Selective Laser Melting of Ti-6Al-4V Alloy: Correlation Between Processing Parameters, Microstructure and Corrosion Properties
Source abstract
Abstract
Additive Manufacturing technology has continually advanced, allowing microstructure and property optimization. In recent years, several studies have been carried out with the aim of understanding mechanisms of formation and evolution of the microstructure and, consequently, their influence on mechanical properties. However, correlations between microstructure and corrosion properties are not completely understood, making more systematic investigations necessary. In this work, samples of the Ti-6Al-4V alloy were produced by combining different laser powers and scanning speeds in order to generate different energy density values (VED) with subsequent microstructures and properties. The samples were characterized by optical and scanning electron microscopy, hardness and relative density. Complementarily, corrosion tests were carried out. For the entire set of parameters used, the processed samples showed the formation of acicular martensite α´, followed by different levels of porosity depending on the applied energy density. VED proved to be an important control parameter, and the best combinations of hardness and corrosion resistance were obtained for the parameter ratio that generated energy densities greater than 100 J/mm3.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Universidade Estadual de Campinas, Brasil
References (61)
Show source-provided references
1. An overview of the thermomechanical processing of α/β titanium alloys: current status and future research opportunities10.1007/s11661-020-05625-3 ↗
2. Recent development in beta titanium alloys for biomedical applications
3. Evolution of equiaxed and lamellar α during hot compression in a near alpha titanium alloy with bimodal microstructure10.1016/j.matchar.2019.03.005 ↗
4. Trends in dental implant use in the U.S., 1999-2016, and projections to 202610.1177/0022034518792567 ↗
5. 2020
6. Role of additive manufacturing applications towards environmental sustainability
7. Comparative environmental impacts of additive and subtractive manufacturing technologies10.1016/j.cirp.2016.04.036 ↗
8. Sustainability of additive manufacturing: measuring the energy consumption of the laser sintering process10.1177/0954405411406044 ↗
9. Sustainability-induced dual-level optimization of additive manufacturing process10.1007/s00170-016-8905-9 ↗
10. Energy consumption modeling of stereolithography-based additive manufacturing toward environmental sustainability10.1111/jiec.12589 ↗
11. Possibilities and limitations of titanium alloy additive manufacturing10.1051/matecconf/201822401064 ↗
12. The rise of 3-D printing: the advantages of additive manufacturing over traditional manufacturing10.1016/j.bushor.2017.05.011 ↗
13. Alloy design via additive manufacturing: advantages, challenges, applications and perspectives10.1016/j.mattod.2021.11.026 ↗
14. A comprehensive review on metallic implant biomaterials and their subtractive manufacturing10.1007/s00170-022-08770-8 ↗
15. The status, challenges, and future of additive manufacturing in engineering10.1016/j.cad.2015.04.001 ↗
16. Role of titanium in bio implants and additive manufacturing: an overview10.1016/j.matpr.2020.02.636 ↗
17. Biomedical applications of the powder‐based 3D printed titanium alloys: a review10.1016/j.jmst.2021.11.084 ↗
18. Design strategies for the process of additive manufacturing10.1016/j.procir.2015.01.082 ↗
19. Benefits of titanium additive manufacturing for industrial design development. Trends, limitations and applications
20. Current advances in additive manufacturing10.1016/j.procir.2020.05.076 ↗
21. Fracture testing of polymer materials processed via fused filament fabrication: a survey of materials, methods, and design applications10.1007/s40964-021-00196-0 ↗
22. The influence of bending mode ultrasonic-assisted friction stir welding of Al-6061-T6 alloy on residual stress, welding force and macrostructure10.1007/s00170-017-1431-6 ↗
23. Microstructure and mechanical behavior of Ti-6Al-4V produced by rapid-layer manufacturing, for biomedical applications10.1016/j.jmbbm.2008.05.004 ↗
24. The effects of hot isostatic pressing (HIP) and solubilization heat treatment on the density, mechanical properties, and microstructure of austenitic stainless steel parts produced by selective laser melting (SLM)10.1007/s00170-020-05072-9 ↗
25. A critical review on additive manufacturing of Ti-6Al-4V alloy: microstructure and mechanical properties10.1016/j.jmrt.2022.04.055 ↗
26. Additive manufacturing of martensitic stainless steel matrix composites with simultaneously enhanced strength-ductility and corrosion resistance10.1016/j.compositesb.2022.109745 ↗
27. Corrosion behavior of additively manufactured Ti-6Al-4V parts and the effect of post annealing
28. Additive manufacturing of corrosion-resistant maraging steel M789 by directed energy deposition
29. The effect of strain rate on stress corrosion performance of Ti6Al4V alloy produced by additive manufacturing process10.1016/j.jmrt.2020.02.035 ↗
30. Sercombe TB · 2018 · 303
31. Surface morphology, roughness, and corrosion resistance of dental implants produced by additive manufacturing10.1016/j.jmrt.2022.10.114 ↗
32. The tribological and corrosion properties of anodized Ti6Al4V/316L bimetallic structures manufactured by additive manufacturing
33. The anisotropic corrosion behaviour of wire arc additive manufactured Ti-6Al-4V alloy in 3.5% NaCl solution10.1016/j.corsci.2018.03.047 ↗
34. Effects of electropolishing on mechanical properties beam melting additive manufacturing10.3390/ma12091466 ↗
35. Direct laser deposition-additive manufacturing of Ti-15Mo alloy: effect of build orientation induced surface topography on corrosion and bioactivity10.1007/s12540-019-00464-3 ↗
36. Laser additive manufactured Ti-6Al-4V alloy: tribology and corrosion studies10.1007/s00170-017-0410-2 ↗
37. Corrosion assessment of Ti-6Al-4V fabricated using laser powder-bed fusion additive manufacturing10.1016/j.electacta.2018.04.189 ↗
38. Grain refinement of alloys in fusion-based additive manufacturing processes10.1007/s11661-020-05880-4 ↗
39. Material characterization and corrosion behavior of hybrid coating Ti−Al−Si−Cu/Ti−6Al-4V composite10.1002/mawe.202000019 ↗
40. Mechanical and corrosion properties of CoCrFeNiTi-based high-entropy alloy additive manufactured using selective laser melting
41. Review on corrosion characteristics of porous titanium alloys fabricated by additive manufacturing10.1007/s12204-021-2314-4 ↗
42. Evaluating corrosion resistance of biomedical Ti-6Al-4 V alloys fabricated via additive manufacturing using electrochemical critical localized corrosion potential10.1007/s12540-021-00972-1 ↗
43. 2013
44. Plugin for analysis of porous scaffolds used in tissue engineering10.5334/jors.bn ↗
45. Study on influence of porosity, pore size, spatial and topological distribution of pores on microhardness of as plasma sprayed ceramic coatings10.1016/j.msea.2006.09.042 ↗
46. Effect of processing parameters on pore structures, grain features, and mechanical properties in Ti-6Al-4V by laser powder bed fusion
47. Additive manufacturing of 316l stainless steel by selective laser melting
48. The effect of atmosphere on the structure and properties of a selective laser melted Al-12Si alloy10.1016/j.msea.2014.01.012 ↗
49. Selective laser melting of tungsten and tungsten alloys10.1016/j.ijrmhm.2017.12.005 ↗
50. Analysis of defect generation in Ti-6Al-4V parts made using powder bed fusion additive manufacturing processes
51. Quantification and prediction of lack-of-fusion porosity in the high porosity regime during laser powder bed fusion of Ti-6Al-4V10.1016/j.jmatprotec.2021.117426 ↗
52. The effect of SLM process parameters on density, hardness, tensile strength and surface quality of Ti-6Al-4V
53. Effect of the volume energy density and heat treatment on the defect, microstructure, and hardness of L-PBF inconel 62510.1007/s11661-020-05992-x ↗
54. Formation and control of martensite in Ti-6Al-4V alloy produced by selective laser melting10.1016/j.matdes.2016.06.117 ↗
55. Mechanical and corrosion behavior of titanium alloys additively manufactured by selective laser melting - a comparison between nearly β titanium, α titanium and α + β titanium10.1016/j.optlastec.2019.105625 ↗
56. Bandar A · 2002
57. Corrosion behavior of selective laser melted Ti-6Al-4 V alloy in NaCl solution10.1016/j.corsci.2015.10.041 ↗
58. Heat treatments effects on functionalization and corrosion behavior of Ti-6Al-4V ELI alloy made by additive manufacturing10.1016/j.jallcom.2018.06.319 ↗
59. Additive manufacturing of titanium-based alloys- a review of methods, properties, challenges, and prospects10.1016/j.heliyon.2022.e09041 ↗
60. Corrosion resistance improvement of additive manufactured scaffolds by anodizing10.1016/j.electacta.2020.137423 ↗
61. Corrosion of Ti6Al4V pins produced by direct metal laser sintering10.1016/j.apsusc.2016.10.031 ↗