Abstract

Abstract In last two decades a promising performance improvement in the electrical insulation materials has been reported by many researchers using different nano fillers (NFs). In recent years another type of NFs called core–shell type nano fillers have shown even more attention than ordinary NFs. The core–shell NFs are a combination of nano particle core coated with outer nano layer of different material. The core–shell NFs combine the beneficial properties of two material with in one NF. Recently a few studies have reported a considerable improvement in the dielectric properties of epoxy by utilising TiO2@SiO2 core–shell NFs. The TiO2@SiO2 particles have a core of TiO2 coated with an out layer of SiO2 at nano level. This study investigates the improvement in tracking performance of silicone rubber (SiR) using TiO2@SiO2 core–shell nano particles which has not been reported previously. The tracking immunity of low (below 1%) and high (above 1%) filler concentrations of nano TiO2@SiO2 incorporated into SiR was investigated according to IEC 60587. The results showed that an optimum percentage of 0.6 wt% of TiO2@SiO2 imparts best immunity to silicone rubber against tracking.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High voltage insulation and dielectric phenomena · Power Transformer Diagnostics and Insulation · Dielectric materials and actuators

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Aging of silicone rubber composite insulators on 400 kV transmission lines10.1109/TDEI.2007.302881 ↗
2. Papailiou · 2013
3. Tracking and erosion resistance of LSR and HTV silicon rubber samples under acid rain conditions10.1109/TDEI.2018.006672 ↗
4. Tracking and erosion of HTV silicone rubbers of different thickness10.1109/94.946722 ↗
5. The DC inclined-plane tracking and erosion test and the role of inorganic fillers in silicone rubber for DC insulation10.1109/MEI.2015.6996674 ↗
6. Performance of silicone rubber nanocomposites in salt-fog, inclined plane, and laser ablation tests10.1109/TDEI.2010.5412019 ↗
7. Comparison of ATH and SiO2 fillers filled silicone rubber composites for HTV insulators10.1016/j.compscitech.2017.12.006 ↗
8. Polydimethylsiloxane and alumina trihydrate system subjected to dry-band discharges or high temperature part II: electrical insulation10.1109/TDEI.2004.1324359 ↗
9. The effect of ATH and silica on tracking and erosion resistance of silicone rubber compounds for outdoor insulation10.1109/ELINSL.2002.995929 ↗
10. Erosion of silicone rubber composites in the AC and DC inclined plane tests10.1109/TDEI.2013.6451362 ↗
11. Tracking and erosion resistance performance investigation on nano-sized SiO2 filled silicone rubber for outdoor insulation applications10.1109/TDEI.2014.003892 ↗
12. Tracking, erosion and thermal distribution of micro-AlN+ nano-SiO2 co-filled silicone rubber for high-voltage outdoor insulation10.1049/hve.2018.5033 ↗
13. Effects of thermal properties on tracking and erosion resistance of micro-ATH/AlN/BN filled silicone rubber composites10.1109/TDEI.2018.007125 ↗
14. Tracking/erosion resistance analysis of nano-al(OH)3 filled silicone rubber insulating materials for high voltage DC applications10.5370/JEET.2015.10.1.355 ↗
15. Tracking and erosion resistance of silicone rubber/BN nanocomposites under DC voltage10.1109/ICSD.2013.6619791 ↗
16. Tracking and surface degradation of barium titanate filled silicone rubber nanocomposites10.1109/CEIDP.2015.7352062 ↗
17. Analysis of surface tracking of micro and nano size alumina filled silicone rubber for high voltage AC transmission10.5370/JEET.2013.8.2.345 ↗
18. Thermal distribution analysis and suppression mechanism of carbonized tracking and erosion in silicone rubber/SiO2 nanocomposites10.1016/j.polymertesting.2018.07.013 ↗
19. Effect of filler concentration on tracking resistance of ATH-filled silicone rubber nanocomposites10.3390/en12122401 ↗
20. Investigation on relationship between breakdown strength enhancement of composites and dielectric characteristics of nanoparticle10.1109/TDEI.2015.005378 ↗
21. Investigation on optimal filler loadings for dielectric strength enhancement of epoxy/TiO2@SiO2 nanocomposite,’10.1088/2053-1591/ab0ef2 ↗
22. Effect of nano filler concentration on leakage current and partial discharge properties of zepoxy nano composites10.1007/s42452-019-1227-4 ↗
23. Synthesis, characterization and photocatalytic activity of carbon nanotube/titanium dioxide nanocomposites10.1007/s13369-017-2861-z ↗
24. Low dielectric constant materials for microelectronics
25. Performance of silicone rubber in DC inclined plane tracking tests10.1109/TDEI.2010.5448108 ↗
26. Effects of nano-SiO2 particles on surface tracking characteristics of silicone rubber composites10.1063/1.4895734 ↗