journal article·2020-06

Impact of hot isostatic pressing on the mechanical and microstructural properties of additively manufactured Ti–6Al–4V fabricated using directed energy deposition

J.S. Keist, S. Nayir, T.A. Palmer

Publisher page

Abstract

Abstract Laser and electron beam (EB) based directed energy deposition (DED) additive manufacturing (AM) processes, followed by hot isostatic pressing (HIP), are potential routes for producing large Ti–6Al–4V structures. Changes in the heat input between the laser DED and EB DED processes impacted the as-deposited and HIP post processed microstructures and mechanical properties for different wall thicknesses and orientations. The significantly lower as-deposited strengths observed in the higher heat input EB DED builds were attributed to losses of important alloying elements and coarsening of prior beta (β) grains and alpha (α) lath structures. These coarsened microstructural features also produced similar properties across the builds, minimizing location and orientation specific changes in properties observed in the laser DED builds. When materials were subjected to HIP post processing, the α-lath structures further coarsened in both the laser DED and EB DED builds, leading to a general decrease in strength. A comparison between the as-deposited and HIP yield strengths showed that the higher strength as-deposited laser DED builds displayed larger decreases in strength than the EB DED builds after HIP post processing. However, the orientation specific strength relationships observed in the as-deposited laser DED builds were only reduced and not eliminated after HIP post-processing. Interactions between chemical composition and α-lath thickness on the mechanical properties were further evaluated using a conventional strengthening model, and the magnitude of each contribution on yield strength was determined for each processing route in the as-deposited and HIP conditions.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (59)

Show source-provided references
1. Role of geometry on properties of additively manufactured Ti-6Al-4V structures fabricated using laser based directed energy deposition10.1016/j.matdes.2016.05.045 ↗
2. Wire based additive layer manufacturing: comparison of microstructure and mechanical properties of Ti-6Al-4V components fabricated by laser-beam deposition and shaped metal deposition10.1016/j.jmatprotec.2011.01.018 ↗
3. Progress toward an integration of process-structure-property-performance models for "three-dimensional (3-D) printing" of titanium alloys
4. Development of strength-hardness relationships in additively manufactured titanium alloys10.1016/j.msea.2017.03.102 ↗
5. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
6. Optimisation of process parameters to address fundamental challenges during selective laser melting of Ti-6Al-4V: a review10.1016/j.ijmachtools.2018.01.003 ↗
7. Metal additive manufacturing: a review of mechanical properties10.1146/annurev-matsci-070115-032024 ↗
8. Local and global mechanical behavior and microstructure of Ti6Al4V parts built using electron beam melting technology10.1007/s11661-015-2965-6 ↗
9. Direct metal laser melting of Inconel 718: process impact on grain formation and orientation10.1016/j.jallcom.2017.11.130 ↗
10. Impact of interlayer dwell time on microstructure and mechanical properties of nickel and titanium alloys10.1007/s11661-017-4164-0 ↗
11. Microstructure and mechanical properties of wire and arc additive manufactured Ti-6Al-4V10.1007/s11661-012-1444-6 ↗
12. Rapid manufacturing of metal components by laser forming10.1016/j.ijmachtools.2005.09.005 ↗
13. Electron beam melted Ti-6Al-4V: microstructure, texture and mechanical behavior of the as-built and heat-treated material10.1016/j.msea.2015.11.052 ↗
14. Additive manufactured Ti-6Al-4V using welding wire: comparison of laser and are beam deposition and evaluation with respect to aerospace material specifications10.1016/j.phpro.2010.08.087 ↗
15. Microtexture in additively manufactured Ti-6Al-4V fabricated using directed energy deposition10.1016/j.msea.2018.07.098 ↗
16. The origin of microstructural diversity, texture, and mechanical properties in electron beam melted Ti-6Al-4V10.1007/s11661-010-0397-x ↗
17. Fabrication of large Ti-6Al-4V structures by direct laser deposition10.1016/j.jallcom.2014.12.234 ↗
18. Temperature profile, bead geometry, and rlemental rvaporation in laser powder bed fusion additive manufacturing process
19. A comparative study of additive manufacturing techniques: residual stress and microstructural analysis of CLAD and WAAM printed Ti-6Al-4V components10.1016/j.matdes.2015.09.115 ↗
20. Structure‐property correlations for additively manufactured Ti‐6Al‐4V components produced using directed energy deposition processes
21. Additive manufacturing of metals: a brief review of the characteristic microstructures and properties of steels, Ti-6Al-4V and high-entropy alloys10.1080/14686996.2017.1361305 ↗
22. Optimising the mechanical properties of Ti-6Al-4V components produced by wire+ arc additive manufacturing with post-process heat treatments10.1016/j.jallcom.2018.04.158 ↗
23. Fatigue behavior and failure mechanisms of direct laser deposited Ti-6Al-4V10.1016/j.msea.2015.12.026 ↗
24. Review of mechanical properties of Ti-6Al-4V made by laser-based additive manufacturing using powder feedstock
25. Effects of heat treatments on microstructure and properties of Ti-6Al-4V ELI alloy fabricated by electron beam melting (EBM)10.1016/j.msea.2017.01.019 ↗
26. Influences of post-processing, location, orientation, and induced porosity on the dynamic compression behavior of Ti–6Al–4V alloy built through additive manufacturing10.1007/s40870-018-0157-3 ↗
27. Investigation of the mechanisms by which hot isostatic pressing improves the fatigue performance of powder bed fused Ti-6Al-4V10.1016/j.ijfatigue.2018.10.015 ↗
28. Microstructure and mechanical properties of long Ti-6Al-4V rods additively manufactured by selective electron beam melting out of a deep powder bed and the effect of subsequent hot isostatic pressing10.1007/s11661-015-2976-3 ↗
29. Microstructure and tensile properties of selectively laser-melted and of HIPed laser-melted Ti-6Al-4V10.1016/j.msea.2013.04.099 ↗
30. The positive effect of hot isostatic pressing on improving the anisotropies of bending and impact properties in selective laser melted Ti-6Al-4V alloy10.1016/j.msea.2016.02.023 ↗
31. Fatigue characterization of titanium Ti-6A1-4V samples produced by additive manufacturing
32. Mechanical properties and microstructural features of direct laser-deposited Ti-6Al-4V
33. Critical assessment of the fatigue performance of additively manufactured Ti-6Al-4V and perspective for future research10.1016/j.ijfatigue.2015.12.003 ↗
34. Effects of defects, surface roughness and HIP on fatigue strength of Ti-6Al-4V manufactured by additive manufacturing
35. 2008
36. Quantification of microstructural features in alpha/beta titanium alloys10.1016/j.msea.2003.12.008 ↗
37. 2012 · 27
38. 2013
39. 2009
40. 2010
41. 2013
42. Thermal and microstructural analysis of laser-based directed energy deposition for Ti-6Al-4V and Inconel 625 deposits10.1016/j.msea.2018.01.060 ↗
43. Microstructural evolution in laser-deposited multilayer Ti-M-4V builds: Part I. Microstructural characterization10.1007/s11661-004-0094-8 ↗
44. Microstructural evolution in laser-deposited multilayer Ti-6AI-4V builds: Part II. Thermal modeling10.1007/s11661-004-0095-7 ↗
45. 2013 · 8
46. 2011
47. Additive manufacturing and postprocessing of Ti-6Al-4V for superior mechanical properties10.1557/mrs.2016.215 ↗
48. Influence of microstructure on mechanical properties of laser metal wire-deposited Ti-6Al-4V10.1016/j.msea.2016.07.038 ↗
49. Anisotropic properties of directed energy deposition (DED)-processed Ti-6Al-4V10.1016/j.jmapro.2016.06.020 ↗
50. Effect of deposition parameters on mechanical properties of shaped metal deposition parts10.1177/0954405411403669 ↗
51. Correlations between microstructure characteristics and mechanical properties in 5183 aluminium alloy fabricated by wire-arc additive manufacturing with different arc modes10.3390/ma11112075 ↗
52. Yield strength prediction of titanium alloys
53. A constitutive equation relating composition and microstructure to properties in Ti-6Al-4V: as derived using a novel integrated computational approach10.1007/s11661-015-3072-4 ↗
54. Developing a phenomenological equation to predict yield strength from composition and microstructure in beta processed Ti-6Al-4V10.1016/j.msea.2016.02.052 ↗
55. Advanced metal powder based manufacturing of complex components by electron beam melting10.1179/106678509X12475882446133 ↗
56. Additive manufacturing of titanium alloys by electron beam melting: a review10.1002/adem.201700842 ↗
57. Predicting tensile properties of Ti-6Al-4V produced via directed energy deposition10.1016/j.actamat.2017.05.025 ↗
58. The effect of alpha platelet thickness on plastic flow during hot working of Ti-6Al-4V with a transformed microstructure10.1016/S1359-6454(01)00236-1 ↗
59. Dynamic response of conventional and hot isostatically pressed Ti-6Al-4V alloys: experiments and modeling10.1016/S0167-6636(01)00063-1 ↗