Precipitation behavior during low-temperature aging in Al–Mg–Si alloy using STEM-EDS intensity correlograms

Genki Saito, Yamato Sano, Kazuya Mizuno, Shoma Torigoe, Ken Takata, Toshihiro Okajima, Shunsuke Muto

Abstract

Al–Mg–Si alloys are extensively used in automotive panels because of their high formability and age-hardening capabilities during paint baking. Natural aging that occurs after the solution treatment inhibits formation of β″ precipitates during subsequent artificial aging, reducing the hardness. The precipitation behavior of Al–0.65Mg–0.81Si mass% alloy during isothermal aging at 100 °C over various durations is investigated in this study using scanning transmission electron microscopy (STEM) and STEM energy-dispersive X-ray spectroscopy (EDS). The analysis reveals the formation of Guinier–Preston (GP) zones and β″ precipitates, which influence the mechanical properties of the alloy. After 1 h of aging, no GP zones are observed; however, clusters with diameters of 1.0–1.5 nm formed, increasing and decreasing in density at 10 and 400 h, respectively. Further, β″-related structures with a Mg/Si ratio of ∼1 started forming at 10 h and grew in number by 400 h, with most particles being spherical and some elongated along the [100] Al direction. These microstructural changes correlate with yield strength variations, highlighting the role of pre-aging in promoting β″ formation during subsequent artificial aging. In addition, a novel STEM-EDS intensity correlogram method is introduced to effectively distinguish aging products from the matrix and deepen the understanding of microstructural evolution in Al–Mg–Si alloys. • Microstructural evolution of Al-Mg-Si alloys was investigated during isothermal aging. • Clusters and β″ precipitates were identified during aging using STEM-LAADF and STEM-EDS. • Novel STEM-EDS correlogram method effectively distinguishes aging products. • Clusters with widely distributed compositions formed after 1 h of aging. • β″-related structures with Mg/Si ratio of ∼1 started forming between 1 and 10 h of aging.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Review on recent progress in Al–Mg–Si 6xxx conductor alloys10.1557/s43578-022-00488-3 ↗
2. Nanocluster control for achieving high strength aluminum alloys10.2320/matertrans.M2017390 ↗
3. uuml, rgen, Aluminium in innovative light-weight car design10.2320/matertrans.L-MZ201132 ↗
4. The precipitation sequence in Al–Mg–Si alloys10.1016/S1359-6454(98)00059-7 ↗
5. Change in the structure and mechanical properties of Al–Mg–Si alloys caused by the addition of other elements: a comprehensive review10.1016/j.jmrt.2023.09.220 ↗
6. Structure determination of Mg5Si6 particles in Al by dynamic electron diffraction studies10.1126/science.277.5330.1221 ↗
7. The crystal structure of the β″ phase in Al–Mg–Si alloys10.1016/S1359-6454(97)00493-X ↗
8. Atomic model for GP-zones in a 6082 Al–Mg–Si system10.1016/S1359-6454(00)00302-5 ↗
9. Detailed atomistic insight into the β″ phase in Al–Mg–Si alloys10.1016/j.actamat.2014.01.052 ↗
10. Composition of β″ precipitates in Al–Mg–Si alloys by atom probe tomography and first principles calculations10.1063/1.3269714 ↗
11. First-principles study of crystal structure and stability of Al–Mg–Si–(Cu) precipitates10.1016/j.actamat.2004.05.037 ↗
12. Structural and compositional study of precipitates in under-aged Cu-added Al-Mg-Si alloy10.1038/s41598-018-35134-8 ↗
13. Effect of natural aging and preaging on subsequent precipitation process of an AI-Mg-Si alloy with high excess silicon10.1179/mst.1997.13.11.905 ↗
14. Mechanisms controlling the artificial aging of Al–Mg–Si Alloys10.1016/j.actamat.2011.02.010 ↗
15. The basic processes affecting two-step ageing in an Al-Mg-Si alloy10.1080/14786436708229257 ↗
16. Pre-precipitate clusters and precipitation processes in Al–Mg–Si alloys10.1016/S1359-6454(99)00033-6 ↗
17. Improvement of strength–elongation balance of Al–Mg–Si sheet alloy by utilising Mg–Si cluster and its proposed mechanism10.2320/matertrans.M2016258 ↗
18. The influence of composition and natural aging on clustering during preaging in Al–Mg–Si alloys10.1063/1.3481090 ↗
19. Formation and reversion of clusters during natural aging and subsequent artificial aging in an Al–Mg–Si alloy10.1016/j.msea.2015.02.035 ↗
20. Atomic structure of clusters and GP-zones in an Al-Mg-Si alloy10.1016/j.actamat.2024.119811 ↗
21. Effects of cluster characteristics on two-step aging behavior in Al-Mg-Si alloys with different Mg/Si ratios and natural aging periods10.1016/j.msea.2018.01.086 ↗
22. Formulation of initial artificial age-hardening response in an Al-Mg-Si alloy based on the cluster classification using a high-detection-efficiency atom probe10.1016/j.jallcom.2017.10.220 ↗
23. Effects of natural aging after pre-aging on clustering and bake-hardening behavior in an Al–Mg–Si alloy10.1016/j.scriptamat.2016.01.019 ↗
24. Three-dimensional atom probe characterization of nanoclusters responsible for multistep aging behavior of an Al-Mg-Si alloy10.1007/s11661-007-9438-5 ↗
25. Effect of natural ageing or pre-ageing on the evolution of precipitate structure and strength during age hardening of Al–Mg–Si alloy AA 601610.1016/j.msea.2019.05.073 ↗
26. Effect of two-step aging on cluster formation in Al–Mg–Si alloys10.2320/matertrans.M2013388 ↗
27. The nanocluster formation and vacancy behavior of step-quenched Al–Mg–Si alloy and its effect on transition to β" phase via advanced methods10.1016/j.msea.2021.141032 ↗
28. Data analysis and other considerations concerning the study of precipitation in Al–Mg–Si alloys by atom probe tomography10.1016/j.dib.2015.09.045 ↗
29. Study of precipitation in Al–Mg–Si alloys by atom probe tomography I. Microstructural changes as a function of ageing temperature10.1016/j.actamat.2015.08.017 ↗
30. Dr. Probe: a software for high-resolution STEM image simulation10.1016/j.ultramic.2018.06.003 ↗
31. 2024
32. Design of solute clustering during thermomechanical processing of AA6016 Al–Mg–Si alloy10.1016/j.actamat.2020.10.074 ↗
33. Effects of local bonding between solute atoms and vacancy on formation of nanoclusters in Al–Mg–Si alloys10.2320/matertrans.MT-L2023006 ↗
34. Vacancy behavior during aging at 50 and 100°C in Al–Mg–Si alloys with excess Si studied by positron annihilation spectroscopy10.2320/matertrans.L-M2019846 ↗
35. Investigation of precipitation strengthening behavior of Al-Mg-Si alloy using SAXS10.1016/S1003-6326(23)66184-9 ↗
36. On the critical resolved shear stress of solid solutions containing coherent precipitates10.1002/pssb.19660160234 ↗
37. Improving mechanical properties of AlSi10Mg aluminum alloy using ultrasonic melt treatment combined with T6 heat treatment10.4149/km_2019_1_33 ↗