Effect of Y addition on the aging hardening behavior and precipitation evolution of extruded Mg-Al-Zn alloys
Source abstract
Abstract
Abstract: The 443 K aging hardening behavior and microstructure evolution of extruded Mg-Al-Zn-Y alloys was investigated in aspects of yttrium (Y) content (0.2–0.8 wt%), holding time (0.5–156 h) and the initial states (as-extruded, solution treated). The grain size, precipitation evolution, phases and chemical composition were characterized by the optical microscope, scanning electron microscope, X-ray diffraction, and energy dispersive spectrometer, respectively. The corresponding mechanical response, including the hardness, uniaxial tensile strength were measured with the Vickers hardness tester and universal testing machine, respectively. The results show that, firstly, there is reversal hardness anisotropy between extrusion direction and normal direction in as-extruded Mg-Al-Zn-Y sheets compared with T5 treated ones. Secondly, the short-term aging softening exist at the beginning of T5 treatment which results in a lower hardness even be close to that of solution treated ones, but not for T6 conditions. Thirdly, the suppression of discontinuous precipitation during the aging treatment become more remarkable with increasing Y addition which because of the reduction of diffusional coherency strain near grain boundary, increasing activation energy for the discontinuous precipitates (β-Mg17Al12 phase, DPs) formation and the dilution region of Al near the Al2Y. Serrated GBs can also provide more nucleation sites for DPs and lead to relatively more precipitates during T5 treatment. Moreover, the proportional precipitation strengthening in yield strength and hardness was verified in Mg-Al-Zn-Y alloy during the aging process.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Plastic behavior of AZ80 alloy during low strain rate tension at elevated temperature10.1016/j.msea.2014.06.004 ↗
2. Process and property of superplastic mould forged AZ80 wheel hub10.4028/www.scientific.net/MSF.788.12 ↗
3. , Phase diagrams of binary magnesium alloys
4. On the competition between continuous and discontinuous precipitations in binary Mg-Al alloys
5. Discontinuous and continuous precipitation in magnesium–aluminium type alloys10.1016/j.jallcom.2008.11.008 ↗
6. Effect of micro-alloying elements on deformation behavior in Mg-Y binary alloys10.2320/matertrans.M2013303 ↗
7. Microalloying effects of Ca and Ni on high-temperature creep behavior in Mg-Y-Zn Alloys10.2320/matertrans.MC200722 ↗
8. Effect of heat treatment and pre-deformation on damping capacity of cast Mg-Y binary alloys10.1016/j.jallcom.2016.12.299 ↗
9. The role of Al 2 Y in grain refinement in Mg–Al–Y alloy system10.1016/j.jma.2013.07.006 ↗
10. A new approach to designing a grain refiner for Mg casting alloys and its use in Mg–Y-based alloys10.1016/j.actamat.2009.03.011 ↗
11. Corrosive wear resistance of Mg–Al–Zn alloys with alloyed yttrium10.1016/j.wear.2013.01.013 ↗
12. First-principles study of structural stabilities and elastic properties of Mg17Al12, Al2Y and Al2Ca phases
13. Precipitation and hardening in magnesium alloys10.1007/s11661-012-1217-2 ↗
14. Effects of cerium on microstructures, recovery behavior and mechanical properties of backward extruded Mg–0.5Mn alloys10.1016/j.msea.2012.11.107 ↗
15. Acceleration or suppression of α-phase precipitation using isothermal ω, phase in Ti-20 at.pct Nb alloy10.1007/s11661-013-2092-1 ↗
16. Suppression of discontinuous precipitation in AZ91 by the addition of Sn10.1007/s12540-013-6008-9 ↗
17. The effect of Ca and RE elements on the precipitation kinetics of Mg17Al12, phase during artificial aging of magnesium alloy AZ9110.1016/j.msea.2011.03.022 ↗
18. The effect of gold additions on the ageing behaviour and creep properties of the magnesium alloy AZ91E10.1016/S0921-5093(02)00731-1 ↗
19. The microstructure and impression creep behavior of cast AZ80 magnesium alloy with yttrium additions10.1016/j.matdes.2012.02.036 ↗
20. A test for diffusional coherency strain hypothesis in the discontinuous precipitation in Mg-Al alloy10.1007/BF02720085 ↗
21. Effect of Pb and Sb additions on the precipitation kinetics of AZ91 magnesium alloy10.1016/j.msea.2006.12.132 ↗
22. Shock wave propagation and spall failure in single crystal Mg at atomic scales10.1063/1.4944942 ↗
23. Callister · 2001 · 180
24. Recrystallization and texture evolution of Mg–3%Al–1%Zn–(0.4–0.8)%Sr alloys during extrusion10.1016/j.msea.2010.10.096 ↗
25. Microstructures and mechanical properties of Mg-Al-Ca alloys affected by Ca/Al ratio10.1016/j.msea.2015.03.100 ↗
26. Jackson · 2010 · 7 · 63
27. Ag precipitation and dissolution reactions in the Cu–3wt% Al–4wt% Ag alloy10.1016/j.msea.2006.08.055 ↗
28. Dynamic continuous recrystallization characteristics in two stage deformation of Mg–3Al–1Zn alloy sheet10.1016/S0921-5093(02)00096-5 ↗