journal article·2016-08

Failure behavior of high pressure die casting AZ91D magnesium alloy

X. Li, S.M. Xiong, Z. Guo

Publisher page

Abstract

Abstract The failure behavior of high pressure die casting AZ91D magnesium alloy during both tensile and fatigue tests was studied in situ by using scanning electron microscope. Attention was focused on the role of microstructure played in crack initiation and propagation. Results showed that the defects in castings, including gas pore, shrinkage pore and defect band, were the crack initiation sources. In tensile test, the crack propagated in a combination of intergranular and transgranular modes, and the specimen fractured by connecting defects at the section with minimum effective force bearing area. In fatigue test, the crack propagated in a transgranular mode at specific crystalline planes. When the crack was in contact with the β-phase, the crack would pass through, and fracture the network β-phase, whereas bypass the island β-phase by detaching it from the surrounding α-Mg grains. Besides, defects in front of the crack would act as the secondary crack initiation sources, from which new cracks would initiate and propagate. With the propagation of the fatigue crack, the actual maximum cyclic stress would increase to the fracture stress of the left cross section and lead to the final fracture of the specimen.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Research for a new age of magnesium in the automotive industry10.1016/S0924-0136(01)00780-4 ↗
2. Magnesium properties-application-potential10.1016/S0921-5093(00)01351-4 ↗
3. Relationship between internal porosity and fracture strength of die-cast magnesium AM60B alloy10.1016/j.msea.2004.12.042 ↗
4. Variability in the tensile ductility of high-pressure die-cast AM50 Mg-alloy10.1016/j.scriptamat.2005.06.002 ↗
5. Quantitative fractographic analysis of variability in the tensile ductility of high-pressure die-cast AE44 Mg-alloy10.1016/j.msea.2006.04.108 ↗
6. The correlation between microstructure and mechanical properties of high-pressure die-cast AM50 alloy10.1016/j.jallcom.2008.11.040 ↗
7. In situ observation of tensile deformation of high-pressure die-cast specimens of AM50 alloy10.1016/j.msea.2009.05.042 ↗
8. Modeling the tensile failure of cast magnesium alloys10.1016/j.jallcom.2012.05.090 ↗
9. Predicting the influence of pore characteristics on ductility of thin-walled high pressure die casting magnesium10.1016/j.msea.2013.02.026 ↗
10. Micro-macro interactions and effect of section thickness of hpdc AZ91 Mg alloy10.1016/j.jallcom.2007.09.134 ↗
11. Fatigue crack growth mechanisms in high-pressure die-cast magnesium alloys10.1007/s11661-007-9328-x ↗
12. Improved bending fatigue and corrosion properties of a Mg–Al–Mn alloy by super vacuum die casting10.1016/j.scriptamat.2012.08.010 ↗
13. Effects of rheo-die casting process on the microstructure and mechanical properties of AM50 magnesium alloy10.1179/174328405X51820 ↗
14. Microstructure and mechanical properties of a rheo-diecast Mg–10Zn–4.5Al alloy10.2320/matertrans.46.2221 ↗
15. Microstructural refinement of AZ91D die-cast alloy by intensive shearing10.1016/j.msea.2010.01.013 ↗
16. Comparison of mechanical properties and microstructure of AZ91D alloy motorcycle wheels formed by die casting and double control forming10.1016/j.matdes.2012.04.029 ↗
17. Cyclic deformation behavior of a super-vacuum die cast magnesium alloy10.1016/j.msea.2012.03.028 ↗
18. Improvements engineered in UTS and elongation of aluminum alloy high pressure die castings through the alteration of runner geometry and plunger velocity10.1016/j.msea.2012.08.098 ↗
19. Weibull statistical analysis of the effect of melt conditioning on the mechanical properties of AM60 alloy10.1016/j.msea.2012.12.079 ↗
20. Mechanical properties and fatigue behavior of vacuum-assist die cast AlMgSiMn alloy10.1016/j.msea.2013.03.042 ↗
21. Improved mechanical properties in vacuum-assist high-pressure diecasting of AZ91D alloy10.1016/j.jmatprotec.2015.12.005 ↗
22. The heat transfer during filling of a high-pressure die-casting shot sleeve10.1016/j.msea.2005.08.166 ↗
23. Microstructure characteristics of the eutectics of die cast AM60B magnesium alloy10.1016/S1005-0302(12)60011-5 ↗
24. Formation of gas induced shrinkage porosity in Mg-alloy high-pressure die-castings10.1016/j.scriptamat.2006.04.040 ↗
25. Defect band characteristics in Mg–Al and Al–Si high-pressure die castings. Metall10.1007/s11661-007-9243-1 ↗
26. Brown · 1969
27. Correlation between porosity and fracture mechanism in high pressure die casting of AM60B alloy10.1016/j.jmst.2015.10.002 ↗
28. Roles of deformation twinning and dislocation slip in the fatigue failure mechanism of AZ31 Mg alloys10.1016/j.scriptamat.2010.03.021 ↗
29. Identification and modeling of fatigue crack growth mechanisms in a die-cast AM50 magnesium alloy10.1016/j.actamat.2006.06.039 ↗
30. Low-cycle fatigue behavior of die-cast Mg alloys AZ91 and AM6010.1007/s11661-012-1114-8 ↗