Abstract The microstructure and microtexture evolution of Ti–6Al–4V T-joints produced by dual laser beam bilateral synchronous welding (DLBSW) were investigated using the optical microscopy (OM) and electron back-scattered diffraction (EBSD) and correlated with the mechanical properties of the joint. We demonstrate important differences in temperature field, grain morphology, misorientation angles and texture intensity between the base material (BM), the skin-side heat-affected zone (SK-HAZ), the stringer-side heat-affected zone (ST-HAZ) and the weld seam (WS). Through in-depth crystallographic analysis, we demonstrate that the kernel average misorientation curve of the WS is steeper and the peak misorientation angle is larger, revealing that the WS has a lower geometrically necessary dislocations density and a smaller residual strain. Due to the different orientation of each a-phase colony at the interface of the two phases, it is not conducive to the deformation mode of dislocation slip, so a large number of twins are generated in the WS. Furthermore, the WS has a strong crystal preferential orientation and the maximum polar density of the pole figure is 17.05, which is significantly higher than the polar density of the base material. It is found that the gradient of microstructure variation in the narrow HAZ is higher than that in the WS, which leads to more heterogeneous properties in the HAZ compared to the weld. This research result is consistent with the phenomenon that all the fractures of the resultant T-joints occurred in the HAZ.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Welding Techniques and Residual Stresses · Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Double-sided laser beam welded T-joints for aluminum aircraft fuselage panels: process, microstructure, and mechanical propertiesMater
2. Numerical investigation on novel geometrical configuration for adhesively bonded T-joint between aluminum and sandwich panel10.1016/j.tws.2018.06.039 ↗
3. A study on an efficient prediction of welding deformation for T-joint laser welding of sandwich panel Part II: proposal of a method to use shell element modelInt10.2478/IJNAOE-2013-0176 ↗
4. Double-sided laser beam welded T-joints for aluminum-lithium alloy aircraft fuselage panels: effects of filler elements on microstructure and mechanical propertiesOpt10.1016/j.optlastec.2017.02.004 ↗
5. Development of an end-to-end simulation process chain for prediction of self-piercing riveting joint geometry and strength10.1016/j.jmapro.2020.07.004 ↗
6. Effect of riveting process parameters on the local stress field of a T-joint10.1016/j.ijmecsci.2011.07.013 ↗
7. Variation modeling of aeronautical thin-walled structures with multi-state riveting10.1016/j.jmsy.2011.05.004 ↗
8. Light-weight structures produced by laser beam joining for future applications in automobile and aerospace industry10.1016/S0924-0136(01)00756-7 ↗
9. Microstructural and mechanical characterization of laser beam welded AA6056 Al-alloyMater10.1016/j.msea.2011.06.010 ↗
10. Nano-indentation and in-situ investigations of double-sided laser beam welded 2060-T8/2099-T83 Al-Li alloys T-jointsMater10.1016/j.msea.2019.04.066 ↗
11. Effect of activated flux on penetration depth, microstructure and mechanical properties of Ti-6Al-4V TIG weldsJ10.1016/j.jmatprotec.2018.06.024 ↗
12. Effect of post heat treatment on microstructure and mechanical properties of Ti-6Al-4V jointing parts proceeded by laser additive manufacturing10.1016/j.msea.2020.139544 ↗
13. Improvement in mechanical properties of commercially pure titanium through reverse rolling10.1080/09500839.2017.1341647 ↗
14. Effect of strain-paths on mechanical properties of hot rolled commercially pure titanium10.1016/j.matlet.2016.05.162 ↗
15. Fiber laser welding of dissimilar titanium (Ti-6Al-4V/cp-Ti) T-joints and their laser forming process for aircraft application10.1016/j.optlastec.2017.05.017 ↗
16. Effect of welding direction on deformation of Ti6Al4V alloy coplanar double lap-joint produced by dual laser beam bilateral synchronous weldingOpt10.1016/j.optlastec.2020.106447 ↗
17. Influence of the local chemical composition on the mechanical properties of laser beam welded
18. Nano-indentation investigation on the local softening of equiaxed zone in 2060-T8/2099-T83 aluminum-lithium alloys T-joints welded by double-sided laser beam welding10.1016/j.jallcom.2018.05.014 ↗
19. Formation, microstructure and mechanical properties of double-sided laser beam welded Ti–6Al–4V T-joint10.1016/S1003-6326(16)64163-8 ↗
20. Fatigue behavior of double-sided laser shock peened Ti-6Al-4V thin blade subjected to foreign object damageOpt10.1016/j.optlastec.2019.105784 ↗
21. Multi-laser powder bed fusion of Ti–6Al–4V alloy: defect, microstructure, and mechanical property of overlap region10.1016/j.msea.2020.140644 ↗
22. Microstructure and deformation behavior of Ti-6Al-4V alloy by high-power laser solid forming10.1016/j.actamat.2017.04.026 ↗
23. Optimising the mechanical properties of Ti-6Al-4V components produced by wire + arc additive manufacturing with post-process heat treatments10.1016/j.jallcom.2018.04.158 ↗
24. Effects of internal porosity and crystallographic texture on Charpy absorbed energy of electron beam melting titanium alloy (Ti-6Al-4V)10.1016/j.msea.2018.11.005 ↗
25. Targeted heat treatment of additively manufactured Ti-6Al-4V for controlled formation of Bi-lamellar microstructures10.1016/j.jmst.2021.01.004 ↗
26. Double-sided fiber laser beam welding process of T-joints for aluminum aircraft fuselage panels: filler wire melting behavior, process stability, and their effects on porosity defects10.1016/j.optlastec.2013.04.003 ↗
27. Effects of heat treatment on microstructure and mechanical properties of double-sided laser-welded AA2060/AA2099 T-Joint10.1016/j.jmatprotec.2020.116777 ↗
28. Temperature distribution and melt geometry in laser and electron-beam melting processes-A comparison among common materials
29. Laser additive melting and solidification of inconel 718: finite element simulation and experiment10.1007/s11837-015-1765-1 ↗
30. Study on 2219 Al-Cu alloy T-joint used dual laser beam bilateral synchronous welding: parameters optimization based on the simulation of temperature field and residual stress10.1016/j.optlastec.2020.106481 ↗
31. The research on the heat source characteristics and the equivalent heat source of the arc in gaps10.1016/j.ijheatmasstransfer.2018.03.048 ↗
32. Heat and mass transfer in laser dissimilar welding of stainless steel and nickel10.1016/j.apsusc.2012.02.143 ↗
33. Correlation of microstructure with mechanical properties of TIG weldments of Ti–6Al–4V made with and without current pulsing10.1016/j.matchar.2006.07.001 ↗
34. Effect of trace lanthanum hexaboride on the phase, grain structure, and texture of electron beam melted Ti-6Al-4V
35. Variant selection and intervariant crystallographic planes distribution in martensite in a Ti–6Al–4V alloy10.1016/j.actamat.2014.06.064 ↗
36. Crystallographic features of α variants and β phase for Ti-6Al-4V alloy fabricated by selective laser melting10.1016/j.msea.2017.09.068 ↗
37. Crystallographic variant selection in Ti–6Al–4V10.1016/j.actamat.2004.07.034 ↗
38. Selective laser melting of Ti-5Al-2.5Sn alloy with isotropic tensile properties: the combined effect of densification state, microstructural morphology, and crystallographic orientation characteristics10.1016/j.jmatprotec.2019.04.003 ↗
39. Analysing the combined effect of crystallographic orientation and grain refinement on mechanical properties and corrosion behaviour of ECAPed ZE41 Mg alloy10.1016/j.jma.2020.08.015 ↗
40. Mechanism of texture and microstructure evolution during warm rolling of Ti-6Al-4V alloy10.1080/14786435.2018.1493237 ↗
41. Microstructure and texture evolution during annealing of Ti-6Al-4V alloy10.1080/02670836.2019.1706816 ↗
42. Microstructure, texture, mean free path of dislocations and mechanical properties of Ti-6A1-4V alloy during uniaxial compression at elevated temperatures10.1016/j.msea.2020.139042 ↗