The role of Cr additions and Fe-rich compounds on microstructural features and impact toughness of AlSi9Cu3(Fe) diecasting alloys
Source abstract
Abstract
Abstract The effect of chromium content on the microstructural evolution of primary and secondary Fe-rich compounds in a high-pressure die-cast AlSi9Cu3(Fe) alloy is reported and then addressed to the impact toughness of the material. Metallographic and image analysis techniques have been used to quantitatively examine the microstructural changes occurring at different Cr levels. The results reveal that the salient microstructural features of diecastings, such as segregation bands and externally solidified grains, are not affected by Cr content, which contrary promotes the formation of primary sludge particles and proeutectic α-Al x (Fe,Mn,Cr) y Si z intermetallic compounds. Any increase in the amount of these Fe-rich particles is coupled with an increase in their size. Upon increasing the Cr level, the modification of sludge morphology from more or less well-formed hexagon to branched or star-like shapes occurs. The polyhedral sludge is associated to a regular rhombic dodecahedron, while the star-like and branched morphologies originate from hollowed rhombic dodecahedron. On the other hand, the morphology of secondary Fe-rich particles seems to not be influenced by Cr content and mainly determined by high cooling rate of diecasting. The impact toughness and the maximum load of the diecast AlSi9Cu3(Fe) alloy decrease as the Cr level exceeds 0.12 wt%.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Metallurgy and Material Science
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. J.W. Bray, in: ASM International Handbook Committee (Eds.), Aluminum Mill and Engineered Wrought Products, ASM Handbook, vol. 2, ASM International, The Materials Information Society, Materials Park, OH, 1990, pp. 118–177.
2. Cho · Mater. Sci. Forum · 2006 · 519–521 · 46110.4028/www.scientific.net/MSF.519-521.461 ↗
3. Lodgaard · Mater. Sci. Eng. A · 2000 · 283 · 14410.1016/S0921-5093(00)00734-6 ↗
4. Kim · Mater. Lett. · 2006 · 60 · 188010.1016/j.matlet.2005.12.042 ↗
5. Eidhed · J. Mater. Sci. Technol. · 2008 · 24 · 4510.1179/174328407X248523 ↗
6. Mahta · Int. J. Cast Met. Res. · 2005 · 18 · 7310.1179/136404605225022928 ↗
7. L.A. Narayanan, Crystallization and Dissolution studies of Iron Intermetallics in Al–Si Alloys (PhD dissertation), McGill University, Montreal, Quebec, Canada, 1994.
8. M.M. Makhlouf, D. Apelian, Casting Characteristics of Aluminum Die Casting Alloys. 〈http://metalcasting.govtools.us/reports/casting_characteristics_of_aluminum.pdf〉 (accessed 5.2.02).
9. Shabestari · Mater. Sci. Eng. A · 2004 · 383 · 28910.1016/j.msea.2004.06.022 ↗
10. Shabestari · Metall. Mater. Trans. A · 1995 · 26 · 99910.1007/BF02649097 ↗
11. Wallace · 2006
12. Jorstad · Die Cast. Eng. · 1986 · 11/12 · 30
13. Gobrecht · Giesserei · 1975 · 61 · 263
14. Wang · Int. J. Cast Met. Res. · 2003 · 16 · 40910.1080/13640461.2003.11819617 ↗
15. Cao · Int. J. Cast Met. Res. · 2004 · 17 · 110.1179/136404604225014792 ↗
16. Makhlouf · 1998
17. Conserva · Diecasting Foundry Tech. · 2013 · 8 · 28
18. EN 1706, Aluminium and Aluminium Alloys – Castings – Chemical Composition and Mechanical Properties, 2010.
19. Timelli · Mater. Sci. Eng. A · 2010 · 528 · 27310.1016/j.msea.2010.08.079 ↗
20. ASTM E2298-13a · 2013 · 1
21. Gourlay · Metall. Mater. Trans. A · 2007 · 38 · 183310.1007/s11661-007-9243-1 ↗
22. Otarawanna · Metall. Mater. Trans. A · 2009 · 40 · 164510.1007/s11661-009-9841-1 ↗
23. Gourlay · Nature · 2007 · 445 · 7010.1038/nature05426 ↗
24. Meylan · Scr. Mater. · 2010 · 63 · 118510.1016/j.scriptamat.2010.08.032 ↗
25. L. Bäckerud, G. Chai, J. Tamminen, Foundry Alloys, first ed., vol. 2, American Foundrymen׳s Society Inc., Des Plaines, IL, 1990.
26. Makhlouf · J. Light Met. · 2001 · 1 · 19910.1016/S1471-5317(02)00003-2 ↗
27. Laukli · Mater. Sci. Eng. A · 2005 · 413–414 · 9210.1016/j.msea.2005.08.194 ↗
28. Otarawanna · Mater. Charact. · 2009 · 60 · 143210.1016/j.matchar.2009.06.016 ↗
29. Laukli · Metall. Mater. Trans. A · 2005 · 36 · 80510.1007/s11661-005-1011-5 ↗
30. Kral · Mater. Lett. · 2005 · 59 · 227110.1016/j.matlet.2004.05.091 ↗
31. Orozco-González · Rev. Metall. · 2011 · 47 · 45310.3989/revmetalm.1068 ↗
32. Wang · Mater. Des. · 2011 · 32 · 433310.1016/j.matdes.2011.04.005 ↗
33. Murali · Mater. Charact. · 1994 · 33 · 9910.1016/1044-5803(94)90072-8 ↗
34. A. Fabrizi, S. Ferraro, G. Timelli, in: M. Tiryakiogˇlu, J. Campbell, G. Byczynski (Eds.), Shape Casting 5: International Symposium 2014, John Wiley and Sons, Inc., Hoboken, New Jersey, 2014, pp. 277–284.
35. Kim · Mater. Sci. Forum · 2010 · 654–656 · 97410.4028/www.scientific.net/MSF.654-656.974 ↗
36. Šerák · Aluminium · 2002 · 78 · 384
37. Seifeddine · Mater. Sci. Eng. A · 2008 · 490 · 38510.1016/j.msea.2008.01.056 ↗
38. ISO 14556, Steel – Charpy V-Notch Pendulum Impact Test – Instrumented Test Method, 2010.
39. Green · J. Mech. Phys. Solids · 1965 · 4 · 12810.1016/0022-5096(56)90085-0 ↗
40. Server · 1978 · 100 · 183
41. Alexopoulos · Mater. Sci. Eng. A · 2011 · 528 · 630310.1016/j.msea.2011.04.086 ↗
42. Stepanov · Strength Mater. · 1985 · 17 · 110210.1007/BF01533792 ↗
43. Klepaczko · J. Mech. Phys. Solids · 1998 · 46 · 213910.1016/S0022-5096(98)00025-8 ↗
44. Kobayashi · Eng. Fract. Mech. · 1984 · 19 · 6710.1016/0013-7944(84)90069-9 ↗
45. Cáceres · Acta Mater. · 1996 · 44 · 2510.1016/1359-6454(95)00172-8 ↗
46. Wang · Metall. Mater. Trans. A · 2003 · 34 · 288710.1007/s11661-003-0189-7 ↗