Analysis of fracture toughness properties of wire + arc additive manufactured high strength low alloy structural steel components
Source abstract
Abstract
The uncertainty surrounding the fracture behaviour of CMT-WAAM deposited steel, in terms of crack tip condition (J and CTOD) needed to cause crack tip extension, has made this manufacturing technique unpopular to date. Fracture toughness parameters are crucial in the structural integrity assessment of components and structures in various industries for assessing the suitability of a manufacturing process and material. In the offshore wind industry, the EN-GJS-400-18-LT ductile cast grade for the mainframe and hub has lower fracture toughness resistance for its high strength grade. Its high weight level affects the Eigen frequency of the tower and imposes high installation cost incurred from heavy lifting equipment usage. Poor fracture toughness is currently a challenge for wind turbine manufacturers in the quest for a cleaner and cheaper energy in the form of offshore wind. In this study, CMT-WAAM is used in depositing steel components with an oscillatory and single pass deposition strategy. The effects of microstructural variation, as a result of layer by layer deposition and the layer band spacing, on the fracture resistance in the build and welding direction was shown here. The fracture mechanics and failure mode of the WAAM deposited parts were investigated. The microstructural variation, again as a result of the layer by layer deposition and the layer band spacing, are the key parameters that control the fracture toughness of WAAM steel. Anisotropic behaviour in the Jq values was observed between both fracture orientations. The constructive transformation mechanism of the WAAM oscillatory process made way for intragranular nucleation of acicular ferrite on the Ti containing inclusion, thereby improving the toughness of the ER70S-6 deposit with a unique microstructure and Jq value of 640kJ/m2.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Ductile iron for heavy section wind mill castings: an European experience
2. The Crown Estate · 2016
3. Large scale axial fatigue testing of ductile cast iron for heavy section wind turbine components10.1016/j.engfailanal.2011.05.005 ↗
4. Fatigue life distribution and size effect in ductile cast iron for wind turbine components10.1016/j.engfailanal.2010.07.001 ↗
5. Patel · 2012 · 171
6. Influence of alloying elements on the mechanical properties of high-strength weld metal10.1080/13621718.2016.1274095 ↗
7. The physical metallurgy of HSLA linepipe steels—a review10.1007/BF03338239 ↗
8. The evolution of HSLA steels10.1007/BF03337994 ↗
9. Thermodynamic study of inclusion formation in low alloy steel weld metals10.1179/stw.1997.2.2.65 ↗
10. The role of molybdenum additions and prior deformation on acicular ferrite formation in microalloyed Nb-Ti low-carbon line-pipe steels10.1016/j.matchar.2007.06.001 ↗
11. Influence of acicular ferrite and bainite microstructures on toughness for an ultra-low-carbon alloy steel weld metal10.1007/BF00506341 ↗
12. Structure-property relationships in bainitic steels10.1007/BF02672567 ↗
13. A study on the relationship between microstructure and mechanical properties of acicular ferrite and upper bainite10.1016/j.msea.2016.03.103 ↗
14. On the toughness scatter in low alloy C-Mn steel samples fabricated using wire arc additive manufacturing10.1016/j.msea.2017.11.101 ↗
15. Effect of Ti-containing inclusions on the nucleation of acicula10.1016/j.micron.2012.11.004 ↗
16. In pursuit of optimum welding system design for steels10.1179/1362171811Y.0000000019 ↗
17. The effects of thermo-mechanical control process on microstructures and mechanical properties of a commercial pipeline steel10.1016/S0921-5093(01)01904-9 ↗
18. In situ TEM study of the effect of M/A films at grain boundaries on crack propagation in an ultra-fine acicular ferrite pipeline steel10.1016/j.actamat.2005.09.015 ↗
19. Microstructural evolution and mechanical properties of maraging steel produced by wire + arc additive manufacture process10.1016/j.matchar.2017.12.002 ↗
20. Improving mechanical properties of wire plus arc additively manufactured maraging steel through plastic deformation enhanced aging response10.1016/j.msea.2018.12.114 ↗
21. Wire + Arc Additive Manufacture of 17-4 PH stainless steel: effect of different processing conditions on microstructure, hardness, and tensile strength10.1016/j.jmatprotec.2019.01.007 ↗
22. Acta Materialia on the origin of microstructural banding in Ti-6Al4V wire-arc based high deposition rate additive manufacturing10.1016/j.actamat.2018.12.038 ↗
23. Wire and arc additive manufactured steel: tensile and wear properties10.1016/j.addma.2017.05.010 ↗
24. Wire and arc additive manufacturing of HSLA steel: effect of thermal cycles on microstructure and mechanical properties10.1016/j.addma.2019.03.029 ↗
25. Chen · 2013 · 1
26. Underwood · 1976 · vol. 601 · 312
27. Effectiveness of cold metal transfer process for welding 7075 aluminium alloys10.1179/1362171815Y.0000000017 ↗
28. Effect of nickel and molybdenum additions on weld metal toughness in a submerged arc welded HSLA line-pipe steel
29. The formation of austenite in a low alloy steel10.1007/BF02700436 ↗
30. Sindo · 2003
31. Mechanisms and modeling of cleavage fracture in simulated heat-affected zone microstructures of a high-strength low alloy steel10.1007/s11661-004-1007-6 ↗
32. The mechanism of acicular ferrite in weld deposits10.1016/j.cossms.2004.10.001 ↗
33. Fracture toughness and fatigue crack growth rate properties in wire + arc additive manufactured Ti-6Al-4V10.1111/ffe.12547 ↗
34. Microstructure of interpass rolled wire + arc additive manufacturing Ti-6Al-4V components10.1007/s11661-015-3172-1 ↗
35. Effect of the welding thermal cycles on the structural changes in the heat affected zone and on its properties in joints welded in low-alloy steels10.1080/09507110009549281 ↗
36. Energy input effect on morphology and microstructure of selective laser melting single track from metallic powder10.1016/j.jmatprotec.2012.11.014 ↗
37. Steady state columnar and equiaxed growth of dendrites and eutectic10.1016/0025-5416(84)90201-5 ↗
38. Characterization of wire arc additive manufacturing 2Cr13 part: process stability, microstructural evolution, and tensile properties10.1016/j.jallcom.2018.03.222 ↗
39. Non-metallic inclusion and intragranular nucleation of ferrite in Ti-killed C – Mn steel10.1016/S1359-6454(02)00560-8 ↗
40. Embrittlement of 2-1/4Cr-1Mo steel weld metal by postweld heat treatment
41. Influence of microstructural variations in the weldment on the high-temperature corrosion of 2 . 25Cr-1Mo steel10.1007/BF02670772 ↗
42. Relation between inclusion surface and acicular ferrite in low carbon low alloy steel weld10.2355/isijinternational.49.1059 ↗
43. On the role of non-metallic inclusions in the nucleation of acicular ferrite in steels10.2355/isijinternational.49.1063 ↗
44. Effect of TiO2-containing fluxes on the mechanical properties and microstructure in submerged-arc weld steels10.1016/j.matchar.2008.06.003 ↗
45. Kou · 2003
46. Influence of Ti on non-metallic inclusion formation and acicular ferrite nucleation in high-strength low-alloy steel weld metals10.1007/s12540-014-1013-1 ↗
47. Role of inclusions in formation of high strength steel weld metal microstructures10.1179/1362171813Y.0000000138 ↗