Effect of Mg content on the microstructure and properties of high strength, high conductivity Cu–Fe–Cr–Si–Mg alloy
Source abstract
Abstract
A new strategy for the preparation of Cu–Fe alloy with excellent comprehensive performance is proposed. This strategy combines the construction of dual-scale polymetallic second phases with the addition of trace solid-solution atoms. A series of Cu–2Fe-0.3Cr-0.2Si-xMg (x = 0.1, 0.3, 0.5) alloys are designed and prepared through multi-stage thermo-mechanical treatment. Among the reported Cu–Fe alloys with low Fe content (Fe content less than 3 wt%), the designed Cu–2Fe-0.3Cr-0.2Si-0.3 Mg alloy has the highest product of the tensile strength times the electrical conductivity (PSC). The tensile strength and PSC of the Cu–2Fe-0.3Cr-0.2Si-0.3 Mg alloy are 698 MPa and 43.9 GPa∙%IACS, respectively. The dual-scale polymetallic second phase has been successfully constructed. The submicron-scale Fe 8 CrSi phase triggers the generation of substructures, such as geometrically necessary dislocation boundaries in lamellar structures and random dislocation boundaries in cell shapes. The high-density low angle grain boundaries (LAGBs) of substructure evolution enhances the substructure strengthening of the alloy. The main strengthening phase in precipitation strengthening is the nanoscale Fe 11 CrSi 4 phase. An appropriate amount of Mg reduces the ultimate solid solubility of Fe atoms in Cu alloys, promotes the formation of a dual-scale second phase and refines the grain size of the alloy. Therefore, the comprehensive performance of the design alloy is significantly improved.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Microstructure and mechanical properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Bodyakova · 2023
2. Microstructure and properties of Cu-Zn-Cr-Zr alloy treated by multistage thermo-mechanical treatment10.1016/j.msea.2023.144679 ↗
3. Evolution of microstructure and properties of an ultrahigh strength Cu–Ni–Sn alloy with low Sn content during the multi-stage thermomechanical treatment10.1016/j.msea.2023.144933 ↗
4. Effects of a thermal-ultrasonic stress relaxation process on the residual stress, mechanical properties and microstructures of C19400 copper alloy strips10.1016/j.msea.2022.143014 ↗
5. Microstructure formation and electrical resistivity behavior of rapidly solidified Cu-Fe-Zr immiscible alloys10.1016/j.jmst.2019.10.038 ↗
6. Microstructure evolution and deformation behaviour of Cu-10 wt%Fe alloy during cold rolling10.1016/j.msea.2020.140379 ↗
7. Mechanical properties and microstructural change in (Cu–Fe) immiscible metal matrix composite: effect of Mg on secondary phase separation10.1016/j.jmrt.2020.11.049 ↗
8. Investigation on the dual-phase co-deformation behavior and strengthening mechanism in cold-drawn Cu–20Fe alloy10.1016/j.msea.2022.144474 ↗
9. High strength and high electrical conductivity in Cu–Fe alloys with nano and micro Fe particles10.1016/j.msea.2022.143948 ↗
10. Study on high-strength and high-conductivity Cu–Fe–P alloys10.1016/j.msea.2006.01.068 ↗
11. Effect of dual-scale FeCrSi phase on the strength and conductivity of Cu-2.5Fe-0.3Cr-0.2Si alloy10.1016/j.msea.2022.144340 ↗
12. Aging behavior and precipitate analysis of copper-rich Cu–Fe–Mn–P alloy10.1016/j.msea.2012.04.055 ↗
13. Nanoprecipitates induced dislocation pinning and multiplication strategy for designing high strength, plasticity and conductivity Cu alloys10.1016/j.scriptamat.2021.113741 ↗
14. Effects of thermo-mechanical processing and trace amount of carbon addition on tensile properties of Cu–2.5Fe–0.1P alloys10.1016/j.msea.2009.05.021 ↗
15. Effects of Si addition on mechanical, electrical and magnetic property of Cu-10Fe alloy10.1016/j.matchar.2022.112612 ↗
16. Microstructure and properties of high strength, high conductivity and magnetic Cu–10Fe-0.4Si alloy10.1016/j.msea.2021.142012 ↗
17. High strength, high conductivity and good softening resistance Cu-Fe-Ti alloy10.1016/j.jallcom.2022.166595 ↗
18. Microstructure and properties of Cu-Fe-Cr-Ag alloy prepared by directional solidification and upward continuous casting10.1007/s11661-021-06239-z ↗
19. Influence of Ag micro-alloying on the thermal stability and ageing characteristics of a Cu–14Fe in-situ composite10.1016/j.msea.2016.07.017 ↗
20. Effect of Mg addition on Fe phase morphology, distribution and aging kinetics of Cu-6.5Fe alloy10.1016/j.msea.2021.141064 ↗
21. Tailoring microstructural evolution and fracture damage behavior of a Mg–Y–Zn alloy during hot tensile deformation10.1016/j.msea.2023.144857 ↗
22. Microstructure change characteristic and fracture mechanism of Ti-47.5Al-2.5V-1.0Cr-0.2Zr alloy during high temperature tensile deformation10.1016/j.jallcom.2023.169963 ↗
23. X-ray line broadening from filed aluminium and wolfram10.1016/0001-6160(53)90006-6 ↗
24. Dislocation densities in some annealed and cold-worked metals from measurements on the X-ray debye-scherrer spectrum10.1080/14786435608238074 ↗
25. Honeycombe · 1968
26. Geometrically necessary boundaries, incidental dislocation boundaries and geometrically necessary dislocations10.1016/S1359-6462(02)00358-5 ↗
27. A review of microstructure and texture evolution with nanoscale precipitates for copper alloys10.1016/j.jmrt.2020.08.055 ↗
28. Stress–strain behavior of ferrite and bainite with nano-precipitation in low carbon steels10.1016/j.actamat.2014.10.010 ↗
29. Ha · 1983
30. Solution hardening by tetragonal dist ortions: application to irradiation hardening10.1016/0001-6160(62)90098-6 ↗
31. Substitutional solution hardening10.1016/0001-6160(63)90213-X ↗
32. Quantitative size-factors for metallic solid solutions10.1007/BF00549722 ↗
33. A precipitation-hardened high-entropy alloy with outstanding tensile properties10.1016/j.actamat.2015.08.076 ↗
34. A modified Hall–Petch relationship in ultrafine-grained titanium recycled from chips by equal channel angular pressing10.1016/j.scriptamat.2012.02.008 ↗
35. Relationship between microstructure, properties and reaction conditions for Cu–TiB2 alloys prepared by in situ reaction10.1016/j.actamat.2009.06.030 ↗
36. Deviations from Matthiessen's rule and longitudinal magnetoresistance in copper10.1007/BF00628101 ↗
37. Scattering cancellation by a monolayer cloak in oxide dispersion‐strengthened alloys10.1002/adfm.202003270 ↗
38. Application of an extension of Linde's rule to some dilute alloys of Cu, Mg, and Al10.1063/1.1708269 ↗
39. Anomalous temperature dependence of the electrical resistivity in binary and pseudobinary alloys based on Fe3Si10.1103/PhysRevB.48.13607 ↗
40. Calculation of electrical resistivity produced by dislocations and grain boundaries in metals10.1088/0953-8984/6/4/007 ↗
41. The electrical resistivity of dislocations10.1080/14786436308209092 ↗
42. First-Principles study on the Cu/Fe interface properties of ternary Cu-Fe-X alloys10.3390/ma13143112 ↗
43. First-principles study on the solubility of iron in dilute Cu-Fe-X alloys10.1016/j.jallcom.2016.08.247 ↗