journal article·2023-04

Laser powder bed fusion of oxidized microscale SiC-particle-reinforced AlSi10Mg matrix composites: Microstructure, porosity, and mechanical properties

Yan Chen, Yongming Ren, Kan Li, Bo Dang, Zengyun Jian

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (62)

Show source-provided references
1. Progress in structural materials for aerospace systems10.1016/j.actamat.2003.08.023 ↗
2. Fine-structured aluminium products with controllable texture by selective laser melting of pre-alloyed AlSi10Mg powder10.1016/j.actamat.2012.11.052 ↗
3. Particle-reinforced metal matrix nanocomposites fabricated by selective laser melting: a state of the art review10.1016/j.pmatsci.2019.04.006 ↗
4. Microstructural and mechanical characteristics of in situ metal matrix composites10.1016/S0927-796X(00)00024-3 ↗
5. On the breakdown of SiC during the selective laser melting of aluminum matrix composites10.1002/adem.201600835 ↗
6. Microstructure and mechanical properties of SiCnp/Al6082 aluminum matrix composites prepared by squeeze casting combined with stir casting
7. Properties of P/M processed particle reinforced metal matrix composites specified by reinforcement concentration and matrix-to-reinforcement particle size ratio10.1016/j.actamat.2005.08.036 ↗
8. Microstructure and strength of selectively laser melted AlSi10Mg10.1016/j.actamat.2016.07.012 ↗
9. Material-structure-performance integrated laser-metal additive manufacturing10.1126/science.abg1487 ↗
10. Developing a high-strength Al-Mg-Si-Sc-Zr alloy for selective laser melting: crack-inhibiting and multiple strengthening mechanisms10.1016/j.actamat.2020.03.060 ↗
11. Effect of process parameters on the density and porosity of laser melted AlSi10Mg/SiC metal matrix composite10.1007/s11465-018-0521-y ↗
12. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
13. Rapid fabrication of Al-based bulk-form nanocomposites with novel reinforcement and enhanced performance by selective laser melting10.1016/j.scriptamat.2014.10.011 ↗
14. Laser additive manufacturing of carbon nanotubes (CNTs) reinforced aluminum matrix nanocomposites: processing optimization, microstructure evolution and mechanical properties
15. A novel method to 3D-print fine-grained AlSi10Mg alloy with isotropic properties via inoculation with LaB6 nanoparticles
16. Selective laser melting of nano-TiB2 decorated AlSi10Mg alloy with high fracture strength and ductility10.1016/j.actamat.2017.02.062 ↗
17. Achieving simultaneously improved tensile strength and ductility of a nano-TiB2/AlSi10Mg composite produced by cold spray additive manufacturing10.1016/j.compositesb.2020.108404 ↗
18. Fatigue behavior of in-situ TiB2/7050Al metal matrix composites: fracture mechanisms and fatigue life modeling after milling10.1016/j.ijfatigue.2020.105698 ↗
19. Simultaneous enhancement of strength, ductility, and hardness of TiN/AlSi10Mg nanocomposites via selective laser melting
20. Simultaneously improving the tensile strength and ductility of the AlNp/Al composites by the particle's hierarchical structure with bimodal distribution and nano-network10.1016/j.msea.2019.138519 ↗
21. Laser powder-bed-fusion of Si3N4 reinforced AlSi10Mg composites: processing, mechanical properties and strengthening mechanisms10.1016/j.msea.2021.141874 ↗
22. LPBF-processed Sc- and Zr- modified Al-Mg alloy: mechanical properties and microstructural effects of heat treatment10.1016/j.msea.2017.06.089 ↗
23. Making selective-laser-melted high-strength Al–Mg–Sc–Zr alloy tough via ultrafine and heterogeneous microstructure10.1016/j.scriptamat.2021.114052 ↗
24. Effect of SiC particle size on densification behavior and mechanical properties of SiCp/AlSi10Mg composites fabricated by laser powder bed fusion10.1016/j.jallcom.2020.156260 ↗
25. Microstructure evolution and properties of nanoparticulate SiC modified AlSi10Mg alloys10.1016/j.msea.2021.140864 ↗
26. Selective laser melting of in-situ Al4SiC4 + SiC hybrid reinforced Al matrix composites: influence of starting SiC particle size10.1016/j.surfcoat.2015.04.029 ↗
27. An enhanced continuum model for size-dependent strengthening and failure of particle-reinforced composites10.1016/j.actamat.2009.08.010 ↗
28. Microstructure and mechanical properties of SiC reinforced AlSi10Mg composites fabricated by laser metal deposition10.1016/j.jmapro.2020.08.073 ↗
29. Influence of processing parameters on selective laser melted SiCp/AlSi10Mg composites: densification, microstructure and mechanical properties10.1016/j.msea.2019.138155 ↗
30. Gu · 2015
31. Microstructure characteristics and its formation mechanism of selective laser melting SiC reinforced Al-based composites10.1016/j.vacuum.2018.11.022 ↗
32. 3D printing of Aluminium alloys: additive Manufacturing of Aluminium alloys using selective laser melting10.1016/j.pmatsci.2019.100578 ↗
33. Effect of SiC particles on the laser sintering of Al–7Si–0.3Mg alloy10.1016/j.scriptamat.2008.03.007 ↗
34. A solution to the hot cracking problem for aluminium alloys manufactured by laser beam melting10.1016/j.actamat.2020.07.015 ↗
35. A review on selective laser sintering/melting (SLS/LPBF) of aluminium alloy powders: processing, microstructure, and properties10.1016/j.pmatsci.2015.03.002 ↗
36. Effect of copper coated SiC reinforcements on microstructure, mechanical properties and wear of aluminium composites10.1088/1757-899X/225/1/012265 ↗
37. Effects of Ti-coating layer on the distribution of SiCP in the SiCP/2014Al composites10.1016/j.matdes.2015.09.089 ↗
38. Thermal spray coating
39. A new electroless nickel deposition technique to metallise SiCp/Al composites10.1016/j.surfcoat.2005.05.031 ↗
40. Production of Al based composite reinforced with SnO2 coated SiC particles10.1177/0021998307082174 ↗
41. Design and fabrication of the ceramic composites via in-situ oxidized process: phase and microstructure evolution in in-situ oxidized SiC/Al–Mg–Si process10.1016/j.ceramint.2022.10.202 ↗
42. Effect of oxidation of SiC particles on mechanical properties and wear behavior of SiCp/Al6061 composites10.1016/j.jallcom.2018.07.355 ↗
43. Effects of particle size and surface modification of SiC on the wear behavior of high volume fraction Al/SiCp composites10.1016/j.jallcom.2020.154647 ↗
44. Atomistic deformation modes and intrinsic brittleness ofAl4SiC4: a first-principles investigation10.1103/PhysRevB.74.174112 ↗
45. Effect of hot isostatic pressing on the critical defect size distribution in AlSi7Mg0.6 alloy obtained by selective laser melting10.1016/j.ijfatigue.2020.105797 ↗
46. The influence of particle size and particle fracture on the elastic/plastic deformation of metal matrix composites10.1016/1359-6454(96)00008-0 ↗
47. Tensile and compressive behaviour of additively manufactured AlSi10Mg samples10.1007/s40964-020-00131-9 ↗
48. Microstructure of selective laser melted AlSi10Mg alloy10.1016/j.matdes.2019.107677 ↗
49. Prediction of Si contents to suppress the formation of Al4C3 in the SiCpAl composite10.1016/S1359-6454(97)00265-6 ↗
50. Stable and metastable phase equilibria in the chemical interaction between aluminium and silicon carbide10.1007/BF01045395 ↗
51. Microstructure and deformation behavior of Ti-6Al-4V alloy by high-power laser solid forming10.1016/j.actamat.2017.04.026 ↗
52. Strengthening mechanisms in direct metal laser sintered AlSi10Mg: comparison between virgin and recycled powders
53. Fracture resistance of AlSi10Mg fabricated by laser powder bed fusion10.1016/j.actamat.2021.116869 ↗
54. Comparative study of performance comparison of AlSi10Mg alloy prepared by selective laser melting and casting10.1016/j.jmst.2019.08.049 ↗
55. 2019
56. SiC reinforced AlSi10Mg composites fabricated by selective laser melting10.1016/j.jallcom.2021.162365 ↗
57. The mechanical behavior and microstructure of additively manufactured AlSi10Mg for different material states and loading conditions10.1016/j.msea.2021.141134 ↗
58. Strain rate sensitivity and fracture mechanism of AlSi10Mg parts produced by selective laser melting10.1016/j.msea.2016.11.070 ↗
59. Mechanical behavior of additive manufactured, powder-bed laser-fused materials10.1016/j.msea.2015.10.068 ↗
60. Heterogeneous microstructure and voids dependence of tensile deformation in a selective laser melted AlSi10Mg alloy10.1016/j.msea.2020.140109 ↗
61. Selective laser melted AlSi10Mg alloy under melting mode transition: microstructure evolution, nanomechanical behaviors and tensile properties10.1016/j.jallcom.2021.159823 ↗
62. A review of selective laser melting of aluminum alloys: processing, microstructure, property and developing trends10.1016/j.jmst.2018.09.004 ↗