Effect of heat treatment on microstructure evolution and mechanical properties of selective laser melted Ti–6Al–4V and TiB/Ti–6Al–4V composite: A comparative study
Source abstract
Abstract
Abstract Post heat treatment has been considered as an essential process to relieve residual stress, tailor the microstructure and obtain desired mechanical properties of the parts manufactured by selective laser melting (SLM) technology. The present work comparatively investigated the effect of heat treatment on microstructure evolution and mechanical properties of the SLM-fabricated Ti–6Al–4V alloy (Ti64) and 2 vol% TiB/Ti–6Al–4V titanium matrix composite (TMC). Microstructure analysis indicated that the as-built and heat treated TMC samples showed profoundly different microstructures compared to that of Ti64 samples. With heat treatment temperature increasing, the dominant acicular α′ martensite of Ti64 was decomposed into fine (α+β) lamella and microstructure coarsening occurred. A finer (α+β) dual-phase matrix microstructure, compared to that of Ti64, was achieved for TMC samples when heat treatment temperature exceeded 850 °C. The densely dispersed clusters of parallel nanoscale TiB precipitates of the TMC grew into individually separate TiB whiskers with larger nanoscale and sub-microscale size through a stacking up process of (100) planes based on an Ostwald ripening process. Mechanical testing results showed that the hardness and yield strength values of TMC samples before and after heat treatment were all higher than that of the Ti64 samples. A superior comprehensive mechanical performance with relatively high yield strength (1345 MPa) and significantly improved fracture strain from 17.6% to 31.3% was achieved for the TMC sample after heat treatment at 850 °C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Titanium metal matrix composites: An overview10.1016/j.compositesa.2019.04.005 ↗
2. Review: titanium-titanium boride composites10.1007/s10853-018-03283-w ↗
3. Spark plasma sintering of functionally graded material in the Ti-TiB2-B system10.1016/j.msea.2005.02.003 ↗
4. Processing-structure-property aspects of particulate- and whisker-reinforced titanium matrix composites10.1016/j.compscitech.2007.07.016 ↗
5. Selective laser melting of titanium Alloys and titanium matrix composites for biomedical Applications: A review10.1002/adem.201500419 ↗
6. Laser powder bed fusion for metal additive manufacturing: perspectives on recent developments10.1080/17452759.2020.1779999 ↗
7. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
8. Review of selective laser melting: materials and applications10.1063/1.4935926 ↗
9. Densification behavior, microstructure evolution, and wear performance of selective laser melting processed commercially pure titanium10.1016/j.actamat.2012.04.006 ↗
10. Microstructure and tensile properties of selectively laser-melted and of HIPed laser-melted Ti–6Al–4V10.1016/j.msea.2013.04.099 ↗
11. Particle-reinforced metal matrix nanocomposites fabricated by selective laser melting: A state of the art review10.1016/j.pmatsci.2019.04.006 ↗
12. Nanocrystalline TiC reinforced Ti matrix bulk-form nanocomposites by Selective Laser Melting (SLM): densification, growth mechanism and wear behavior10.1016/j.compscitech.2011.07.010 ↗
13. Selective laser melting of in situ titanium-titanium boride composites: processing, microstructure and mechanical properties10.1016/j.actamat.2014.05.022 ↗
14. Additive manufacturing of strong and ductile Ti-6Al-4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
15. In-situ residual stress reduction, martensitic decomposition and mechanical properties enhancement through high temperature powder bed pre-heating of Selective Laser Melted Ti6Al4V10.1016/j.msea.2017.04.033 ↗
16. Microstructure evolution and mechanical properties of selective laser melted bulk-form titanium matrix nanocomposites with minor B4C additions10.1016/j.matdes.2019.108245 ↗
17. On the role of different annealing heat treatments on mechanical properties and microstructure of selective laser melted and conventional wrought Ti-6Al-4V10.1108/RPJ-02-2016-0022 ↗
18. Heat treatment of Ti6Al4V produced by selective laser melting: microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
19. Effect of subtransus heat treatment on the microstructure and mechanical properties of additively manufactured Ti-6Al-4V alloy10.1016/j.jallcom.2017.11.263 ↗
20. Selective laser melting of TiC/Ti bulk nanocomposites: influence of nanoscale reinforcement10.1016/j.scriptamat.2012.04.013 ↗
21. Effect of TiB2 addition on the microstructure and wear resistance of Ti-6Al-4V alloy fabricated through direct metal laser sintering (DMLS)10.1016/j.jallcom.2018.10.308 ↗
22. A study of the microstructural evolution during selective laser melting of Ti–6Al–4V10.1016/j.actamat.2010.02.004 ↗
23. Cyclic plasticity and microstructure of as-built SLM Ti-6Al-4V: the effect of build orientation10.1016/j.msea.2017.06.069 ↗
24. Controlling martensitic decomposition during selective laser melting to achieve best ductility in high strength Ti-6Al-4V10.1016/j.msea.2018.12.047 ↗
25. In-situ preparation and formation of TiB/Ti-6Al-4V nanocomposite via laser additive manufacturing: microstructure evolution and tribological behavior10.1016/j.powtec.2018.09.088 ↗
26. Microstructure and mechanical properties of in situ TiB reinforced titanium matrix composites based on Ti–FeMo–B prepared by spark plasma sintering10.1016/j.compscitech.2004.05.013 ↗
27. Effect of boron concentration on martensitic transformation temperatures, stress for inducing martensite and slip stress of Ti-24 mol%Nb-3 mol%Al superelastic Alloy10.2320/matertrans.48.407 ↗
28. Effect of β heat treatment temperature on microstructure and mechanical properties of in situ titanium matrix composites10.1016/j.matdes.2010.04.003 ↗
29. Effects of heat treatments on the microstructure and mechanical properties of as-extruded TiBw/Ti6Al4V composites10.1016/j.msea.2012.08.071 ↗
30. Direct laser deposition of in situ Ti–6Al–4V–TiB composites10.1016/S0921-5093(03)00299-5 ↗
31. Growth mechanism of in situ TiB whiskers in spark plasma sintered TiB/Ti metal matrix composites10.1021/cg050443k ↗
32. Physical stability of nanosuspensions: investigation of the role of stabilizers on Ostwald ripening10.1016/j.ijpharm.2010.12.027 ↗
33. As-fabricated and heat-treated microstructures of the Ti-6Al-4V Alloy processed by selective laser melting10.1007/s11661-011-0731-y ↗
34. Effect of nano-yttria stabilized zirconia addition on the microstructure and mechanical properties of Ti6Al4V parts manufactured by selective laser melting10.1016/j.matdes.2019.107909 ↗