Influence of Nanoxides on Diffusivity and Solubility of Hydrogen in Pd-based alloys
Source abstract
Abstract
The hydrogen interaction in palladium alloys with addition of Ce, Zr and Y was studied. These alloys are produced by arc-melting and then cold rolled into thin foils. Heat treatment at 800ºC for 24h in air atmosphere is applied to induce internal oxidation. Hydrogen permeation tests and TDS (Thermal Desorption Spectroscopy) are carried out to evaluate hydrogen interaction with three different microstructures which can be characterized by dislocations, substitutional atoms and nanoxides. For alloys argon annealed, Ce is the element that delays the most hydrogen diffusion, followed by Zr and Y. However alloys with yttrium nanoxides exhibit the highest solubility and the smallest diffusivity due to their small size, spherical shape and dispersion throughout the matrix. Analyzing TDS curves, it is shown that nanoxides are irreversible traps that improve hydrogen stored on palladium alloys. Dislocations and impurity atom on solid solution have little binding energy that detraps hydrogen at smaller temperatures.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Nuclear Materials and Properties · Hydrogen embrittlement and corrosion behaviors in metals · Hydrogen Storage and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Universidade Federal do Rio de Janeiro - UFRJ, Brazil
Instituto Federal de Educação Ciência e Tecnologia do Espírito Santo - IFES, Brasil
Universidade Federal do Rio de Janeiro - UFRJ, Brazil; Universidade Federal do Rio de Janeiro - UFRJ, Brazil
Universidade Federal Fluminense - UFF, Brazil
References (12)
Show source-provided references
1. Simulation of hydrogen trapping at defects in Pd10.1016/j.ijhydene.2009.02.048 ↗
2. Hydrogen diffusion in ultrafine-grained palladium: Roles of dislocations and grain boundaries10.1016/j.actamat.2016.01.069 ↗
3. Hydrogen environment embrittlement of an ODS RAF steel - Role of irreversible hydrogen trap sites10.1016/j.ijhydene.2010.06.071 ↗
4. Nature of hydrogen atom trapped inside palladium lattice10.1016/j.ijhydene.2010.03.117 ↗
5. Hydrogen segregation to internal interfaces of Pd-yttria composite prepared by internal oxidation of Pd-Y alloys10.1016/S0925-8388(01)01751-0 ↗
6. Study of an internally-oxidized Pd0.97Ce0.03 alloy10.1016/j.scriptamat.2006.01.039 ↗
7. The use of electrochemical hydrogen permeation techniques to detect hydride phase separation in amorphous metallic alloys10.1016/S0022-3093(98)00487-6 ↗
8. Hydrogen solubility in Pd/Al2O3 composites prepared by internal oxidation of Pd-Al alloys10.1016/S1359-6454(96)00255-8 ↗
9. Diffusivity of hydrogen in dilute alloys of copper and niobium in palladium10.1016/0001-6160(80)90056-5 ↗
10. Modeling of hydrogen trapping in the deformed Pd and Pd77Ag23 alloy10.1016/j.msea.2004.01.035 ↗
11. Transmission electron microscopy of hydrogen effects in internally oxidized palladium-chromium alloys10.1016/j.jallcom.2005.03.100 ↗
12. Hydrogen and oxygen at metal/oxide interfaces10.1016/0956-7151(91)90289-D ↗