Abstract The corrosion rate in a modified Hanks’ solution (containing no Ca2+ ions) was higher than in Hanks’ solution. The increase was by a factor of ∼12 for HP Mg and AZ91, and a factor of ∼6 for WE43. This quantitatively highlights the critical role of Ca2+ ions for Mg corrosion in synthetic body fluids. The Ca2+ ion containing solutions produced a dense corrosion-product layer of hydroxyapatite, Ca3(PO4)2) · Ca(OH)2, a greater fraction of which stayed on the corroding surface (∼0.2–0.3) compared with the Ca2+ ion free solutions which produced magnesium phosphate, Mg3(PO4)2.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Corrosion Behavior and Inhibition · Magnesium Oxide Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (57)

Show source-provided references
1. Magnesium and its alloys as orthopedic biomaterials: a review10.1016/j.biomaterials.2005.10.003 ↗
2. Biodegradable metals10.1016/j.mser.2014.01.001 ↗
3. A review on magnesium alloys as biodegradable materials10.1007/s11706-010-0024-1 ↗
4. High purity biodegradable magnesium coating for implant application10.1016/j.mseb.2011.07.002 ↗
5. In vitro and in vivo corrosion measurements of magnesium alloys10.1016/j.biomaterials.2005.07.037 ↗
6. Degradable biomaterials based on magnesium corrosion10.1016/j.cossms.2009.04.001 ↗
7. In vivo corrosion of four magnesium alloys and the associated bone response10.1016/j.biomaterials.2004.09.049 ↗
8. Magnesium-based compression screws: a novelty in the clinical use of implants10.1007/s11837-015-1773-1 ↗
9. Magnesium-based implants: beyond fixators10.1016/j.jot.2016.12.001 ↗
10. Safety and performance of the second-generation drug-eluting absorbable metal scaffold in patients with de-novo coronary artery lesions (BIOSOLVE-II): 6 month results of a prospective, multicentre, non-randomised, first-in-man trial10.1016/S0140-6736(15)00447-X ↗
11. Rates of in vivo (arterial) and in vitro biocorrosion for pure magnesium10.1002/jbm.a.35179 ↗
12. Recent advances in biodegradable metals for medical sutures: a critical review10.1002/adhm.201500189 ↗
13. Absorbable Mg surgical tack: proof of concept & in situ fixation strength10.1016/j.jmbbm.2019.05.035 ↗
14. Fabrication of a magnesium alloy with excellent ductility for biodegradable clips10.1016/j.actbio.2015.10.023 ↗
15. Review of recent developments in the field of magnesium corrosion10.1002/adem.201400434 ↗
16. Building towards a standardised approach to biocorrosion studies: a review of factors influencing Mg corrosion in vitro pertinent to in vivo corrosion10.1007/s40843-017-9173-7 ↗
17. Evolution of hydrogen at dissolving magnesium surfaces10.1016/j.corsci.2013.01.017 ↗
18. Influence of crystallographic texture and grain size on the corrosion behaviour of as-extruded Mg alloy AZ31 sheets10.1016/j.corsci.2017.08.004 ↗
19. Potentiodynamic polarisation study of bulk metallic glasses based on the Mg-Zn-Ca ternary system10.1179/1743278212Y.0000000016 ↗
20. In vivo quantification of hydrogen gas concentration in bone marrow surrounding magnesium fracture fixation hardware using an electrochemical hydrogen gas sensor10.1016/j.actbio.2018.04.032 ↗
21. Current status on clinical applications of magnesium-based orthopaedic implants: a review from clinical translational perspective10.1016/j.biomaterials.2016.10.017 ↗
22. Effect of stress on corrosion of high-purity magnesium in vitro and in vivo10.1016/j.actbio.2018.11.019 ↗
23. In vivo characterization of magnesium alloy biodegradation using electrochemical H2 monitoring, ICP-MS, and XPS10.1016/j.actbio.2017.01.024 ↗
24. Mechanical behavior of in vivo degraded second generation resorbable magnesium scaffolds (RMS)10.1016/j.jmbbm.2018.12.008 ↗
25. Selecting medium for corrosion testing of bioabsorbable magnesium and other metals–a critical review10.1016/j.corsci.2020.108722 ↗
26. Possible dissolution pathways participating in the Mg corrosion reaction10.1016/j.corsci.2014.12.004 ↗
27. Corrosion performance and mechanical properties of sputter-deposited MgY and MgGd alloys10.1016/j.corsci.2013.08.027 ↗
28. Corrosion of ultra-high-purity Mg in 3.5% NaCl solution saturated with Mg (OH)210.1016/j.corsci.2013.05.018 ↗
29. Advances in Mg corrosion and research suggestions10.1016/j.jma.2013.09.003 ↗
30. Galvanostatic anodic polarisation curves and galvanic corrosion of high purity Mg in 3.5% NaCl saturated with Mg (OH)210.1016/j.corsci.2011.12.002 ↗
31. Calculated phase diagrams and the corrosion of die-cast Mg–Al alloys10.1016/j.corsci.2008.12.015 ↗
32. Influence of the β-phase morphology on the corrosion of the Mg alloy AZ9110.1016/j.corsci.2008.04.010 ↗
33. Understanding magnesium corrosion—a framework for improved alloy performance10.1002/adem.200310405 ↗
34. Corrosion mechanisms of magnesium alloys10.1002/(SICI)1527-2648(199909)1:1<11::AID-ADEM11>3.0.CO;2-N ↗
35. An innovative specimen configuration for the study of Mg corrosion10.1016/j.corsci.2010.09.016 ↗
36. Understanding Mg corrosion in the body for biodegradable medical implants10.1016/j.scriptamat.2018.05.021 ↗
37. Understanding the corrosion of Mg and Mg alloys10.1016/B978-0-12-409547-2.13426-2 ↗
38. The influence of pH on the corrosion rate of high-purity Mg, AZ91 and ZE41 in bicarbonate buffered Hanks’ solution10.1016/j.corsci.2015.09.018 ↗
39. In vitro corrosion and biocompatibility of binary magnesium alloys10.1016/j.biomaterials.2008.10.021 ↗
40. Corrosion mechanism applicable to biodegradable magnesium implants10.1016/j.mseb.2010.12.017 ↗
41. Assessing the degradation performance of ultrahigh-purity magnesium in vitro and in vivo10.1016/j.corsci.2014.09.008 ↗
42. Influence of testing environment on the degradation behavior of magnesium alloys for bioabsorbable implants, TMS 2015
43. Corrosion of high purity Mg, Mg2Zn0.2Mn, ZE41 and AZ91 in Hank’s solution at 37 C10.1016/j.corsci.2011.06.030 ↗
44. Corrosion of high purity Mg, AZ91, ZE41 and Mg2Zn0.2Mn in Hank’s solution at room temperature10.1016/j.corsci.2010.10.008 ↗
45. The in vivo and in vitro corrosion of high-purity magnesium and magnesium alloys WZ21 and AZ9110.1016/j.corsci.2013.06.019 ↗
46. Influence of the chloride ion concentration on the corrosion of high-purity Mg, ZE41 and AZ91 in buffered Hank’s solution10.1007/s10856-013-5087-y ↗
47. In vivo and in vitro degradation comparison of pure Mg, Mg-10Gd and Mg-2Ag: a short term study10.22203/eCM.v033a07 ↗
48. Magnesium alloys: predicting in vivo corrosion with in vitro immersion testing10.1002/jbm.b.32680 ↗
49. The in vitro and in vivo evaluation of the biocompatibility of Mg alloys10.1088/1748-6041/9/1/015006 ↗
50. Understanding the corrosion of Mg and Mg alloys10.1016/B978-0-12-409547-2.13426-2 ↗
51. Understanding the corrosion of Mg and Mg alloys10.1016/B978-0-12-409547-2.13426-2 ↗
52. The role of individual components of simulated body fluid on the corrosion behavior of commercially pure Mg10.1016/j.corsci.2018.11.011 ↗
53. Influence of hot rolling on the corrosion behavior of several Mg–X alloys10.1016/j.corsci.2014.10.012 ↗
54. Local pH and its evolution near Mg alloy surfaces exposed to simulated body fluids10.1002/admi.201800169 ↗
55. FIB-TEM study of magnesium corrosion products after 14 days in the murine artery10.1021/acsbiomaterials.5b00044 ↗
56. Magnesium in the murine artery: probing the products of corrosion10.1016/j.actbio.2013.11.021 ↗
57. Research on Mg-Zn as a degradable biomaterial10.1016/j.actbio.2009.06.028 ↗