Abstract This study investigates the possibility of accelerating the slow early reaction process of sodium carbonate (SC) activated slag (GGBFS) mixtures by adding a small amount of calcium oxide (quicklime, CaO) or calcium hydroxide (hydrated lime, Ca(OH) 2 ). The effects of these additions on the compressive strength of SC-activated slag (SCAS) binders at ambient temperature and steam curing conditions have been investigated. Test results showed that the flowability of the mortars decreased with the substitution of quicklime and hydrated lime. It has been observed that the SCAS mixture, which has a very long setting time and very low compressive strength, can have reasonable early and ultimate compressive strength (up to about 8 MPa at 2-day and 45 MPa at 28-day) and setting times (between 25–240 min) with the addition of a small amount of quicklime or hydrated lime. The ultimate compressive strength of SCAS cured at ambient temperature showed a decreasing tendency with increased quicklime and hydrated lime contents. The optimum lime content for both quicklime and hydrated lime was found to be between 3% and 4%. The early age compressive strength of quicklime and hydrated lime incorporated SCAS can be significantly improved by steam curing. Compressive strength values reaching 28 MPa at 2 days was achieved by steam curing at 50 °C after a 24 h pre-curing time. Steam curing temperatures above 50 °C caused a significant reduction in the ultimate compressive strength of SCAS.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Concrete and Cement Materials Research · Microbial Applications in Construction Materials · Magnesium Oxide Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Innovation in in use and research on cementitious material10.1016/j.cemconres.2007.09.025 ↗
2. Low-CO2 emission strategies to achieve net zero target in cement sector10.1016/j.jclepro.2023.137466 ↗
3. Properties of alkali activated blast furnace slag and fly ash based mortars
4. Mechanical properties and durability of volcanic ash based geopolymer mortars10.1016/j.conbuildmat.2016.07.141 ↗
5. Effect of freeze–thaw cycles on the mechanical behavior of geopolymer concrete and Portland cement concrete containing microencapsulated phase change materials10.1016/j.conbuildmat.2018.12.057 ↗
6. Early structural build-up behavior, setting mechanism, and nanostructure of alkali-activated GGBFS mixtures10.1111/jace.19458 ↗
7. Geopolymer technology: the current state of the art10.1007/s10853-006-0637-z ↗
8. Development of greener alkali-activated cement: utilisation of sodium carbonate for activating slag and fly ash mixtures10.1016/j.jclepro.2015.12.010 ↗
9. On the development of fly ash-based geopolymer concrete
10. Setting and mechanical properties of alkali-activated fly ash/slag concrete manufactured at room temperature10.1016/j.conbuildmat.2013.05.107 ↗
11. Shrinkage compensation of alkali-activated slag concrete and microstructural analysis10.1016/j.conbuildmat.2014.05.085 ↗
12. A review on shrinkage-reducing methods and mechanisms of alkali-activated/geopolymer systems: effects of chemical additives10.1016/j.jobe.2022.104056 ↗
13. Setting of alkali-activated slag cement. Influence of activator nature10.1680/adcr.2001.13.3.115 ↗
14. Role of carbonates in the chemical evolution of sodium carbonate-activated slag binders10.1617/s11527-014-0412-6 ↗
15. Effect of activator mix on the hydration and strength behaviour of alkali-activated slag cements10.1680/adcr.2003.15.3.129 ↗
16. Factors affecting the properties of Na2CO3 activated fly Ash/Slag paste
17. Alkali-activated slag mortars Mechanical strength behaviour10.1016/S0008-8846(99)00154-4 ↗
18. Factors affecting the strength of alkali activated slag10.1016/0008-8846(94)90026-4 ↗
19. Effects of type and dosage of alkaline activator and temperature on the properties of alkali-activated slag mixtures10.1016/j.conbuildmat.2006.07.002 ↗
20. Pore solution chemistry of alkali-activated ground granulated blast-furnace slag10.1016/S0008-8846(98)00212-9 ↗
21. Effect of Ca(OH)2 addition on the engineering properties of sodium sulfate activated slag10.3390/ma14154266 ↗
22. Structure of calcium silicate hydrates formed in alkaline-activated slag: influence of the type of alkaline activator10.1111/j.1151-2916.2003.tb03481.x ↗
23. Reaction mechanisms of one-part and two-part slag-based binders activated by sodium carbonate and lime10.1016/j.cemconcomp.2025.105992 ↗
24. Influence of activator on the strength and drying shrinkage of alkali-activated slag mortar10.1016/j.conbuildmat.2007.10.011 ↗
25. Effect of admixtures on properties of alkali-activated slag concrete10.1016/S0008-8846(00)00349-5 ↗
26. Use of glass waste as an activator in the preparation of alkali-activated slag. Mechanical strength and paste characterisation10.1016/j.cemconres.2013.12.005 ↗
27. Accelerating the reaction process of sodium carbonate-activated slag mixtures with the incorporation of a small addition of sodium hydroxide/sodium silicate10.1016/j.cemconcomp.2023.105118 ↗
28. Effect of temperature on the fresh and hardened state properties of alkali-activated slag/fly ash mixtures10.1617/s11527-023-02194-w ↗
29. Reaction kinetics, reaction products and compressive strength of ternary activators activated slag designed by Taguchi method10.1016/j.matdes.2015.07.077 ↗
30. Characterisation of reactive magnesia and sodium carbonate-activated fly ash/slag paste blends10.1016/j.conbuildmat.2015.06.015 ↗
31. Chemical acceleration of a neutral granulated blast-furnace slag activated by sodium carbonate10.1016/j.cemconres.2015.02.014 ↗
32. Fundamental study on alkali-activated slag system with sodium carbonate or calcium hydroxide10.4236/msce.2024.126005 ↗
33. Influence of the combination of calcium oxide and sodium carbonate on the hydration reactivity of alkali-activated slag binders10.1016/j.jclepro.2017.10.077 ↗
34. Influence of various additives on the early age compressive strength of sodium carbonate activated slag composites: an overview10.1515/jmbm-2020-0011 ↗
35. Hot-pressed geopolymer: dual effects of heat and curing time10.1016/j.cemconcomp.2017.11.004 ↗
36. Dissolution mechanism of fly ash to quantify the reactive aluminosilicates in geopolymerisation10.1016/j.resconrec.2019.104421 ↗
37. Neville · 1995
38. Effect of nano-CaCO3 on hydration of cement containing supplementary cementitious materials10.1680/adcr.9.00016 ↗
39. Microstructure and strength development of sodium carbonate-activated blast furnace slags10.1061/(ASCE)MT.1943-5533.0002944 ↗
40. Assessing the chemical involvement of limestone powder in sodium carbonate activated slag10.1617/s11527-017-1003-0 ↗
41. Effect of the curing condition and high-temperature exposure on ground-granulated blast-furnace slag cement concrete10.1186/s40069-020-00437-6 ↗
42. Hydration characteristics and microstructure of alkali-activated slag concrete: a review10.1016/j.eng.2021.07.026 ↗
43. Mechanical properties of alkali activated slag binder based concrete at elevated temperatures10.1007/s43621-025-01542-w ↗
44. Behaviour of alkali-activated concrete at elevated temperatures: a critical review10.1016/j.cemconcomp.2023.104961 ↗
45. Effect of curing temperature on the development of hard structure of metakaolin-based geopolymer10.1016/j.conbuildmat.2009.12.023 ↗
46. Effect of GGBFS on setting, workability and early strength properties of fly ash geopolymer concrete cured in ambient condition10.1016/j.conbuildmat.2014.05.080 ↗
47. Influence mechanism of curing temperature on geopolymerization reaction: a comprehensive review10.1016/j.jobe.2025.112195 ↗
48. Effect of curing temperature on geopolymerization of metakaolin-based geopolymers10.1016/j.clay.2014.06.024 ↗
49. Influence of the long term curing temperature on the hydration of alkaline binders of blast furnace slag-metakaolin10.1016/j.conbuildmat.2016.03.111 ↗