journal article·2020-11

Creep failure of a solution-annealed 15-15Ti steel exposed to stagnant lead-bismuth eutectic at 550 and 600 °C

Xing Gong, Zhibin Yang, Yangbin Deng, Jun Xiao, Hao Wang, Zhiyang Yu, Yuan Yin

Publisher page

Abstract

Abstract Uniaxial creep-to-rupture tests at 550 and 600 °C under a constant load of 300 MPa have been performed to study the effect of lead-bismuth eutectic (LBE) on the creep failure behavior of a solution-annealed 15-15Ti steel. The results show that the secondary creep rate of the steel tested in LBE at 550 and 600 °C is 56 and 6 times higher than that tested in air at the same temperatures, respectively. The transition time from the primary creep to the secondary creep is largely shortened by LBE. As a consequence, the creep life of 15-15Ti in contact with LBE is reduced remarkably. The severe degradation of the creep performance is attributed to uniform dissolution corrosion (elemental leaching) and especially localized intergranular cracking.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Nuclear reactor physics and engineering · Fusion materials and technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Swelling and irradiation creep of neutron-irradiated 316Ti and 15-15Ti steels
2. Creep behaviour of 15-15Ti (Si) austenitic steel in air and in liquid lead at 550 oC
3. Thermal creep properties of Ti-stabilized DIN 1.4970 (15-15Ti) austenitic stainless steel pressurized cladding tubes10.1016/j.jnucmat.2017.06.013 ↗
4. Long-term corrosion of austenitic steels in flowing LBE at 400oC and 10-7 mass% dissolved oxygen in comparison with 450 and 550oC10.1016/j.jnucmat.2015.09.027 ↗
5. Corrosion behavior of austenitic steels 1.4970, 316L and 1.4571 in flowing LBE at 450 and 550oC with 10-7 mass% dissolved oxygen10.1016/j.jnucmat.2014.08.024 ↗
6. Transmission electron microscopy study of complex oxide scales on DIN 1.4970 steel exposed to liquid Pb-Bi eutectic10.1016/j.corsci.2018.10.018 ↗
7. Opportunities for the LWR ATF materials development program to contribute to the LBE-cooled ADS materials qualification program10.1016/j.jnucmat.2016.10.012 ↗
8. 2015
9. Influence of liquid lead and lead-bismuth eutectic on tensile, fatigue and creep properties of ferritic/martensitic and austenitic steels for transmutation systems10.1016/j.jnucmat.2011.04.047 ↗
10. Liquid Pb-Bi embrittlement effects on the T91 steel after different heat treatments10.1016/j.jnucmat.2008.02.050 ↗
11. Slow strain rate tensile tests on T91 in static lead-bismuth eutectic10.1016/j.jnucmat.2006.05.039 ↗
12. Influence of LBE long term exposure and simultaneous fast neutron irradiation on the mechanical properties of T91 and 316L10.1016/j.jnucmat.2016.02.008 ↗
13. Low cycle fatigue behavior of a modified 9Cr-1Mo ferritic-martensitic steel in lead-bismuth eutectic at 350°C - effects of oxygen concentration in the liquid metal and strain rate10.1016/j.corsci.2015.02.022 ↗
14. Low cycle fatigue behaviour of T91 martensitic steel at 300°C in air and in liquid lead bismuth eutectic10.1016/j.ijfatigue.2005.11.003 ↗
15. Characteristics and liquid metal embrittlement of the steel T91 in contact with lead–bismuth eutectic10.1016/j.jnucmat.2015.08.048 ↗
16. Creep-to-rupture tests of T91 steel in flowing Pb-Bi eutectic melt at 550 °C10.1016/j.jnucmat.2009.08.013 ↗
17. The role of oxide films in preventing liquid metal embrittlement of T91 steel exposed to liquid lead-bismuth eutectic10.1016/j.jnucmat.2018.07.018 ↗
18. Temperature dependence of liquid metal embrittlement susceptibility of a modified 9Cr-1Mo steel under low cycle fatigue in lead-bismuth eutectic at 160 to 450°C10.1016/j.jnucmat.2015.06.021 ↗
19. Initiation of LME crack in ferritic martensitic steel in liquid lead-bismuth10.1016/j.jnucmat.2018.09.033 ↗
20. Liquid metal embrittlement sensitivity of the T91 steel in lead, in bismuth and in lead-bismuth eutectic
21. Stability of fatigue cracks at 350°C in air and in liquid metal in T91 martensitic steel10.1016/j.ijfatigue.2019.105265 ↗
22. Kinetics and mechanism of crack initiation of liquid metal embrittlement
23. Environmentally assisted cracking of T91 ferritic-martensitic steel in heavy liquid metals10.1515/corrrev-2019-0035 ↗
24. Study of crack initiation of 15-15Ti austenitic steel in liquid PbBi
25. Multiscale investigation of crack path and microstructural changes during liquid metal embrittlement of 304L austenitic steel in liquid sodium10.1016/j.corsci.2017.08.009 ↗
26. Dissolution corrosion of 316L austenitic stainless steels in contact with static liquid lead-bismuth eutectic (LBE) at 500°C10.1016/j.jnucmat.2017.04.004 ↗
27. Metallurgical analysis of a tube ruptured in the lead bismuth corrosion test facility10.1080/18811248.2006.9711079 ↗
28. Behavior of steels in flowing liquid PbBi eutectic alloy at 420–600°C after 4000–7200h10.1016/j.jnucmat.2004.07.010 ↗
29. Selective leaching of nickel and chromium from Type 316 austenitic steel in oxygen-containing lead–bismuth eutectic (LBE)10.1016/j.corsci.2014.03.016 ↗
30. Orientation relationship of the austenite-to-ferrite transformation in austenitic stainless steels due to dissolution corrosion in contact with liquid Pb-Bi eutectic10.1016/j.scriptamat.2019.03.035 ↗
31. Corrosion scales on various steels after exposure to liquid lead–bismuth eutectic10.1016/j.jnucmat.2013.09.034 ↗
32. Performance of 9% Cr steels in flowing lead-bismuth eutectic at 450 and 550oC, and 10-6 mass% dissolved oxygen10.1016/j.nucengdes.2014.01.023 ↗
33. Corrosion behavior of austenitic steels in liquid lead bismuth containing 10−6 wt% and 10−8 wt% oxygen at 400–500°C10.1016/j.jnucmat.2014.01.046 ↗
34. Corrosion interaction of 9%Cr ferritic/martensitic steels at 450 and 550 °C with flowing Pb–Bi eutectic containing 10−7 mass % dissolved oxygen
35. Corrosion in iron and steel T91 caused by flowing lead–bismuth eutectic at 400 °C and 10−7 mass% dissolved oxygen
36. Creep, creep-rupture tests of Al-surface-alloyed T91 steel in liquid lead bismuth at 500 and 550°C10.1016/j.jnucmat.2011.11.027 ↗
37. Steel T91 subjected to static stress in lead-bismuth eutectic at 450–550°C and low oxygen concentration10.1016/j.jnucmat.2018.09.056 ↗
38. Liquid metal embrittlement susceptibility of a high-entropy alloy exposed to oxygen-depleted liquid lead-bismuth eutectic at 250 and 350°C10.1016/j.jnucmat.2019.151859 ↗
39. Comparison of solid metal-metal oxide reference electrodes for potentiometric oxygen sensors in liquid lead-bismuth eutectic operating at low temperature ranges10.1016/j.snb.2015.03.004 ↗
40. Schroer · 2007
41. Microstructure evolution and interfacial properties in the Fe–Pb system10.1016/S1359-6454(02)00129-5 ↗
42. Review of the studies on fundamental issues in LBE corrosion10.1016/j.jnucmat.2007.06.019 ↗
43. Corrosion behavior of cold-worked austenitic stainless steels in liquid lead–bismuth eutectic10.1016/j.jnucmat.2014.02.006 ↗
44. Liquid metal embrittlement of an Fe10Cr4Al ferritic alloy exposed to oxygen-depleted and -saturated lead-bismuth eutectic at 350°C10.1016/j.corsci.2019.108364 ↗