Ambient- and elevated temperature properties of Sc- and Zr-modified Al–6Ni alloys strengthened by Al3Ni microfibers and Al3(Sc,Zr) nanoprecipitates

C. Suwanpreecha, J.U. Rakhmonov, S. Chankitmunkong, P. Pandee, D.C. Dunand, C. Limmaneevichitr

Abstract

The eutectic Al-6Ni (wt.%) alloy exhibits excellent strength at ambient and elevated temperature, provided by a high volume fraction of Al3Ni microfibers formed during solidification. Here, Al-6Ni is micro-alloyed with Sc and Zr (with 0.1Sc+0.2Zr, 0.2Sc+0.4Zr and 0.3Sc+0.2Zr, wt.%), creating two additional populations of primary and secondary Al3(Sc,Zr) precipitates. The fully eutectic microstructure (α-Al + Al3Ni) observed in Al-6Ni alloy changes, with Sc and Zr addition to hypoeutectic microstructure with primary α-Al grains nucleated on solidification by primary Al3(Sc,Zr) precipitates. Upon subsequent aging, fully-coherent Al3(Sc,Zr) nano-precipitates form in the α-Al matrix between Al3Ni microfibers, providing substantial precipitation strengthening, which is maintained for up to 1 month at 350 °C. Alloy strength - both at ambient temperature and during creep at 300 °C - can be quantitatively described through a superposition of precipitation strengthening by Al3(Sc,Zr) nanoprecipitates and load-transfer strengthening by Al3Ni microfibers.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (76)

Show source-provided references
1. Scandium in aluminium alloys10.1179/174328005X14311 ↗
2. Sustainability through alloy design: challenges and opportunities
3. Double-shell structure of Al3(Zr,Sc) precipitate induced by thermomechanical treatment of Al–Zr–Sc alloy cable10.1016/j.jre.2018.08.009 ↗
4. Criteria for developing castable, creep-resistant aluminum-based alloys – a review10.3139/146.101249 ↗
5. Precipitation evolution in Al–Zr and Al–Zr–Ti alloys during aging at 450–600 °C10.1016/j.actamat.2007.11.011 ↗
6. Significantly improved particle strengthening of Al–Sc alloy by high Sc composition design and rapid solidification10.1016/j.msea.2020.140304 ↗
7. Microstructural evolution and mechanical property of Al–Zr and Al–Zr–Y alloys10.1016/j.msea.2014.08.017 ↗
8. Chapter 12 - aluminium scandium alloys
9. Mechanical properties of Al(Sc,Zr) alloys at ambient and elevated temperatures10.1016/S1359-6454(03)00320-3 ↗
10. Precipitation of Al3Sc in binary Al–Sc alloys10.1016/S0921-5093(01)01326-0 ↗
11. Kinetics and mechanisms of precipitation in an Al–0.2 wt.% Sc alloy10.1016/j.msea.2005.02.015 ↗
12. The Al-Sc (aluminum-scandium) system10.1361/105497198770342120 ↗
13. New generation of eutectic Al-Ni casting alloys for elevated temperature services10.1016/j.msea.2017.10.034 ↗
14. Constitution and age hardening of Al-Sc alloys10.1007/BF00553049 ↗
15. Diffusion coefficients of some solutes in fcc and liquid Al: critical evaluation and correlation10.1016/S0921-5093(03)00624-5 ↗
16. A study of coarsening, recrystallization, and morphology of microstructure in Al-Sc-(Zr)-(Mg) alloys10.1007/s11661-004-0135-3 ↗
17. Temporal evolution of the nanostructure of Al(Sc,Zr) alloys: Part II-coarsening of Al3(Sc1−xZrx) precipitates10.1016/j.actamat.2005.08.015 ↗
18. Segregation in Al3(Sc,Zr) precipitates in Al–Sc–Zr alloys10.1016/j.scriptamat.2004.11.021 ↗
19. Investigation of alloys of the Al-Sc-Zr system in the aluminium-rich range
20. Temporal evolution of the nanostructure of Al(Sc,Zr) alloys: Part I – chemical compositions of Al(ScZr) precipitates10.1016/j.actamat.2005.08.016 ↗
21. Toropova · 1998
22. Micro-segregation and precipitates in as-solidified Al-Sc-Zr-(Mg)-(Si)-(Cu) alloys10.1016/j.matchar.2019.06.021 ↗
23. Correlation between precipitates evolution and mechanical properties of Al-Sc-Zr alloy with Er additions10.1016/j.jmst.2021.05.031 ↗
24. Effect of Sc and Zr additions on the microstructure/strength of Al-Cu binary alloys10.1016/j.msea.2017.09.032 ↗
25. Improving aging and creep resistance in a dilute Al–Sc alloy by microalloying with Si, Zr and Er10.1016/j.actamat.2013.10.008 ↗
26. Scandium-enriched nanoprecipitates in aluminum providing enhanced coarsening and creep resistance
27. Thermal stability of aluminum-nickel binary alloys containing the Al-Al3Ni eutectic10.1007/s11661-021-06372-9 ↗
28. Cast near-eutectic Al-12.5 wt% Ce alloy with high coarsening and creep resistance10.1016/j.msea.2019.138440 ↗
29. Strengthening mechanisms in AlNiSc alloys containing Al3Ni microfibers and Al3Sc nanoprecipitates10.1016/j.actamat.2018.10.059 ↗
30. The effect of introducing the Al–Ni eutectic composition into Al–Zr–V alloys on microstructure and tensile properties10.1016/j.msea.2015.12.044 ↗
31. An alternative eutectic system for casting aluminum alloys II. Modification of the eutectic morphology
32. The Al-Al3Ni eutectic reaction: crystallography and mechanism of formation10.1007/s11661-015-3051-9 ↗
33. Effects of Zr Additions on Structure and Microhardness Evolution of Eutectic Al-6Ni Alloy
34. Isothermal aging of Al-Ni-Sc alloy containing Al3Ni microfibers and Al3Sc nanoprecipitates
35. Alternatives to the Al–Si eutectic system in aluminum casting alloys10.1007/s40962-016-0042-6 ↗
36. Precipitation strengthening in Al-Ni-Mn alloys10.1007/s11661-015-3119-6 ↗
37. Laser powder bed fusion of eutectic Al–Ni alloys: experimental and phase-field studies10.1016/j.matdes.2020.109299 ↗
38. Tensile properties of hypoeutectic Al-Ni alloys: experiments and FE simulations10.1016/j.jallcom.2021.161664 ↗
39. Al-Ni (aluminum-nickel)10.1007/s11669-004-0163-0 ↗
40. Improving the properties of cold-rolled Al–6%Ni sheets by alloying and heat treatment10.1016/j.scriptamat.2003.09.033 ↗
41. Additive manufacturing of high-strength eutectic aluminium-nickel alloys–Processing and mechanical properties10.1016/j.jmatprotec.2021.117315 ↗
42. A high-strength heat-resistant Al− 5.7 Ni eutectic alloy with spherical Al3Ni nano-particles by selective laser melting10.1016/j.scriptamat.2021.114034 ↗
43. Design of heterogeneous structured Al alloys with wide processing window for laser-powder bed fusion additive manufacturing
44. Strengthening mechanisms in aluminum containing coherent Al3Sc precipitates and incoherent Al2O3 dispersoids10.1016/j.actamat.2006.10.004 ↗
45. Michi
46. On the origin of a remarkable increase in strength and stability of an Al rich Al-Ni eutectic alloy by Zr addition10.1016/j.actamat.2019.03.025 ↗
47. Solidification and precipitation in aluminium-zirconium alloys. Pt. 1
48. The solidification behaviour of dilute aluminium–scandium alloys10.1016/S1359-6454(98)00257-2 ↗
49. Precipitation evolution in Al–0.1Sc, Al–0.1Zr and Al–0.1Sc–0.1Zr (at.%) alloys during isochronal aging10.1016/j.actamat.2010.05.054 ↗
50. Effect of Sc, Zr grain refiner on the microstructure and mechanical properties of pure aluminum10.4028/www.scientific.net/AMM.508.16 ↗
51. Handbook · 1990 · 2 · 713
52. The grain refinement of 1070 alloy by different Al-Ti-B mater alloys and its influence on the electrical conductivity10.1016/j.rinp.2019.102482 ↗
53. Effect of Er additions on ambient and high-temperature strength of precipitation-strengthened Al–Zr–Sc–Si alloys10.1016/j.actamat.2012.02.030 ↗
54. Role of silicon in the precipitation kinetics of dilute Al-Sc-Er-Zr alloys10.1016/j.msea.2016.09.065 ↗
55. Ambient- and elevated-temperature strengthening by Al3Zr-Nanoprecipitates and Al3Ni-Microfibers in a cast Al-2.9Ni-0.11Zr-0.02Si-0.005Er (at.%) alloy10.1016/j.msea.2019.05.018 ↗
56. The kinetics of dislocation climb over hard particles—II. Effects of an attractive particle-dislocation interaction10.1016/0001-6160(88)90159-9 ↗
57. Threshold stresses for dislocation climb over hard particles: the effect of an attractive interaction10.1016/0001-6160(86)90247-6 ↗
58. Frost · 1982
59. Roles of impurities on precipitation kinetics of dilute Al–Sc alloys10.1016/j.msea.2010.02.027 ↗
60. Role of silicon in accelerating the nucleation of Al3(Sc,Zr) precipitates in dilute Al–Sc–Zr alloys10.1016/j.actamat.2012.05.036 ↗
61. Role of silicon in the precipitation kinetics of dilute Al-Sc-Er-Zr alloys10.1016/j.msea.2016.09.065 ↗
62. On the origin of a remarkable increase in the strength and stability of an Al rich Al-Ni eutectic alloy by Zr addition10.1016/j.actamat.2019.03.025 ↗
63. Microstructure and creep properties of cast near-eutectic Al–Ce–Ni alloys10.1016/j.msea.2021.142551 ↗
64. On the additivity of solid solution and dispersion strengthening10.1016/S0921-5093(01)00937-6 ↗
65. Effect of Mg addition on the creep and yield behavior of an Al–Sc alloy10.1016/S1359-6454(03)00288-X ↗
66. Kocks · 1975 · 19
67. The effect of prestressing on the strength of neutron‐irradiated copper single crystals10.1063/1.1753962 ↗
68. Precipitation strengthening at ambient and elevated temperatures of heat-treatable Al(Sc) alloys10.1016/S1359-6454(02)00201-X ↗
69. Ambient- and high-temperature mechanical properties of isochronally aged Al–0.06Sc, Al–0.06Zr and Al–0.06Sc–0.06Zr (at.%) alloys10.1016/j.actamat.2010.10.017 ↗
70. Modeling the creep threshold stress due to climb of a dislocation in the stress field of a misfitting precipitate10.1016/j.actamat.2011.04.044 ↗
71. Model for creep threshold stress in precipitation-strengthened alloys with coherent particles10.1016/S1359-6462(02)00165-3 ↗
72. Effect of Si micro-addition on creep resistance of a dilute Al-Sc-Zr-Er alloy10.1016/j.msea.2018.07.053 ↗
73. Creep of metal matrix composites reinforced by combining nano-sized dispersoids with micro-sized ceramic particulates or whiskers10.1504/IJMPT.2003.003593 ↗
74. Creep strengthening in a discontinuous SiC-Al composite10.1007/BF02669441 ↗
75. A unified interpretation of threshold stresses in the creep and high strain rate superplasticity of metal matrix composites10.1016/S1359-6454(99)00219-0 ↗
76. Finite element modeling of creep deformation in dendritic alloys10.1016/j.msea.2021.142171 ↗