Improved workability for Mg-Y-Zn alloys via increased volume fraction of block LPSO phases
Source abstract
Abstract
Abstract As one aspect of LPSO morphology, the volume fraction of block LPSO phases (VFLPSO-B) was tailored by changing the total content of solute atoms in Mg-Y2x-Znx (x = 1, 0.5, and 0.25 at.%) alloys. The effects of VFLPSO-B on compression behavior, dynamic recrystallization (DRX), and workability were investigated. The results reveal that increasing VFLPSO-B leads to higher flow stress, hardness, DRX ratio, and better workability which is embodied in the lower deformation activation energy (Q), broader deformable conditions, and narrower improper processing domains. Kink bands and initial grain boundaries are ideal sites for the nucleation of DRX grains during compression. Block LPSO phases near the initial grain boundaries further promote the nucleation of DRX grains but inhibit their growth, which contributes to increasing the DRXed grain size exponent (m). This paper reveals the feasibility of improving the workability of LPSO-containing Mg alloys by modifying the LPSO morphology to broaden their applications.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Metal and Thin Film Mechanics · Hydrogen Storage and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Fabrication of a high strength Mg-11Gd-4.5Y-1Nd-1.5Zn-0.5Zr (wt%) alloy by thermomechanical treatments10.1016/j.msea.2014.10.077 ↗
2. Recent developments in high-strength Mg-RE-based alloys: focusing on Mg-Gd and Mg-Y systems10.1016/j.jma.2018.08.001 ↗
3. Fabrication of high-strength AZ80 alloys via multidirectional forging in air with no need of ageing treatment10.1016/j.jallcom.2019.02.133 ↗
4. Strain path dependent evolutions of microstructure and texture in AZ80 magnesium alloy during hot deformation10.1016/j.jallcom.2019.07.262 ↗
5. Recent progress in magnesium hydride modified through catalysis and nanoconfinement10.1016/j.ijhydene.2017.11.135 ↗
6. Enhanced hydrogen storage properties and mechanisms of magnesium hydride modified by transition metal dissolved magnesium oxides10.1016/j.ijhydene.2018.10.017 ↗
7. Influences and mechanisms of graphene-doping on dehydrogenation properties of MgH2: experimental and first-principles studies10.1016/j.energy.2015.06.037 ↗
8. Catalytic effect and mechanism of NiCu solid solutions on hydrogen storage properties of MgH210.1016/j.renene.2020.03.089 ↗
9. Novel Mg-based alloys by selective laser melting for biomedical applications: microstructure evolution, microhardness and in vitro degradation behaviour10.1080/17452759.2017.1411662 ↗
10. In vitro degradation behavior and cytocompatibility of ZK30/bioactive glass composites fabricated by selective laser melting for biomedical applications10.1016/j.jallcom.2019.01.165 ↗
11. Biodegradable magnesium matrix composites: a review10.1007/s12613-020-1987-2 ↗
12. Rapidly solidified powder metallurgy Mg97Zn1Y2 alloys with excellent tensile yield strength above 600 MPa10.2320/matertrans.42.1172 ↗
13. Achieving ultra-high hardness of nanostructured Mg-8.2Gd-3.2Y-1.0Zn-0.4Zr alloy produced by a combination of high pressure torsion and ageing treatment10.1016/j.scriptamat.2018.06.009 ↗
14. Formation and mechanical properties of Mg97Zn1RE2 alloys with long-period stacking ordered structure10.2320/matertrans.MER2007142 ↗
15. The effect of LPSO phase on hot deformation behavior and dynamic recrystallization evolution of Mg–2.0Zn–0.3Zr–5.8Y alloy10.1016/j.msea.2013.05.022 ↗
16. The effect of 14H LPSO phase on dynamic recrystallization behavior and hot workability of Mg–2.0Zn–0.3Zr–5.8Y alloy10.1016/j.msea.2014.01.079 ↗
17. Hot compression behavior of the Mg-Gd-Y-Zn-Zr alloy filled with intragranular long-period stacking ordered phases10.1016/j.jallcom.2017.07.088 ↗
18. The roles of long period stacking ordered structure and Zn solute in the hot deformation behavior of Mg-Gd-Zn alloys10.1016/j.jallcom.2018.02.149 ↗
19. The 18R and 14H long-period stacking ordered structures in Mg–Y–Zn alloys10.1016/j.actamat.2010.01.022 ↗
20. Evolution of LPSO phases and their effect on dynamic recrystallization in a Mg-Gd-Y-Zn-Zr alloy10.1007/s11661-017-4081-2 ↗
21. Mechanical properties of the Mg-Gd-Y-Zn-Zr alloys with different morphologies of long-period stacking ordered phases10.1007/s11665-018-3713-z ↗
22. Effect of morphology of long period stacking ordered phase on mechanical properties of Mg-10Gd-1Zn-0.5Zr magnesium alloy10.1016/j.msea.2018.04.079 ↗
23. Growth and transformation mechanisms of 18R and 14H in Mg–Y–Zn alloys10.1016/j.actamat.2012.08.022 ↗
24. Effect of the LPSO volume fraction on the microstructure and mechanical properties of Mg–Y2X–ZnX alloys10.1007/s10853-011-5899-4 ↗
25. Improved workability and ductility of the Mg-Gd-Y-Zn-Zr alloy via enhanced kinking and dynamic recrystallization10.1016/j.jallcom.2018.03.359 ↗
26. Effect of the morphology of long-period stacking ordered phase on mechanical properties and corrosion behavior of cast Mg-Zn-Y-Ti alloy10.1016/j.jallcom.2018.06.056 ↗
27. Microstructure evolution and mechanical properties of magnesium alloys containing long period stacking ordered phase10.1016/j.matchar.2018.04.044 ↗
28. The role of long period stacking ordered phase in dynamic recrystallization of a Mg–Zn–Y alloy during hot compression10.1016/j.jallcom.2019.152814 ↗
29. Modeling of hardening and softening processes in Mg alloys10.1016/j.jallcom.2003.10.098 ↗
30. Hot tensile deformation and fracture behaviors of AZ31 magnesium alloy10.1016/j.matdes.2013.01.023 ↗
31. Long period stacking structures observed in Mg97Zn1Y2 alloy10.1016/j.scriptamat.2004.04.003 ↗
32. Elastic properties of an Mg–Zn–Y alloy single crystal with a long-period stacking-ordered structure10.1016/j.actamat.2013.06.041 ↗
33. The relevance of dynamic recrystallization in the hot deformation of IF steel at high strain rates10.1016/j.msea.2006.12.003 ↗
34. Grain size control of commercial wrought Mg-Al-Zn alloys utilizing dynamic recrystallization10.2320/matertrans.42.1200 ↗
35. Quasi-static and dynamic forced shear deformation behaviors of Ti-5Mo-5V-8Cr-3Al alloy10.1016/j.msea.2017.03.005 ↗
36. Particle effects on recrystallization in magnesium–manganese alloys: particle-stimulated nucleation10.1016/j.actamat.2009.02.032 ↗
37. Hot deformation and dynamic recrystallization behaviors of Mg-Gd-Y-Zr alloy10.1016/j.msea.2015.01.041 ↗
38. Effect of final rolling reduction on the microstructure and mechanical properties of Mg–Gd–Y–Zn–Zr alloy sheets10.1016/j.msea.2012.08.089 ↗
39. On the Zener drag10.1016/0001-6160(85)90214-7 ↗
40. Processing and properties of Mg-6Gd-1Zn-0.6Zr: Part 1-recrystallization and texture development10.1016/j.msea.2010.12.100 ↗
41. Texture evolution, deformation mechanism and mechanical properties of the hot rolled Mg-Gd-Y-Zn-Zr alloy containing LPSO phase10.1016/j.msea.2018.06.062 ↗
42. Plastic deformation behavior of Mg12YZn with 18R long-period stacking ordered structure10.1016/j.intermet.2009.07.014 ↗
43. Constitutive analysis of Mg-Al-Zn magnesium alloys during hot deformation10.1016/j.mechmat.2014.07.004 ↗
44. Flow behavior and microstructure of ZK60 magnesium alloy compressed at high strain rate10.1016/S1003-6326(14)63145-9 ↗
45. Characterization of hot deformation behavior of extruded ZK60 magnesium alloy using 3D processing maps10.1016/j.matdes.2013.11.037 ↗
46. Study of Hot Compression behavior of ZK60 magnesium alloy at elevated temperature
47. Deformation behavior, microstructure evolution and hot workability of Mg-3.7Gd-2.9Y-0.7Zn-0.7Zr alloy10.1007/s12540-017-6352-2 ↗
48. Effects of rare-earth elements Gd and Y on the solid solution strengthening of Mg alloys10.1016/j.jallcom.2009.02.131 ↗
49. Role of RE in the deformation and recrystallization of Mg alloy and a new alloy design concept for Mg–RE alloys10.1016/j.scriptamat.2014.12.010 ↗
50. Microstructure and mechanical properties of extruded Mg-Gd-Y-Zn-Zr alloys filled with intragranular LPSO phases10.1016/j.matchar.2017.11.027 ↗