journal article·2020-08

Microstructure and mechanical behavior of as-built and heat-treated Ti–6Al–7Nb produced by laser powder bed fusion

Chao Xu, Fatih Sikan, Sila Ece Atabay, Jose Alberto Muñiz-Lerma, Oscar Sanchez-Mata, Xianglong Wang, Mathieu Brochu

Publisher page

Abstract

Abstract Ti–6Al–4V and Ti–6Al–7Nb were manufactured with laser powder bed fusion (LPBF). Microstructural comparison study between Ti–6Al–4V and Ti6Al–6Nb was used to understand processability similarities between two different titanium alloys. Quantitative similarities between two alloys revealed that Ti–6Al–4V processing parameters can be used for optimization of Ti–6Al–7Nb. The microstructure, processing, properties relationship and the influence of heat treatments were investigated for Ti–6Al–7Nb. The as-built microstructure was composed of a columnar prior β grains with fine acicular α′ martensite resulting in a yield strength of 1082 MPa and an ultimate tensile strength of 1160 MPa with an elongation of 9.7%. Solutionizing at 1055 °C and aging at 540 °C completely transformed the columnar structure of the prior β grains to equiaxed via phase transformation and grain growth, solutionized the α’ martensite into β and then created a fine lamellar α + β structure with air cooling. The resultant microstructure had reduced strength and hardness but increased ductility. The reduction in yield (871 MPa) and ultimate tensile (940 MPa) strength would be positive to minimize stress shielding of orthopedic implants. The improved elongation of 11.5% meets the requirements for biomedical applications which stipulates an elongation of at least 10% according to the ISO 5832-3 Standard.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Additive manufacturing: technology, applications and research needs10.1007/s11465-013-0248-8 ↗
2. Additive manufacturing of tissues and organs10.1016/j.progpolymsci.2011.11.007 ↗
3. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
4. Heat treatment of Ti‐6Al‐7Nb components produced by selective laser melting10.1108/13552540810907974 ↗
5. Tilton · 2018 · 21
6. Selective laser melting of biocompatible metals for rapid manufacturing of medical parts10.1108/13552540710776142 ↗
7. Mechanical biocompatibilities of titanium alloys for biomedical applications10.1016/j.jmbbm.2007.07.001 ↗
8. Wear properties of Ti and Ti–6Al–7Nb castings for dental prostheses10.1016/S0142-9612(02)00533-1 ↗
9. Structural, mechanical and in vitro characterization of individually structured Ti–6Al–4V produced by direct laser forming10.1016/j.biomaterials.2005.07.041 ↗
10. Corrosion behaviour of Ti–6Al–7Nb and Ti–6Al–4V ELI alloys in the simulated body fluid solution by electrochemical impedance spectroscopy10.1016/j.electacta.2006.06.018 ↗
11. The influence of niobium and vanadium on passivity of titanium-based implants in physiological solution10.1016/S0142-9612(03)00252-7 ↗
12. Biomedical applications of titanium and its alloys
13. Titanium alloys for biomedical applications10.1016/j.msec.2005.08.032 ↗
14. In vitro corrosion behaviour of titanium alloys without vanadium10.1016/S0013-4686(01)00860-X ↗
15. Microstructure and mechanical behaviour of Ti―6Al―7Nb alloy produced by selective laser melting10.1016/j.matchar.2011.03.006 ↗
16. Lütjering · 2007
17. Christoph · 2003
18. MICROSTRUCTURE AND MECHANICAL PROPERTIES OF HEAT TREATED Ti-6Al-7Nb ALLOY
19. Effect of scanning strategies on residual stress and mechanical properties of Selective Laser Melted Ti6Al4V10.1016/j.msea.2017.11.103 ↗
20. Phase transformations during cooling in alpha+beta titanium alloys10.1016/S0921-5093(97)00802-2 ↗
21. Microstructural optimization through heat treatment for enhancing the fracture toughness and fatigue crack growth resistance of selective laser melted Ti 6Al 4V alloy10.1016/j.actamat.2019.03.003 ↗
22. Surface modification of titanium, titanium alloys, and related materials for biomedical applications10.1016/j.mser.2004.11.001 ↗
23. Microstructure and Mechanical Properties of Heat Treated Ti-6Al-7Nb Alloy, Processing, Properties, and Design of Advanced Ceramics and Composites II.
24. Fabrication of microscaffolds from Ti-6Al-7Nb alloy by SLM10.1108/RPJ-10-2013-0101 ↗
25. Rheological behavior of β-Ti and NiTi powders produced by atomization for SLM production of open porous orthopedic implants10.1016/j.powtec.2015.05.015 ↗
26. Microstructure-properties relationships of Ti-6Al-4V parts fabricated by selective laser melting10.1007/s40684-018-0062-1 ↗
27. The effect of heat treatment on microstructure evolution and tensile properties of selective laser melted Ti6Al4V alloy10.1016/j.jallcom.2018.12.051 ↗
28. Effect of heat treatment on the phase transformation and mechanical properties of Ti6Al4V fabricated by selective laser melting10.1016/j.jallcom.2018.06.076 ↗
29. Formation and control of martensite in Ti-6Al-4V alloy produced by selective laser melting10.1016/j.matdes.2016.06.117 ↗
30. Titanium-based biomaterials for preventing stress shielding between implant devices and bone
31. Fully porous 3D printed titanium femoral stem to reduce stress‐shielding following total hip arthroplasty10.1002/jor.23445 ↗
32. Gum metal and related alloys
33. Influence of processing on microstructure and mechanical properties of (α+ β) titanium alloys10.1016/S0921-5093(97)00778-8 ↗
34. Effect of Nb addition on microstructure, mechanical properties and castability of β-type Ti–Mo alloys10.1016/S1003-6326(15)63834-1 ↗
35. Effect of Nb on the microstructure, mechanical properties, corrosion behavior, and cytotoxicity of Ti-Nb alloys10.3390/ma8095287 ↗
36. Cavitation erosion of austenitic stainless steel and effect of boron and nitrogen ion implantation10.1016/0001-6160(89)90104-1 ↗