journal article·2020-01

Fractographic features of technically pure magnesium, AZ31 and ZK60 alloys subjected to stress corrosion cracking

Evgeniy Merson, Vitaliy Poluyanov, Pavel Myagkikh, Dmitri Merson, Alexei Vinogradov

Publisher page

Abstract

Abstract Using quantitative fractography, the present study clarifies the effect of chemical composition and preliminary plastic deformation on the fracture mode of structural magnesium alloys experienced stress corrosion cracking (SCC). It is demonstrated that the fracture surfaces of alloys ZK60 and AZ31 failed during slow strain rate testing (SSRT) under SCC conditions are commonly featured by (i) the close-to-side surface region of typically brittle fracture initiation composing of intergranular and cleavage facets, which gradually transforms to (ii) the region of transgranular fluted facets optionally followed by the regions of (iii) fluted facets with secondary cracks, (iv) flat dimpled rapture and (v) slant dimpled rapture. Counterintuitively, the preliminary plastic strain introduced in air results in the increase of the fraction of the ductile mode on the fracture surface, elongation and stress at fracture of both alloys SSRT tested in corrosive media. The positive effect of pre-straining can be likely explained from the mechanistic viewpoint due to the increase of the yield stress, which has to be overcome to trigger plastic deformation needed to break the surface protective film. Features of the SCC mechanisms affecting the fracture surface appearance are quantified and discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Stress corrosion cracking (SCC) of magnesium alloys
2. Fractography of stress corrosion cracking of Mg-Al alloys10.1007/s11661-008-9475-8 ↗
3. Environmentally-induced cracking of magnesium10.1016/0010-938X(84)90017-9 ↗
4. Pitting-induced hydrogen embrittlement of magnesium-aluminium alloy10.1016/j.matdes.2012.06.007 ↗
5. Stress corrosion cracking of biodegradable Mg-4Zn alloy in simulated body fluid at different strain rates – a fractographic investigation10.1016/j.msea.2018.06.002 ↗
6. Hydrogen embrittlement of magnesium and magnesium alloys: a review10.1149/2.023304jes ↗
7. The transgranular SCC of a Mg-Al alloy: crystallographic, fractographic and acoustic-emission studies10.1007/BF02658523 ↗
8. Stress corrosion cracking and liquid metal embrittlement in pure magnesium10.5006/1.3583907 ↗
9. On the fractography of transgranular stress corrosion failures in a Mg-Al alloy10.5006/0010-9312-31.7.247 ↗
10. Hydrogen embrittlement in a Mg-Al alloy10.1007/BF02644454 ↗
11. Characterisation of stress corrosion cracking ( SCC ) of Mg – Al alloys10.1016/j.msea.2007.11.064 ↗
12. Stress corrosion cracking behavior of ZK60 magnesium alloy under different conditions10.1016/j.ijhydene.2017.08.161 ↗
13. Hydrogen-induced embrittlement of fine-grained twin-roll cast AZ31 in distilled water and NaCl solutions10.1007/s10853-015-9064-3 ↗
14. Hydrogen embrittlement understood10.1007/s11661-015-2836-1 ↗
15. Hydrogen embrittlement phenomena and mechanisms10.1515/corrrev-2012-0501 ↗
16. Environmentally assisted cracking: overview of evidence for an adsorption-induced localised-slip process10.1016/0001-6160(88)90113-7 ↗
17. Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials10.1016/j.actamat.2018.12.014 ↗
18. On the role of hydrogen in stress corrosion cracking of magnesium and its alloys: gas-analysis study10.1016/j.msea.2019.01.107 ↗
19. Microstructural origin of flutes and their use in distinguishing striationless fatigue cleavage from stress-corrosion crack- ing in titanium alloys
20. Environmentally-induced cracking of zirconium alloys - a review10.1016/0022-3115(90)90321-D ↗
21. Corrosion fatigue growth of zirconium in boiling nitric acid10.5006/1.3277645 ↗
22. Analysis of service stress corrosion cracking in a natural gas transmission pipeline, active or dormant?10.1016/j.engfailanal.2003.08.001 ↗
23. Initiation of stress corrosion cracking for pipeline steels in a carbonate-bicarbonate solution10.1007/BF02652362 ↗
24. Cyclic loading effects in the environment sensitive cracking of α-brass10.1016/0010-938X(91)90090-C ↗
25. A critical review of the Stress Corrosion Cracking (SCC) of magnesium alloys10.1002/adem.200500071 ↗
26. Characterisation of stress corrosion cracking ( SCC ) of Mg – Al alloys10.1016/j.msea.2007.11.064 ↗
27. Effect of grain size on the mechanisms of plastic deformation in wrought Mg-Zn-Zr alloy revealed by acoustic emission measurements10.1016/j.actamat.2012.12.024 ↗