journal article·2021-02-01Open access

Research on the preparation method, microstructure and performance of hard silver plated/Cu-Cr0.6-Zr0.02 alloy contact

Xinghai Shao, Qianqian Yang, Yuan Liu, Molin Zhao, Biao Wang, Yu Xu, Yao Wang, Changle Zhang, Lei Cao

Materials Research Express· Volume 8· Issue 2

Abstract

Abstract This paper developed a new type of disconnect switch contact with high-conductivity, oxidation resistance and wear resistance. Contact material and preparation were researched. The Cu–Cr–Zr alloy was prepared by vacuum induction melting, then the plate was obtained after rolling and aging strengthening. Contact sample was formed by die stamping, at last, a wear-resistant coating/Cu–Cr–Zr alloy switch contact was manufactured, after the silver antimony alloy hard coating was electroplated on the surface. In order to further study the Cu–Cr–Zr alloy and hard silver coating of the contact, microstructure analysis and performance testing are carried out. A large number of nano-sized pure Cr phases were found to exist in the Cu–Cr–Zr alloy matrix, and the material conductivity was 76.3% IACS. Compared with T2 copper, its mechanical properties and oxidation resistance were significantly improved, which helped to delay the corrosion progress of the substrate after the coating disappeared. The hard silver coating contains 1% of the alloy element Sb. Compared with the silver coating, its wear resistance was increased by 135.30%. Cu–Cr–Zr alloy and hard silver plating technology are effective for improving strength, corrosion resistance and wear resistance of contact.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced materials and composites · Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. Effect of Al2O3 content and milling time on the properties of silver coated Cu matrix composites fabricated by electroless plating and hot pressing10.1016/j.mtcomm.2020.101153 ↗
2. The effect of flake-like morphology on the coating properties of silver coated copper particles fabricated by electroless plating10.1016/j.jallcom.2018.12.229 ↗
3. Microstructure evolution of Cu-1.0Co-0.65Si-0.1Ti alloy during hot deformation10.1016/j.vacuum.2020.109376 ↗
4. The synergistic effect of dilute alloying and nanostructuring of copper on the improvement of mechanical and tribological response10.1016/j.compositesb.2019.01.077 ↗
5. Microstructure and properties of Cu–Cr coatings deposited by cold spraying10.1016/j.vacuum.2019.109032 ↗
6. Synergistic effect between cavitation erosion and corrosion for various copper alloys in sulphide-containing 3.5% NaCl solutions10.1016/j.wear.2020.203258 ↗
7. Engineering prediction of fatigue strength for copper alloy netting structure by experimental method10.1016/j.aquaeng.2020.102087 ↗
8. Effect of Cr content on microstructure and oxidation resistance of laser-clad Cu–Ni–Fe–Mo-xCr alloy coating10.1016/j.surfcoat.2019.125316 ↗
9. Performance studies of Ag, Ag-graphite, and Ag-graphene coatings on Cu substrate for high-voltage isolation switch10.1002/maco.201810053 ↗
10. Solidification microstructure of Cu–Cr and Cu–Cr-In alloys
11. The synergistic effect of dilute alloying and nanostructuring of copper on the improvement of mechanical and tribological response10.1016/j.compositesb.2019.01.077 ↗
12. Energy of compressed aluminum foam10.1002/adem.200400164 ↗
13. Effect of ARB cycle number on cell morphology of closed-cell Al-Si alloy foam10.2320/matertrans.45.2389 ↗
14. Low cycle fatigue behavior of precipitation-strengthened Cu–Cr–Zr contact wires10.1016/j.ijfatigue.2020.105642 ↗
15. Calculation of the Cu–Cr–Zr alloy contact wire used in high-speed electrical railway10.4028/www.scientific.net/AMR.368-373.1165 ↗
16. Effect of processing and heat treatment on behavior of Cu–Cr–Zr alloys to railway contact wire10.1007/BF02586158 ↗
17. Microstructure and properties of rare earth-containing Cu–Cr–Zr alloy10.1016/S1003-6326(15)63717-7 ↗