journal article·2019-04-17

Effect of suction casting process on microstructure and mechanical properties of Au80Sn20 alloy flake

Xiyang Zeng, Yunzhu Ma, Wensheng Liu, Yufeng Huang, Siwei Tang, Baishan Chen

Materials Research Express· Volume 6· Issue 7
Publisher page

Abstract

Gold80–tin20 (Au80Sn20) eutectic alloy with coarse primary ζ ′-phase and irregular eutectic structure is intrinsically brittle. In this study, various processes were applied to prepare Au80Sn20 alloy. The effects of suction casting processing parameters on the solidification structure, indentation hardness, and modulus were investigated, and the underlying mechanism was discussed. Results showed that the conventionally cast microstructure was made up of coarse dendritic ζ ′-Au5Sn (primary phase) and ( ζ ′-Au5Sn and δ -AuSn) eutectic structure; however, in rapid solidification process size of the primary phase decreased from 200 μ m to approximately 10 μ m. Moreover, when the current of arc-melting was increased, size of the primary phase continuously shrunk to approximately 3 μ m, leading to the change in the morphology from fine dendrites to dots-like. Moreover, volume of the primary phase was correspondingly reduced as the lamellar spacing decreased from 500 ± 50 nm to 150 ± 10 nm. The two-phase orientation relationship of lamellar eutectic was ( 11 2 ¯ 0 ) A u 5 S n / / ( 01 1 ¯ 0 ) A u S n . Besides, hardness of the Au80Sn20 eutectic alloy increased from 1.67 to 2.17 GPa, and the modulus increased from 70.67 to 83.17 GPa with increasing suction casting current.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Advanced materials and composites · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. 10.1007/s11664-015-4164-z10.1007/s11664-015-4164-z ↗
2. 10.1007/s11664-016-4733-910.1007/s11664-016-4733-9 ↗
3. 10.1007/s10854-016-4520-710.1007/s10854-016-4520-7 ↗
4. 10.1109/TADVP.2004.83186210.1109/TADVP.2004.831862 ↗
5. 10.1016/j.microrel.2011.11.00910.1016/j.microrel.2011.11.009 ↗
6. 10.1016/j.jallcom.2016.02.06510.1016/j.jallcom.2016.02.065 ↗
7. 10.1109/TCPMT.2016.261194210.1109/TCPMT.2016.2611942 ↗
8. 10.1016/j.matchar.2017.11.04310.1016/j.matchar.2017.11.043 ↗
9. 10.1016/j.microrel.2016.07.01310.1016/j.microrel.2016.07.013 ↗
10. 10.1007/s10854-015-2852-310.1007/s10854-015-2852-3 ↗
11. 10.1016/0925-8388(93)90273-P10.1016/0925-8388(93)90273-P ↗
12. 10.1016/0040-6090(93)90533-U10.1016/0040-6090(93)90533-U ↗
13. 10.1007/s10854-017-7932-010.1007/s10854-017-7932-0 ↗
14. 10.1007/s11664-005-0231-110.1007/s11664-005-0231-1 ↗
15. 10.1007/s12540-011-0202-410.1007/s12540-011-0202-4 ↗
16. 10.3969/j.issn.1005-023X.2013.11.00110.3969/j.issn.1005-023X.2013.11.001 ↗
17. Tokuriki H C L · 1983
18. Tokuriki H C L · 1993
19. Tokuriki H C L · 1990
20. 10.1016/j.msea.2007.03.05010.1016/j.msea.2007.03.050 ↗
21. 10.1007/s12598-011-0440-010.1007/s12598-011-0440-0 ↗
22. 10.1016/j.matchar.2009.06.00510.1016/j.matchar.2009.06.005 ↗
23. 10.3969/j.issn.1673-5196.2004.03.00310.3969/j.issn.1673-5196.2004.03.003 ↗
24. 10.1016/j.susc.2005.10.00910.1016/j.susc.2005.10.009 ↗
25. Hu H · Metal solidification principle. · 1991
26. 10.1016/j.scriptamat.2007.12.01310.1016/j.scriptamat.2007.12.013 ↗
27. 10.1088/0370-1301/64/9/303/meta10.1088/0370-1301/64/9/303/meta ↗
28. Petch N J · J Iron Steel Institute · 1953 · 174 · 25
29. 10.1007/BF0264723610.1007/BF02647236 ↗