Abstract
Abstract The stretch flangeability of a medium Mn steel prepared by quenching and partitioning was examined using a hole-expansion test. Samples were heat-treated at quenching temperatures 90 °C ≤ T Q ≤ 170 °C, at which no secondary martensite is formed upon final quenching. The hole-expansion test used a 60° conical punch. The hole at the center of the specimens was prepared by punching or wire cutting. In both sample preparation conditions, hole expansion ratio (HER) increased as T Q decreased. The dependence of HER on T Q was more pronounced in the samples prepared by punching than in samples prepared by wire cutting. While there is no clear correlation between HER and tensile properties, the HER decreased as retained austenite increased. By punching, the retained austenite transformed to strain-induced martensite in the shear-affected zone near the hole edge. This martensite has a negative impact on the HER.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Magnetic Properties and Applications · Metal Forming Simulation Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. J. Speer, A. Streicher, D. Matlock, F. Rizzo, G. Krauss, Quenching and partitioning: a fundamentally new process to create high strength trip sheet microstructures, in: Symposium on the Thermodynamics, Kinetics, Characterization and Modeling of: Austenite Formation and Decomposition, 2003, pp. 505–522.
2. Carbon partitioning into austenite after martensite transformation10.1016/S1359-6454(03)00059-4 ↗
3. Carbon partitioning to austenite from martensite or bainite during the quench and partition (Q&P) process: a critical assessment10.1016/j.actamat.2007.08.051 ↗
4. Influence of carbon partitioning kinetics on final austenite fraction during quenching and partitioning10.1016/j.scriptamat.2009.03.021 ↗
5. Characterization of the microstructure obtained by the quenching and partitioning process in a low-carbon steel10.1016/j.matchar.2008.04.004 ↗
6. Effect of carbon and manganese on the quenching and partitioning response of CMnSi steels10.2355/isijinternational.51.137 ↗
7. Microstructural development during the quenching and partitioning process in a newly designed low-carbon steel10.1016/j.actamat.2011.06.014 ↗
8. Quenched and partitioned CMnSi steels containing 0.3 wt% and 0.4 wt% carbon10.1007/s11837-015-1620-4 ↗
9. Microstructure-mechanical properties relationships for quenching and partitioning (Q&P) processed steel10.1016/j.actamat.2016.04.048 ↗
10. Application of quenching and partitioning processing to medium Mn steel10.1007/s11661-014-2657-7 ↗
11. Stretch-flangeability of strong multiphase steels10.1179/174328407X179511 ↗
12. S. Sadagopan, D. Urban, Formability characterization of a new generation of high strength steels, AISI/DOE technology roadmap program, 2003.
13. Hole expansion characteristics of ultra high strength steels10.1016/j.proeng.2014.10.066 ↗
14. Factors governing hole expansion ratio of steel sheets with smooth sheared edge10.1007/s12540-016-6346-5 ↗
15. Effect of micro-alloying elements on the stretch-flangeability of dual phase steel10.1016/j.msea.2012.01.003 ↗
16. Non-linear correlation between uniaxial tensile properties and shear-edge hole expansion ratio10.1007/s11665-014-1161-y ↗
17. Effect of a strain-hardening rate at uniform elongation on sheared edge stretching10.1007/s11665-011-0116-9 ↗
18. Ductility and formability of newly developed high strength low alloy TRIP-aided sheet steels with annealed martensite matrix10.2355/isijinternational.42.910 ↗
19. Stretch-flangeability of a high-strength TRIP type bainitic sheet steel10.2355/isijinternational.40.920 ↗
20. N. Pathak, C. Butcher, M. Worswick, Influence of the sheared edge condition on the hole expansion of dual phase steel, in: Proceedings of IDDRG2013, Zürich, 2013, pp. 213–218.
21. O.R. Terrazas, Correlation of Microstructure, Tensile Properties and Hole Expansion Ratio in Cold Rolled Advanced High Strength Steels (Master thesis), Colorado School of Mines, 2016.
22. Effects of microstructure on stretch-flange-formability of 980 MPa grade cold-rolled ultra high strength steel sheets10.2355/isijinternational.44.603 ↗
23. Hole expansion of dual‐phase and complex‐phase AHS steels‐effect of edge conditions
24. Effects of retained austenite parameters on warm stretch-flangeability in TRIP-aided dual-phase sheet steels10.2355/isijinternational.39.56 ↗
25. E. De Moor, D.K. Matlock, J.G. Speer, C. Fojer, J. Penning, Comparison of hole expansion properties of quench & partitioned, quench & tempered and austempered steels, SAE Technical Paper, 2012.10.4271/2012-01-0530 ↗
26. R. Johnson, E. De Moor, N. Fonstein, D. Hanlon, A. Pichler, Retained austenite effects on hole expansion of ultra-high strength steels, Proceedings of the International Symposium on New Developments in Advanced High Strength Sheet Steels. PA: AIST, 2013.
27. I.O.f. Standardization · 2009
28. The effect of morphology on the stability of retained austenite in a quenched and partitioned steel10.1016/j.scriptamat.2012.11.003 ↗
29. Stretch‐flangeability of High Mn TWIP steel10.1002/srin.201000044 ↗
30. Effect of retained austenite on formability of high strength sheet steels10.2355/isijinternational.32.1110 ↗
31. Edge cracking in high strength steels10.1007/BF02833914 ↗
32. Effect of fresh martensite on the stability of retained austenite in quenching and partitioning steel10.1016/j.msea.2014.07.054 ↗
33. Correlation between fracture toughness and stretch-flangeability of advanced high strength steels10.1016/j.matlet.2016.05.145 ↗
34. Relationship between microstructure, mechanical properties and damage mechanisms in high martensite fraction dual phase steels10.2355/isijinternational.ISIJINT-2015-186 ↗
35. Correlation of yield strength and tensile strength with hardness for steels10.1007/s11665-008-9225-5 ↗
36. Failure during sheared edge stretching of dual-phase steels10.1007/s11661-013-1718-7 ↗