journal article·2018-08

Dissimilar welding between Ti–6Al–4V and 17-4PH stainless steel using a vanadium interlayer

Nana Kwabena Adomako, Jeng O. Kim, Se Hwan Lee, Kyung-Ho Noh, Jeoung Han Kim

Publisher page

Abstract

Abstract In this study, electron beam welding, continuous laser welding, and pulsed laser welding were used to join Ti–6Al–4V alloy and 17-4PH stainless steel with a 1 mm pure V sheet interlayer. In addition, the effect of V composition on the mechanical properties of the welded joint by shifting the laser towards the 17-4PH was examined. Vanadium bonded well with Ti, and the weld metal was characterized by a (βTi,V) solid solution. In the V–steel welded joint, similar phases ((Fe,V)ss) but with different compositions were found in the MZs, which affected the mechanical properties. The cracked region was visible at the V–steel interface of the pulsed-laser-welded joint and contributed to its low tensile strength. Electron beam welding showed a good intact joint with no defects, and failure occurred in the vanadium interlayer. A common MZ was created for the three metals in EB1, which formed Fe2Ti and FeTi intermetallic compounds that acted as crack initiation sites and led to the failure of the welded joint during machine processing. Variation in V composition had a significant impact on the mechanical properties of the welded joints. Hardness increased incrementally with the V concentration, and joints with a composition of less than 35 at% V, which corresponded to α-Fe + (Fe,V)σ and α-Fe phase formation ranges, had better tensile properties than those with more than 35 at% V, which corresponded to the single (Fe,V)σ phase. However, care should be taken in regulating the laser beam in order to avoid a very low V content, since this could lead to the formation of unfused regions.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Welding Techniques and Residual Stresses · Hydrogen embrittlement and corrosion behaviors in metals · Additive Manufacturing Materials and Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Mechanical properties of titanium-based Ti–6Al–4V alloys manufactured by powder bed additive manufacture10.1080/02670836.2016.1172787 ↗
2. (Gerd) Lütjering · 2007
3. Dissimilar welding of titanium alloys to steels
4. Stainless steel to titanium bimetallic structure using LENS™10.1016/j.addma.2014.10.002 ↗
5. Fabrication and characterization of a functionally graded material from Ti-6Al-4 V to SS316 by laser metal deposition10.1016/j.addma.2016.12.006 ↗
6. Effect of bonding temperature on the microstructure and mechanical properties of Ti-6Al-4V to AISI 304 transient liquid phase bonded joint10.1016/j.matdes.2016.03.101 ↗
7. Interlayer engineering for dissimilar bonding of titanium to stainless steel10.1016/j.matlet.2010.02.024 ↗
8. Influence of vanadium filler on the properties of titanium and steel TIG welded joints10.1016/j.jmatprotec.2016.06.018 ↗
9. The Fe-V (iron-vanadium) system10.1007/BF02868958 ↗
10. Phase transformations in alloys of the Fe-V system10.1016/j.jallcom.2005.02.030 ↗
11. Study on electron beam weld joints between pure vanadium and SUS316L stainless steel10.1016/j.jnucmat.2013.01.300 ↗
12. High strength electron beam welded titanium-stainless steel joint with V/Cu based composite filler metals10.1016/j.vacuum.2013.01.015 ↗
13. Dissimilar laser welding of AISI 316L stainless steel to Ti6-Al4–6V alloy via pure vanadium interlayer10.1016/j.msea.2014.10.084 ↗
14. Preparation of V-Ti-Fe master alloys by metallothermic reduction method10.1016/S1003-6326(11)61348-4 ↗
15. Assessment of precipitates of aged Ti-6Al-4V alloy by ultrasonic attenuation10.1080/14786435.2016.1244359 ↗
16. Mechanism of sigma-phase formation in the Fe-V system10.1007/s10789-005-0219-5 ↗
17. Low temperature diffusion bonding of Ti-6Al-4V and duplex stainless steel10.1016/j.jmatprotec.2016.03.013 ↗
18. Massalski · 1990
19. Titanium-vanadium binary alloy phase diagram10.1007/BF02664864 ↗
20. Electron beam welding, laser beam welding and gas tungsten arc welding of titanium sheet10.1016/S0921-5093(99)00662-0 ↗
21. Comparison of Ti-5Al-5V-5Mo-3Cr welds performed by laser beam, electron beam and gas tungsten arc welding10.1016/j.proeng.2013.08.202 ↗
22. Introduction to high energy density electron and laser beam welding
23. Iron-Vanadium (Fe-V) Phase Diagram, (n.d.). 〈http://www.calphad.com/iron-vanadium.html〉.
24. Sigma-phase in Fe-Cr and Fe-V alloy systems and its physical properties10.1080/10408436.2011.589232 ↗
25. Effects of temporal pulse shaping on cracking susceptibility of 6061-T6 aluminum Nd: YAG laser welds
26. On the weldability, composition, and hardness of pulsed and continuous Nd:YAG laser welds in aluminum alloys 6061,5456, and 508610.1007/BF02654217 ↗
27. Hot cracking in laser welding of Hastelloy X with pulsed Nd:YAG and continuous wave fiber lasers10.1016/j.matdes.2016.05.124 ↗
28. Solidification behavior and cracking susceptibility of pulsed-laser welds in austenitic stainless steels
29. A study of the mechanism of laser welding defects in low thermal expansion superalloy GH90910.1016/j.matchar.2013.01.008 ↗
30. The liquation cracking behavior of IN738LC superalloy during low power Nd:YAG pulsed laser welding10.1016/j.matchar.2012.02.019 ↗
31. Heat input and the liquation cracking of laser welded IN738LC superalloy