Thermal deformation strengthening of WC-10Co4Cr coating prepared by high velocity air-fule process
Source abstract
Abstract
Abstract In this paper, WC-10Co4Cr coating was prepared on the surface of LC9 aluminum alloy by high velocity air-fule (HVAF) process. And a thermal deformation method was developed to enhance the coating properties. Experimental results show that, during the process of thermal deformation, the increase of temperature and deformation amount could improve the microhardness of coating surface. With temperature of 480 °C and deformation amount of 16% (0.8 mm), the microhardness reached the maximum value of 1349 HV0.3, which increased nearly 20% compared with that of specimen (1137 HV0.3) without compressive deformation. Besides, the strengthening effects of thermal deformation temperature and deformation amount on the bonding strength of coating were obvious. With deformation temperature of 450 °C and deformation amount of 8% (4 mm), the bonding strength reached the maximum critical load of 188 N, which was 17.5% higher than that of initial state.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced materials and composites · Metal and Thin Film Mechanics · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. Effect of external magnetic field on the microstructure and strength of laser-welded aluminum to titanium10.1007/s10853-019-04249-2 ↗
2. Interface morphology and microstructure of high power ultrasonic spot welded Mg/Al dissimilar joint10.1080/13621718.2018.1483598 ↗
3. Formation mechanism and fracture behavior in extra-filling refill friction stir spot weld for Al–Cu–Mg aluminum alloy10.1007/s10853-019-03940-8 ↗
4. Cerium in aluminum alloys10.1007/s10853-019-03892-z ↗
5. Microstructure and mechanical behaviour of CMT-welded Mg/Al dissimilar joint using Inconel 625 as filler metal10.1080/13621718.2019.1603186 ↗
6. Formation and effect of the branched layer during the tunnel etching of aluminum foil10.1007/s10853-019-03979-7 ↗
7. Influence of Ni interlayer width on interfacial reactions and mechanical properties in laser welding/brazing of Al/Mg lap joint10.1080/13621718.2019.1607487 ↗
8. Mechanism of intermetallic compound formation during the dissimilar friction stir welding of aluminum and steel10.1007/s10853-019-04106-2 ↗
9. Microstructure and deformation in the spray deposited Zn–22% Al alloy10.1016/j.msea.2006.06.019 ↗
10. The strengthening mechanism of spray forming Al–Zn–Mg–Cu alloy by underwater friction stir welding10.1016/j.matdes.2016.04.036 ↗
11. Improving the wear resistance of AA 6061 by laser surface alloying with NiTi10.1016/j.matlet.2007.01.016 ↗
12. Variation of structure with input energy during laser surface engineering of ceramic coatings on aluminum alloys10.1016/S0169-4332(02)00799-7 ↗
13. Influence of heat treatment and scandium addition on the electrochemical polarization behavior of Al–Zn–Mg–Cu–Zr alloy10.1007/s11661-007-9303-6 ↗
14. Investigation on the corrosion behaviour and microstructure of 2024-T3 Al alloy treated via plasma electrolytic oxidation10.1016/j.jallcom.2014.03.127 ↗
15. A pragmatic approach and quantitative assessment of silt erosion characteristics of HVOF and HVAF processed WC-CoCr coatings and 16Cr5Ni steel for hydro turbine applications10.1016/j.matdes.2017.06.046 ↗
16. High corrosion and wear resistance of Al-based amorphous metallic coating synthesized by HVAF spraying10.1016/j.jallcom.2017.11.274 ↗
17. Effect of shot peening on the oxidation behavior of thermal barrier coatings10.1016/j.apsusc.2015.06.113 ↗
18. Microstructure and wear behaviors of WC–12%Co coating deposited on ductile iron by electric contact surface strengthening10.1016/j.apsusc.2013.06.032 ↗
19. Effects of loads on friction–wear properties of HVOF sprayed NiCrBSi alloy coatings by laser remelting10.1016/j.jallcom.2017.02.171 ↗
20. In situ synthesized high volume fraction WC reinforced Ni-based coating by laser cladding10.1016/j.matlet.2017.02.076 ↗
21. Study on performance of isothermal oxidation of CoCrAlY coatings prepared by EB-PVD after surface compound shot peening process
22. Effects of laser remelting on wear resistance of Ni-WC composite coatings by flame-spraying10.3788/CJL20083502.0281 ↗