journal article·2017-07Open access

Effect of tungsten concentration on microstructures of Co-10Ni-6Al-(0,2,4,6)W-6Ti (at%) cobalt-based superalloys

Peter J. Bocchini, Chantal K. Sudbrack, Daniel J. Sauza, Ronald D. Noebe, David N. Seidman, David C. Dunand

Abstract

Abstract The effects of reducing the W concentration (and concomitantly mass density) of Co-10Ni-6Al-xW-6Ti at% Co-based superalloys, with a γ(f.c.c.) plus γ′(L1 2 ) microstructure, is investigated for a series of alloys with W concentrations of 6 at% (baseline alloy), 4 and 2 at% (W-reduced) and 0 at% (W-free). The γ′(L1 2 ) solvus temperature decreases strongly (by 46 °C per 1 at% reduction in W), while the liquidus and solvus temperatures decrease mildly (3–5 °C per 1 at% W reduction) as measured by differential scanning calorimetry. Scanning electron microscopy was used to image phase formation in all alloys. When aging at 900 or 1000 °C for 256 h, the W reduction does not result in the appearance of additional phases within the grains beyond the γ(f.c.c.) and γ′(L1 2 ) phases present in the original alloy. Grain-boundary precipitates are present for all alloy compositions: W-rich or W-free precipitates after aging at 1000 °C, and coarsened γ′(L1 2 ) precipitates after aging at 900 °C. The composition of grain boundary precipitates were measured with energy-dispersive X-ray spectroscopy. Vickers microhardness values decrease with decreasing W content, due to a reduction in γ′(L1 2 ) precipitation and reduced solid-solution strengthening.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High Temperature Alloys and Creep · Advanced Materials Characterization Techniques · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Durand-Charre · 1997
2. Reed · 2006
3. Sims · 1987
4. Cobalt-base high-temperature alloys10.1126/science.1121738 ↗
5. Atom-probe tomographic study of γ/γ' interfaces and compositions in an aged Co-Al-W superalloy10.1016/j.scriptamat.2012.11.035 ↗
6. Alloying effects in polycrystalline γ′ strengthened Co–Al–W base alloys10.1016/j.intermet.2013.10.022 ↗
7. A new approach of designing superalloys for low density10.1007/s11837-010-0011-0 ↗
8. Nickel-based superalloys for advanced turbine engines: chemistry, microstructure, and properties10.2514/1.18239 ↗
9. Rene N6: third generation single crystal superalloy
10. Mechanical properties and lattice misfit of γ/γ′ strengthened Co-base superalloys in the Co–W–Al–Ti quaternary system10.1016/j.intermet.2014.07.006 ↗
11. Phase equilibria in the Co-rich Co-Al-W-Ti quaternary system10.1016/j.intermet.2011.08.004 ↗
12. Improved high temperature γ′ stability of Co–Al–W-base alloys containing Ti and Ta10.1016/j.matlet.2013.09.023 ↗
13. P.J. Bocchini, C.K. Sudbrack, D.J. Sauza, R.D. Noebe, D.N. Seidman, Effect of Ti Substitution of Al and W in Co-10Ni-9Al-9W (at%) Superalloys, (submitted for publication).
14. The effect of tungsten content on the properties of L12-hardened Co–Al–W alloys10.1016/j.jallcom.2015.01.031 ↗
15. Phase equilibria and microsctructure on γ′ phase in Co-Ni-Al-W system10.2320/matertrans.MER2008073 ↗
16. Effects of quaternary alloying elements on the γ′ solvus temperature of Co–Al–W based alloys with fcc/L12 two-phase microstructures10.1016/j.jallcom.2010.08.050 ↗
17. Russ · 1986
18. Murray · 1990
19. A revised thermodynamic description of the Co-W-C system10.1007/s11669-005-0133-1 ↗
20. Influence of ruthenium on microstructural evolution in a model CoAlW superalloy10.1016/j.actamat.2016.07.014 ↗
21. Alloying effects on heat-treated microstructure in Co-Al-W base superalloys at 1300 °C and 900 °C10.7449/2012/Superalloys_2012_813_821 ↗
22. High γ' solvus new generation nickel-based superalloys for single crystal turbine blade applications
23. Synthesis of a new tungsten-free γ–γ′ cobalt-based superalloy by tuning alloying additions10.1016/j.actamat.2014.11.016 ↗
24. A new tungsten-free γ–γ’ Co–Al–Mo–Nb-based superalloy10.1016/j.scriptamat.2014.11.009 ↗
25. Microstructural and creep properties of boron- and zirconium-containing cobalt-based superalloys10.1016/j.msea.2016.10.124 ↗
26. Partition behavior of alloying elements and phase transformation temperatures in Co-Al-W-base quaternary systems10.1016/j.intermet.2012.07.033 ↗
27. Creep strength and microstructure of polycrystalline γ′ – strengthened cobalt-base superalloys10.7449/2012/Superalloys_2012_695_703 ↗
28. Creep properties of different γ′-strengthened co-base superalloys10.1016/j.msea.2012.04.083 ↗
29. The importance of sign and magnitude of γ/γ′ lattice misfit in superalloys—with special reference to the new γ′-hardened cobalt-base superalloys10.1016/j.actamat.2014.08.005 ↗
30. Precipitate evolution and creep behavior of a W-free co-based superalloy10.1007/s11661-016-3775-1 ↗