The size effect of martensite laths and precipitates on high strength wear-resistant steels
Source abstract
Abstract
Abstract Low alloy high strength wear resistant steels are with high toughness, low cost and good abrasion resistance. It can effectively resist the propagation of wear cracks and prolong the service life of machine components. This paper focuses on the internal relationship between macroscopic physical properties and microscopic martensite lath and precipitate size throughout thickness of wear resistant steel. Four kinds of 40mm thickness wear resistant steels with different alloy chemical composition were produced and investigated. Results show the strength and hardness performance of ARIV are obviously higher than other three steels. ARI have a relatively large strength difference through thickness. The impact toughness of ARIV is relatively uniform, which is greater than that of the ARIII at middle layer and lower than that of the ARIII at 1/4 layer. The width of martensite lath of ARIV is relatively small, mainly 100 ∼ 300 nm, while that of ARII and ARIII is mainly 200 ∼ 400 nm. ARIV steel has shorter martensite lath band and more precipitates below 50 nm. It indicates that the size of martensite laths and precipitates of wear-resistant steels are important factors to determine its performance throughout thickness.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metal Alloys Wear and Properties · Microstructure and Mechanical Properties of Steels · Mechanical stress and fatigue analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Chen · 2012
2. Study on mechanical properties and microstructure of the ultrastrong low alloy wear-resistant steel10.1002/srin.202000155 ↗
3. Investigation and application of high strength low alloy wear resistant cast steel10.1179/175355510X12767031422841 ↗
4. Review on research progress of steel and iron wear-resistant materials10.11900/0412.1961.2019.00370 ↗
5. Progress and perspective of ultra-high strength steels having high toughness
6. Effect of aluminum on microstructure and properties of martensitic wear-resistant and heat-resistant steel10.1007/s11085-012-9320-8 ↗
7. Effects of tempering temperature and Mo/Ni on microstructures and properties of lath martensitic wear-resistant steels10.1016/S1006-706X(13)60085-0 ↗
8. Effect of boron on microstructure evolution and properties of wear-resistant cast Fe–Si–Mn–Cr–B alloy10.1016/j.jmrt.2020.03.081 ↗
9. Effect of Cu on microstructure, crystallography and mechanical properties in Fe-B-C-Cu alloys10.1016/j.msea.2017.09.135 ↗
10. Effects of chromium addition on fracture toughness and hardness of oriented bulk Fe2B crystals10.1016/j.matchar.2015.10.017 ↗
11. Effects of Mn addition on the two-body abrasive wear behavior of Fe-3.0 wt% B alloy10.1016/j.triboint.2016.07.008 ↗
12. Effect of low-temperature austempering and quenching and partitioning treatments on adhesive wear resistance of high-silicon multiphase steels10.1007/s11665-020-04699-9 ↗
13. Comparison of impact-abrasive wear characteristics and performance of direct quenched (DQ) and direct quenched and partitioned (DQ&P) steels10.1016/j.wear.2017.12.016 ↗
14. Effect of heat treatment on microstructure and mechanical properties of low-alloy wear-resistant steel NM45010.1088/2053-1591/abd72f ↗
15. Effect of tempering and cryogenic treatment on wear and mechanical properties of hot work tool steel (H13)10.1016/j.matpr.2021.01.361 ↗
16. Effect of tempering temperature on microstructures and wear behavior of a 500HB grade wear-resistant steel10.3390/met9010045 ↗
17. Microstructural characteristics and mechanical properties of low-alloy, medium-carbon steels after multiple tempering10.1007/s40195-018-0805-6 ↗
18. Heat treatment of multi-element low alloy wear-resistant steel10.1016/j.msea.2005.01.023 ↗
19. Microstructure and properties evolution of Nb-bearing medium Cr wear-resistant cast steel during heat treatment10.1007/s42243-020-00510-0 ↗
20. Evolution of deformation twins with strain rate in a medium-manganese wear-resistant steel Fe–8Mn–1C–1.2Cr–0.2V10.1007/s42243-018-00225-3 ↗
21. Effect of cooling rate on microstructure, hardness, and residual stress of 0.28C–0.22Ti wear-resistant steel10.1007/s42243-019-00283-1 ↗
22. Three-body abrasion wear resistance of TiC-reinforced low-alloy abrasion-resistant martensitic steel under dry and wet sand conditions10.1016/j.wear.2020.203310 ↗
23. Effect of TiC particles on three-body abrasive wear behaviour of low alloy abrasion-resistant steel10.1016/j.wear.2019.202971 ↗
24. Block and sub-block boundary strengthening in lath martensite10.1016/j.scriptamat.2016.01.043 ↗
25. Effect of hardenability on microstructure and property of low alloy abrasion-resistant steel10.1016/j.msea.2020.139901 ↗
26. Effect of block size on the strength of lath martensite in low carbon steels
27. Anisotropy of strength and plasticity in lath martensite steel10.1016/j.msea.2016.07.047 ↗
28. Effect of Nb on microstructure and yield strength of a high temperature tempered martensitic steel10.1088/2053-1591/aab831 ↗