journal article·2023-10-01Open access

Strengthening phase and mechanical property analysis of artificially aged Al7075 – Ni coated Al2024 composites

Karthik B M, Sathish Kumar K M, Sathyashankara Sharma, Gowrishankar M C, Ananda Hegde, Nithesh K

Materials Research Express· Volume 10· Issue 10

Abstract

Abstract This technical paper demonstrates the possibilities of nickel (Ni) coated Al2024 powder reinforcement in an Al7075 matrix using the liquid stir casting technique. Additionally, the paper focuses on achieving stable properties by implementing artificial aging heat treatment. To apply the Ni coating, the electroless nickel plating technique was utilized, and a minimum coating thickness of 8 μm was determined to effectively prevent the dissolution of Al2024 powder reinforcements within the Al7075 matrix. Stir casting facilitated the uniform dispersion of the coated Al2024 powder up to a weight percentage of 7%. Subsequently, the Al7075 alloy and composites underwent artificial aging through solution heat treatment (SHT) at 450 °C for 4 h, followed by water quenching and aging at temperatures of 120, 150, and 180 °C. Aging at 120 °C was found to yield superior results compared to aging at 150 and 180 °C, thus identified as the optimum aging temperature. When the Ni coating thickness was increased beyond the optimal 8 μm, the resulting enhancements in hardness for both as-cast and peak-aged specimens, as well as the tensile strength, were not significant. The improvements observed were only marginal, ranging between 2 to 3%. Fracture surface analysis revealed that the predominant fracture mode in the Al7075 alloy was ductile, characterized by dimple rupture. In the as-cast Al7075-(7%, 8 μm) Al2024 composite, a mixed fracture mode comprising both brittle and ductile characteristics was observed. In the peak-aged (120 °C) Al7075-(7%, 8 μm)Al2024 composite, the overall fracture mode exhibited a dominant brittle nature. Analytical techniques including XRD, TEM, and EDS confirmed the presence of Mg2Si, MgZn2, CuAl2, and CuAl2Mg phases in the peak-aged (120 °C) Al7075-(7%, 8 μm) Al2024 composite. These phases contributed to the enhancement of the properties of both the Al7075 alloy and its composites. The developed composites can be used in automobile parts and aerospace applications.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Improving both strength and ductility of Al-7075 by combining dual equal channel lateral extrusion with aging heat treatment10.1007/s40997-020-00416-y ↗
2. Holistic life cycle approach for lightweight automotive components10.1051/metal/2014034 ↗
3. Influence of solution heat treatment on mechanical response and fracture behaviour of aluminium alloy sheets: an experimental study10.1016/j.matdes.2015.09.044 ↗
4. Effect of cyclic solution treatment on microstructure and mechanical properties of friction stir welded 7075 Al alloy10.1016/j.msea.2015.10.010 ↗
5. Microstructures and tensile properties of Al2024-Al4Sr composite after hot extrusion and T6 heat treatment10.1016/j.msea.2014.12.023 ↗
6. Mechanical properties, corrosion behavior and microstructures of 7075 aluminium alloy with various aging treatments10.1016/S1003-6326(08)60130-2 ↗
7. Optimisation of porosity of 7075 Al alloy 10% SiC composite produced by stir casting process through Taguchi method10.1504/IJMatEI.2009.024031 ↗
8. Wear behavior and its correlation with mechanical properties of TiB2 reinforced aluminium-based composites10.1155/2011/837469 ↗
9. Effects of particulate reinforcement and heat treatment on the hardness and wear properties of Al2024-MoSi2 nanocomposites10.1016/j.matdes.2010.11.037 ↗
10. Solar selective black nickel–cobalt coatings on aluminum alloys10.1016/j.solmat.2006.12.001 ↗
11. Electroless nickel plating–a review10.1007/s12633-015-9367-7 ↗
12. Fabrication of Al7075 metal matrix composite through stir casting method - a review
13. Study of Cu addition on precipitation behaviors and mechanical properties in AA6082 Al-Mg-Si Alloy10.4028/www.scientific.net/MSF.546-549.825 ↗
14. Aluminium alloys--A century of age hardening
15. Effect of precipitation during quenching on the mechanical properties of the aluminium alloy 7010 in the W-temper10.1016/j.jmatprotec.2004.04.226 ↗
16. A new paradigm in the design of aluminum alloys for aerospace applications10.4028/www.scientific.net/MSF.331-337.127 ↗
17. HREM study and structure modeling of the η′ phase, the hardening precipitates in commercial Al–Zn–Mg alloys10.1016/S1359-6454(99)00138-X ↗
18. Effect of heat treatment on some mechanical properties of 7075 aluminium alloy10.1590/S1516-14392012005000167 ↗
19. Investigation of microstructural evolution and mechanical properties during two-step ageing treatment at 115 and 160 ◦C in an Al–Zn–Mg– Cu alloy pre-stretched thick plate10.1016/j.matchar.2007.01.006 ↗
20. Aging behavior of Li containing Al–Zn–Mg–Cu alloys10.1016/S0921-5093(99)00684-X ↗
21. Characterization of the mechanical properties changes in an Al-Zn-Mg alloy after a two-step ageing treatment at 70 °C and 135 °C10.1016/j.matdes.2009.12.033 ↗
22. Effect of age-hardening temperature on mechanical and wear behavior of furnace-cooled Al7075-tungsten carbide composite10.3390/ma15155344 ↗
23. Development of ultrafine grained high strength age hardenable Al7075 alloy by cryorolling10.1016/j.matdes.2011.02.051 ↗
24. Effect of the over-ageing treatment on the mechanical properties of AA2024 aluminum alloy
25. Secondary precipitation in an Al–Mg–Si–Cu alloy10.1016/j.actamat.2007.01.006 ↗
26. Two types of S phase precipitates in Al–Cu–Mg alloys10.1016/j.actamat.2006.09.015 ↗
27. Quantitative study of dimensional stability mechanism and microstructure evolution during precipitation process of 2024Al alloy10.1016/j.jmst.2021.04.002 ↗
28. Reply to the comments on ‘Room-temperature precipitation in quenched Al–Cu–Mg alloys: a model for the reaction kinetics and yield-strength development10.1080/09500830600678888 ↗
29. A multi-mechanistic model for precipitation strengthening in Al-Cu-Mg alloys during non-isothermal heat treatments10.4028/www.scientific.net/MSF.519-521.277 ↗
30. Effect of the age-hardening time on the microstructure of cold rolled Al2024 alloy10.1017/S1431927619013862 ↗
31. Effect of SiC content on mechanical and tribological properties of Al2024-SiC Composites10.1007/s12633-020-00757-y ↗
32. On the correlation of mechanical and physical properties of 7075-T6 Al alloy10.1016/j.engfailanal.2004.09.005 ↗
33. T6 heat treatment of rheocasting 7075 Al alloy10.1016/j.msea.2011.10.068 ↗
34. Improvements in mechanical and stres corrosion cracking properties in Al-alloy 7075 via retrogression and reaging10.1016/j.msea.2007.08.025 ↗
35. Evolution of grain boundary precipitates in Al 7075 upon aging and correlation with stress corrosion cracking behavior10.1007/s11661-012-1413-0 ↗
36. Effect of heat treatment on hardness of Al7075-Albite particulate composites10.1016/j.matpr.2017.08.028 ↗
37. Fabrication of aluminium composites reinforced with carbon fibres by a centrifugal infiltration process10.1016/j.compositesa.2010.07.014 ↗
38. Microstructural features and mechanical properties of artificially aged Al202410.1007/s11223-013-9504-8 ↗
39. Influence of aging & varying weight fraction of Al2O3 particles on the mechanical behaviour & volumetric wear rate of Al 7075 alloy composite produced by liquid metallurgy route10.1088/2053-1591/ab20b8 ↗
40. Effects of aging and deep cryogenic treatment on wear behavior of Al7075 Alloy10.1115/1.4052481 ↗
41. The effects of precipitate size on the hardness and wear behaviors of aged 7075 aluminum alloys produced by powder metallurgy route10.1007/s13369-016-2078-6 ↗
42. Influence of Cu addition on the heat treatment response of A356 foundry alloy10.1016/j.mtcomm.2019.02.013 ↗
43. Enhancement of impact toughness properties of Al7075 alloy via double aging heat treatment10.29109/gujsc.1108116 ↗
44. Mechanical and electrochemical characteristics of solutionized AA 6061, AA6013 and AA 5086 aluminum alloys10.1016/j.jmrt.2018.12.014 ↗
45. Effect of the age-hardening time on the microstructure of cold rolled Al2024 alloy10.1017/S1431927619013862 ↗
46. The effect of rolling and aging on mechanical and tribological properties in B4C particle reinforced Al7075 matrix composites10.1007/s13369-022-06891-6 ↗
47. Tensile properties and fracture toughness of heat treated Al 6082 alloy
48. Effect of aging time and aging temperature on fatigue and fracture behavior of 6063 aluminum alloy under seawater influence10.1016/j.matdes.2006.12.003 ↗
49. Heat treatment of metals
50. Aging behavior and tensile properties of squeeze cast Al6061/SiC metal matrix composites
51. Experimental investigation on the influence of reinforcement and precipitation hardening parameters of AA 6061-SiCp composites