Effect of adding 0.5 wt% ZnO nanoparticles, temperature and strain rate on tensile properties of Sn–5.0 wt% Sb–0.5 wt% Cu (SSC505) lead free solder alloy
Source abstract
Abstract
Abstract This study investigates the effect of adding 0.5 wt% ZnO nanoparticles into Sn–5 wt% Sb–0.5 wt% Cu (SSC505) solder alloy on the growth of intermetallic compounds (IMCs) as well as the associated changes of microstructure. It was found that, the morphologies of the IMCs transformed to refinement forms due to the adsorption effect of ZnO nanoparticles. Systematic study of tensile properties was performed for bulk solders over a wide range of strain rates at various temperatures to determine the plastic deformation mechanism. Obviously, the ultimate tensile strength (UTS) and the yield stress ( σ y ) were improved. This can be attributed to reinforcement of ZnO nanoparticles, refined β-Sn grains and IMCs that could obstruct the dislocation slipping. The obtained results are consistent with the prediction of the classic theory of dispersion strengthening. Furthermore, the average activation energy ( Q ) for plain and composite solders were 57 and 59 kJ/mol, respectively, which close to that of pipe-diffusion mechanism in Sn based solder matrix.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Aluminum Alloys Composites Properties · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Lead-free Solders in Microelectronics10.1016/S0927-796X(00)00010-3 ↗
2. Research advances in nano-composite solders10.1016/j.microrel.2008.10.004 ↗
3. Composite lead-free electronic solders
4. New, creep-resistant, low melting point solders with ultrafine oxide dispersions10.1007/s11664-998-0072-9 ↗
5. Lead-free universal solders for optical and electronic devices10.1007/s11664-002-0005-y ↗
6. Creep behavior of eutectic 80Au/20Sn solder alloy10.1016/j.jallcom.2008.09.009 ↗
7. Lead (Pb)-free solders for electronic packaging10.1007/BF02651362 ↗
8. Influence of ZnO nano-particles addition on thermal analysis microstructure evolution and tensile behavior of Sn–5.0wt% Sb–0.5wt% Cu lead-free solder alloy10.1016/j.msea.2015.02.070 ↗
9. Microstructure and impression creep behavior of lead-free Sn–5Sb solder alloy containing Bi and Ag10.1016/j.msea.2012.03.093 ↗
10. Creep properties of Sn–Sb based lead-free solder alloys10.1016/j.jallcom.2008.03.097 ↗
11. Power law indentation creep of Sn–5% Sb solder alloy10.1007/s10853-005-0421-5 ↗
12. Study of the mechanical and thermal properties of Sn–5wt% Sb solder alloy at two annealing temperatures10.1002/pssa.200306592 ↗
13. Lowering of Sn–Sb alloy melting points caused by substrate dissolution10.1007/s11664-006-0303-x ↗
14. Microstructure and tensile behavior of Sn–5Sb lead-free solder alloy containing Bi and Cu10.1016/j.msea.2011.09.103 ↗
15. In search of new lead-free electronic solders10.1007/BF02651363 ↗
16. Microstructural evolution and tensile properties of Sn–5Sb solder alloy containing small amount of Ag and Cu10.1016/j.jallcom.2011.01.109 ↗
17. Creep behavior of near-peritectic Sn–5Sb solders containing small amount of Ag and Cu10.1016/j.msea.2010.11.001 ↗
18. Creep and thermo-mechanical fatigue properties of in-situ Cu6Sn5 reinforced lead-free composite solder10.1016/j.msea.2010.02.048 ↗
19. Morphological transition of interfacial Ni3Sn4 grains at the Sn–3.5Ag/Ni joint10.1007/BF02690537 ↗
20. Creep properties of Sn–Ag solder joints containing intermetallic particles10.1007/s11837-001-0098-4 ↗
21. Creep properties of eutectic Sn–3.5Ag solder joints reinforced with mechanically incorporated Ni particles10.1007/s11664-001-0153-5 ↗
22. Influence of ceramic reinforcements on the wettability and mechanical properties of novel lead-free solder composites10.1016/j.tsf.2005.09.057 ↗
23. Effect of SiC nanoparticle additions on microstructure and microhardness of Sn–Ag–Cu solder alloy10.1007/s11664-007-0366-3 ↗
24. Strengthening mechanism of SiC-particulate reinforced Sn–3.7Ag–0.9Zn lead-free solder10.1016/j.jallcom.2009.02.002 ↗
25. Structural characterization and creep resistance of nano-silicon carbide reinforced Sn–1.0Ag–0.5Cu lead-free solder alloy10.1016/j.matdes.2013.10.043 ↗
26. High-temperature shear strength of lead-free Sn–Sb–Ag/Al2O3 composite solder10.1016/j.msea.2011.02.034 ↗
27. Effects of nano-TiO2 additions on thermal analysis, microstructure and tensile properties of Sn–3.5Ag–0.25Cu solder10.1016/j.matdes.2009.08.008 ↗
28. Effect of nano-TiO2 addition on the microstructure and bonding strengths of Sn3.5Ag0.5Cu composite solder BGA packages with immersion Sn surface finish
29. Effect of addition of TiO2 nanoparticles on the microstructure, microhardness and interfacial reactions of Sn3.5Ag–XCu solder10.1016/j.matdes.2011.06.044 ↗
30. Development of lead-free Sn–3.5Ag/SnO2 nanocomposite solders
31. Effects of ZrO2 nanoparticles on the mechanical properties of Sn–Zn solder joints on Au/Ni/Cu pads10.1016/j.jallcom.2008.10.140 ↗
32. Strengthening effects of ZrO2 nanoparticles on the microstructure and microhardness of Sn–3.5Ag lead-free solder10.1007/s11664-006-0216-8 ↗
33. Tensile deformation behavior and melting property of nano-sized ZnO particles reinforced Sn–3.0Ag–0.5Cu lead-free solder10.1016/j.msea.2014.09.028 ↗
34. Effect of ZnO nanoparticles addition on thermal, microstructure and tensile properties of Sn–3.5 Ag–0.5 Cu (SAC355) solder alloy
35. Tensile creep characteristics of Sn–3.5Ag–0.5Cu (SAC355) solder reinforced with nano-metric ZnO particles10.1016/j.msea.2014.02.061 ↗
36. Creep of tin, Sb-solution-strengthened tin, and SbSn-precipitate-strengthened10.1007/s11661-002-0075-8 ↗
37. High creep resistance tin-based alloys for soldering applications10.1007/s11664-002-0021-y ↗
38. Formability of AA8011 aluminum alloy sheet in homogenized and unhomogenized conditions10.1023/B:JMSC.0000044884.25589.9b ↗
39. Humphreys · 2004 · 114
40. A unified model for the prediction of yield strength in particulate-reinforced metal matrix nanocomposites10.3390/ma8085138 ↗
41. Enhancing compressive response of AZ31B magnesium alloy using alumina nano-particulates10.1016/j.compscitech.2008.04.020 ↗
42. Hot deformation of ultrafine-grained Al6063/Al2O3 nanocomposites10.1007/s10853-011-5418-7 ↗
43. Enhancing strength and ductility of magnesium by integrating it with aluminum nanoparticles10.1016/j.actamat.2007.07.039 ↗
44. Influence of single-wall carbon nano tube addition on the microstructural and tensile properties of Sn–Pb solder alloy10.1016/j.jallcom.2007.01.045 ↗
45. Improving mechanical properties of magnesium using nano-yttria reinforcement and microwave assisted powder metallurgy method10.1016/j.compscitech.2007.03.006 ↗