Superplasticity in a multi-directionally forged Mg–Li–Zn alloy
Source abstract
Abstract
Abstract Superplastic behavior of the Mg–8Li–1Zn alloy, processed by extrusion at 573 K followed by multi-directional forging (MDF) at 423 K, was studied using shear punch testing (SPT) of miniature specimens at various temperatures and strain rates. Microstructural analysis indicated moderate grain refinement, reducing the gran size from 8 μm in the initial as-extruded condition to 4 μm after 8 passes of MDF. Processing by MDF not only refined the grain structure but also provided a more homogeneous microstructure and a larger fraction of high-angle grain boundaries. SPT was performed at shear strain rates in the range of 3.3 × 10−3–1.3 × 10−1 s−1 and temperatures in the range of 498–573 K. The strain rate sensitivity (SRS) index (m-value), obtained from the slope of the central region of the sigmoidal shear stress–shear strain rate curves, was as high as 0.51 for the MDF processed material at 548 K. This is in contrast to the as-extruded material that exhibited a linear behavior with a maximum m-value of only 0.29 at the same temperature. For the MDF processed material, the activation energy of 61 kJ mol−1, which is close to 67 kJ mol−1 for the grain boundary diffusion in β-Li, and the high m-value of 0.51 suggest that the prevailing deformation mechanism is grain boundary sliding (GBS) controlled by grain boundary diffusion.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Microstructure and mechanical properties · Metallurgy and Material Forming
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Magnesium: properties — applications — potential10.1016/S0921-5093(00)01351-4 ↗
2. Effect of temperature and grain size on the dominant diffusion process for superplastic flow in an AZ61 magnesium alloy10.1016/S1359-6454(99)00253-0 ↗
3. Polmear · 1989 · 170
4. Optimization of the microstructure for improving superplastic forming in magnesium alloys10.1016/j.msea.2007.02.088 ↗
5. Deformation and microstructure evolution of a high strain rate superplastic Mg–Li–Zn alloy10.1016/j.jallcom.2011.07.081 ↗
6. Enhanced superplasticity in equal-channel angularly pressed Sn–5Sb alloy10.1016/j.scriptamat.2010.11.030 ↗
7. Principles of grain refinement and superplastic flow in magnesium alloys processed by ECAP10.1016/j.msea.2008.09.058 ↗
8. An ultrafine-grained AZ31 magnesium alloy sheet with enhanced superplasticity prepared by accumulative roll bonding10.1016/S1006-706X(08)60073-4 ↗
9. Microstructural evolution and superplasticity in an Mg–Gd–Y–Zr alloy after processing by different SPD techniques10.1016/j.msea.2016.11.080 ↗
10. Microstructure and mechanical properties of multi-directionally forged Mg–Al–Zn alloy10.1016/j.scriptamat.2011.10.005 ↗
11. Evolution of microstructure, texture, and mechanical properties in a multi-directionally forged ZK60 Mg alloy10.1016/j.msea.2019.02.095 ↗
12. Superplasticity of fine-grained magnesium alloy AZ31 processed by multi-directional forging10.2320/matertrans.L-MRA2007839 ↗
13. Superplasticity in high temperature magnesium alloy WE4310.1016/j.msea.2016.12.129 ↗
14. Evolution of ultra-fine grains in AZ31 and AZ61 Mg alloys during multi directional forging and their properties10.2320/matertrans.MC200737 ↗
15. Low temperature superplasticity of ECAP processed Mg–10Li–1Zn alloy10.2320/matertrans.43.2419 ↗
16. Influence of preliminary extrusion conditions on the superplastic properties of a magnesium alloy processed by ECAP10.1016/j.actamat.2006.09.027 ↗
17. Superplastic deformatiom of a Mg–8% Li alloy processed at room temperature by ECAP10.4028/www.scientific.net/MSF.539-543.2940 ↗
18. Ultrafine-grained magnesium–lithium alloy processed by high-pressure torsion: low-temperature superplasticity and potential for hydroforming10.1016/j.msea.2015.05.103 ↗
19. Nayeb-Hashemi · 1998 · 184
20. Reviews on the influences of alloying elements on the microstructure and mechanical properties of Mg–Li base alloys
21. Superplasticity of a dual-phase-dominated Mg-Li-Al-Zn-Sr alloy processed by multidirectional forging and rolling10.1016/j.msea.2017.08.037 ↗
22. Shear punch superplasticity in equal-channel angularly pressed Mg–12Li–1Zn alloy10.1016/j.msea.2013.03.080 ↗
23. Superplasticity of a fine-grained Mg–9Gd–4Y–0.4Zr alloy evaluated using shear punch testing10.1016/j.jmrt.2014.04.004 ↗
24. Enhancement of superplasticity in a fine-grained Mg–3Gd–1Zn alloy processed by equal-channel angular pressing10.1016/j.msea.2015.08.074 ↗
25. Microstructure, texture, and superplasticity of a fine-grained Mg–Gd–Zr alloy processed by equal-channel angular pressing10.1007/s11661-016-3765-3 ↗
26. Evaluating high-temperature mechanical behavior of cast Mg–4Zn–xSb magnesium alloys by shear punch testing10.1016/j.msea.2010.03.007 ↗
27. Evaluation of mechanical properties using shear-punch testing10.1016/j.msea.2004.12.048 ↗
28. Dynamic and post-dynamic recrystallization under hot, cold and severe plastic deformation conditions10.1016/j.pmatsci.2013.09.002 ↗
29. Superplasticity—recent advances and future directions10.1016/0079-6425(89)90004-2 ↗
30. Superplasticity in a two-phase Mg–8Li–2Zn alloy processed by two-pass extrusion10.1016/j.msea.2011.04.073 ↗
31. Superplasticity in Mg–Li Zn alloys processed by high ratio extrusion10.1080/10426910701860954 ↗
32. Improving the superplastic properties of a two-phase Mg-8% Li alloy through processing by ECAP10.1016/j.msea.2005.08.143 ↗
33. A unified approach to grain boundary sliding in creep and superplasticity10.1016/0956-7151(94)90322-0 ↗
34. Superplastic behavior of a fine-grained two-phase Mg-9wt.%Li alloy10.1016/0921-5093(90)90169-4 ↗
35. Superplastic behavior of a fine grained Mg-9Li material at low homologous temperature10.1557/JMR.1992.2131 ↗