066 ↗
7. Detection of current‐induced vacancies in thin aluminum–copper lines using positrons10.1063/1.116700 ↗
8. Effect of pulsed DC current on atomic diffusion of Nb–C diffusion couple10.1007/s10853-008-2758-z ↗
9. Influence of electric current on interdiffusion kinetics of W-Ti system during spark plasma sintering10.1016/j.ijrmhm.2018.04.014 ↗
10. Electromigration effect in Fe-Al diffusion couples with field-assisted sintering10.1016/j.actamat.2020.01.008 ↗
11. The influence of porous structure on the interdiffusion kinetics of Cu-Ni system during spark plasma sintering10.1007/s11661-020-05635-1 ↗
12. Prediction of glass forming ability and glass forming range for electrodeposited binary Co-W alloys10.1063/1.4717723 ↗
13. The preferential growth behaviors of the intermetallics at the W/Co interface during spark plasma sintering10.1063/5.0026092 ↗
14. Enhanced growth of intermetallic phases in the Ni–Ti system by current effects10.1016/S1359-6454(03)00284-2 ↗
15. Interface kinetics of combustion–diffusion bonding of Ni3Al/Ni and TiAl/Ti under direct current field10.1007/s10853-012-6869-1 ↗
16. The influence of porous structure on the interdiffusion kinetics of Cu-Ni system during spark plasma sintering10.1007/s11661-020-05635-1 ↗
17. Directional electromigration-enhanced interdiffususion in the Cu–Ni system10.1063/1.2809444 ↗
18. Electric current enhanced defect mobility in Ni3Ti intermetallics10.1063/1.1774268 ↗
19. Influence of electric current on microstructure evolution in Ti/Al and Ti/TiAl3 during spark plasma sintering10.1016/j.jallcom.2015.07.079 ↗