Assessment of the potential of hydrogen plasma charging as compared to conventional electrochemical hydrogen charging on dual phase steel
Source abstract
Abstract
Abstract The present study evaluates the hydrogen induced damage by in-situ hydrogen plasma charging in dual phase (DP) steel. Cold deformation of 15% is applied on the material to change microstructural defects, such as dislocation density. The susceptibility to hydrogen embrittlement is hence evaluated for two material conditions, i.e. DP 0% and DP 15%. Small scale tensile tests are done inside an ESEM chamber for which in-situ hydrogen plasma charging is compared with electrochemical hydrogen charging while uncharged samples serve as a reference. Generally, the hydrogen effect on the ductility and stress level is increased when deformation is applied, due to the hydrogen trapping ability of the deformation induced defects, as confirmed by thermal desorption spectroscopy. Complementary in-situ electrochemical nanoindentation tests verify the more pronounced hardness increase due to hydrogen when cold deformation is applied. A slightly increased ductility loss is observed when the samples are charged electrochemically, although similar tendencies are found for both hydrogen charging procedures. These observations are confirmed by the fractographic analysis, where the detrimental role of MnS inclusions in the segregation line on hydrogen induced cracking is demonstrated as well.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (60)
Show source-provided references
1. Thermal desorption spectroscopy study of the interaction between hydrogen and different microstructural constituents in lab cast Fe-C alloys10.1016/j.corsci.2012.08.017 ↗
2. Internal and surface damage of multiphase steels and pure iron after electrochemical hydrogen charging10.1016/j.corsci.2011.05.060 ↗
3. Determination of the equivalent hydrogen fugacity during electrochemical charging of 3.5NiCrMoV steel10.1016/j.corsci.2017.12.018 ↗
4. Electrochemical and mechanical aspects of hydrogen embrittlement evaluation of martensitic steels
5. Recent developments in the study of hydrogen embrittlement: hydrogen effect on dislocation nucleation10.1016/j.actamat.2010.05.057 ↗
6. Influence of hydrogen on the elastic properties of nickel single crystal: a numerical and experimental investigation10.1016/j.actamat.2018.01.056 ↗
7. Precise determination of the activation energy for desorption of hydrogen in two Ti-added steels by a single thermal-desorption spectrum10.1007/s11663-004-0057-x ↗
8. Thermal desorption spectroscopy study of the interaction of hydrogen with TiC precipitates10.1007/s12540-013-4013-7 ↗
9. Hydrogen diffusivity and tensile-ductility loss of solution-treated austenitic stainless steels with external and internal hydrogen10.1016/j.ijhydene.2017.04.055 ↗
10. Comparative study of hydrogen embrittlement in stable and metastable high-entropy alloys10.1016/j.scriptamat.2018.03.003 ↗
11. Overview of hydrogen embrittlement in high-Mn steels10.1016/j.ijhydene.2017.02.214 ↗
12. On the environmental similitude for fracture in the SENT specimen and a cracked hydrogen gas pipeline10.1016/j.engfracmech.2011.06.002 ↗
13. Hydrogen-induced intergranular failure in nickel revisited10.1016/j.actamat.2012.01.040 ↗
14. In-situ micro-cantilever bending test in environmental scanning electron microscope: real time observation of hydrogen enhanced cracking10.1016/j.scriptamat.2016.08.026 ↗
15. In situ micromechanical testing in environmental scanning electron microscope: a new insight into hydrogen-assisted cracking10.1016/j.actamat.2017.10.037 ↗
16. Hydrogen trapping and hydrogen induced mechanical degradation in lab cast Fe-C-Cr alloys10.1016/j.msea.2016.05.018 ↗
17. Evaluation of the role of Mo2C in hydrogen induced ductility loss in Q&T Fe-C-Mo alloys10.1016/j.ijhydene.2016.05.176 ↗
18. Evaluation of the effect of V4C3 precipitates on the hydrogen induced mechanical degradation in Fe-C-V alloys10.1016/j.msea.2016.08.053 ↗
19. The effect of TiC on the hydrogen induced ductility loss and trapping behavior of Fe-C-Ti alloys10.1016/j.corsci.2016.07.013 ↗
20. The detrimental effect of mobile hydrogen at dislocations on the hydrogen embrittlement susceptibility of Fe-C-X alloys: an experimental proof of the HELP mechanism10.1016/j.ijhydene.2017.12.109 ↗
21. Hydrogen induced mechanical degradation in tungsten alloyed steels10.1016/j.matchar.2017.12.017 ↗
22. Hydrogen embrittlement effect observed by in-situ hydrogen plasma charging on a ferritic alloy10.1016/j.scriptamat.2018.03.038 ↗
23. Embrittlement of Fe-Si alloy crystals by hydrogen glow discharge10.1016/0036-9748(84)90274-6 ↗
24. Plastic softening by hydrogen plasma charging in pure iron10.1016/0036-9748(87)90406-6 ↗
25. Hydrogen-assisted decohesion and localized plasticity in dual-phase steel10.1016/j.actamat.2014.01.048 ↗
26. The role of the microstructure on the influence of hydrogen on some advanced high-strength steels10.1016/j.msea.2017.12.079 ↗
27. Analysis of hydrogen diffusion and trapping in ultra-high strength steel grades10.1016/j.jallcom.2018.02.264 ↗
28. A lamellar structured ultrafine grain ferrite-martensite dual-phase steel and its resistance to hydrogen embrittlement10.1016/j.jallcom.2016.12.224 ↗
29. An overview of dual phase steels: advances in microstructure-oriented processing and micromechanically guided design10.1146/annurev-matsci-070214-021103 ↗
30. Fractographic analysis of the role of hydrogen diffusion on the hydrogen embrittlement susceptibility of DP steel10.1016/j.msea.2015.09.124 ↗
31. Effect of martensite distribution on damage behaviour in DP600 dual phase steels10.1016/j.msea.2009.03.055 ↗
32. Hydrogen embrittlement in HSSs limits use in lightweight body
33. Effect of in-situ hydrogen charging on the mechanical properties of advanced high strength steels10.1016/j.ijhydene.2013.12.190 ↗
34. Hydrogen-enhanced-plasticity mediated decohesion for hydrogen-induced intergranular and “quasi-cleavage”fracture of lath martensitic steels10.1016/j.jmps.2017.12.016 ↗
35. Modeling hydrogen transport by dislocations10.1016/j.jmps.2015.03.002 ↗
36. Effect of hydrogen on the collective behavior of dislocations in the case of nanoindentation10.1016/j.actamat.2018.01.053 ↗
37. Multiscale modeling of hydrogen enhanced homogeneous dislocation nucleation10.1016/j.actamat.2016.01.036 ↗
38. Hydrogen embrittlement revealed via novel in situ fracture experiments using notched micro-cantilever specimens10.1016/j.actamat.2017.09.057 ↗
39. Reduction of thin oxide films on tungsten substrate with highly reactive cold hydrogen plasma10.1002/sia.3185 ↗
40. On the determination of the hydrogen fugacity in an environmental cell TEM facility10.1016/0036-9748(86)90484-9 ↗
41. Hydrogen embrittlement in high purity iron single crystals10.1016/0025-5416(86)90355-1 ↗
42. In situ small-scale hydrogen embrittlement testing made easy: an electrolyte for preserving surface integrity at nano-scale during hydrogen charging”10.1016/j.ijhydene.2018.04.168 ↗
43. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
44. Hydrogen trapping in AISI-4340 steel10.1179/030634583790420619 ↗
45. Hydrogen trapping phenomena in metals with bcc and fcc crystal structures by the desorption thermal-analysis technique10.1016/0257-8972(86)90087-3 ↗
46. The trapping and transport phenomena of hydrogen in nickel
47. Reaction kinetics in differential thermal analysis10.1021/ac60131a045 ↗
48. Porter · 1992
49. „Hydrogen permeation through deformed and10.1080/02670836.2017.1342015 ↗
50. Hydrogen embrittlement of an interstitial equimolar high-entropy alloy10.1016/j.corsci.2018.03.040 ↗
51. Effect of hydrogen on the mechanical properties of multiphase high strength steels
52. On the synergy of diffusible hydrogen content and hydrogen diffusivity in the mechanical degradation of laboratory cast Fe-C alloys10.1016/j.msea.2016.03.107 ↗
53. In situ electrochemical microcantilever bending test: a new insight into hydrogen enhanced cracking10.1016/j.scriptamat.2017.01.019 ↗
54. Combined thermal desorption spectroscopy, differential scanning calorimetry, scanning electron microscopy and X-ray diffraction study of hydrogen trapping in cold deformed TRIP steel10.1016/j.actamat.2012.01.026 ↗
55. Thermal analysis of trapped hydrogen in pure iron
56. Effects of hydrogen on the properties of iron and steel
57. Classification of hydrogen traps in steel
58. Trap-governed hydrogen diffusivity and uptake capacity in ultrahigh strength aermet 100 steel10.1007/s11661-002-0032-6 ↗
59. Evaluation of the hydrogen embrittlement susceptibility in DP steel under static and dynamic tensile conditions10.1016/j.ijimpeng.2018.10.002 ↗
60. Factors affecting hydrogen-assisted cracking in a commercial tempered martensitic steel: Mn segregation, MnS, and the stress state around abnormal cracks10.1016/j.msea.2015.05.083 ↗