Microstructure evolution and mechanical properties of 308L stainless steel coatings fabricated by laser hot wire cladding
Source abstract
Abstract
Abstract Laser hot wire cladding (LHWC) technology has been proved to be a very efficient laser cladding manufacturing process due to its advantages of fast deposition rate, high material utilization rate, and less environmental pollution. In this study, LHWC technology was used to prepare multiple layers of 308L stainless steel coatings on ordinary mild carbon steel substrates. The microstructure of the weldment section was evaluated by optical microscopy (OM). The results showed that the heat-affected zone (HAZ) of the sample was small, with a height of 1.58 mm and an area of 14.28 mm2. The metallurgical bonding between the substrate and coating was good. Because of the temperature gradient and grain growth rate, the grain morphologies in the different coating regions were different. From the bottom to the top, the grain morphologies were planar crystals, columnar dendrites, and equiaxed grains. Electron backscatter diffraction (EBSD) was used to obtain crystallographic information on the entire section of the sample. The interior of the cladding layer was mainly composed of columnar grains growing along the structural direction, most of which were coarse grains. The matrix and the HAZ consisted of fine equiaxed grains, and the crystal orientations were randomly distributed without obviously preferred orientations. Hardness analysis performed that the hardness of the HAZ was the highest, and the matrix had the lowest hardness. The hardness was higher in the layer-to-layer fusion zone and then gradually decreased with an increase in the cladding height inside each layer. The tensile test results illustrated that the elongation of the cladding layer (44.8 %) was higher than that of the HAZ (32.1 %) and the matrix (20.4 %) because the tensile direction of the tensile sample in the cladding layer was parallel to the laser scanning direction, which improved the tensile performance. The average grain size of the HAZ was the smallest, owing to the effect of fine grain strengthening, and the tensile strength was the highest(585 MPa). According to the tensile fracture profile, the sample matrix, HAZ, and the cladding layer exhibited ductile fractures.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Progress in joining of advanced materials10.1179/imr.1998.43.1.1 ↗
2. Erosion wear behavior of laser clad surfaces of low carbon austenitic steel10.1016/j.wear.2008.12.043 ↗
3. Microstructure and properties of laser cladding FeCrBSi composite powder coatings with higher Cr content10.1016/j.jmatprotec.2013.12.009 ↗
4. Selective laser melting of stainless steel 316L with low porosity and high build rates10.1016/j.matdes.2016.05.035 ↗
5. Corrosion behavior of the S136 mold steel fabricated by selective laser melting, Chinese
6. An overview of residual stresses in metal powder bed fusion
7. Wire + Arc additive manufacturing10.1179/1743284715Y.0000000073 ↗
8. Microstructure and mechanical properties of hot wire laser clad layers for repairing precipitation hardening martensitic stainless steel10.1016/j.optlastec.2015.07.014 ↗
9. Deposition of Ti-6Al-4V using laser and wire, part I: microstructural properties of single beads10.1016/j.surfcoat.2011.07.095 ↗
10. Laser cladding of Inconel 625 wire for corrosion protection10.1016/j.jmatprotec.2014.10.024 ↗
11. Real-time monitoring of laser hot-wire cladding of Inconel 62510.1016/j.optlastec.2014.03.007 ↗
12. Formation quality optimization of laser hot wire cladding for repairing martensite precipitation hardening stainless steel10.1016/j.optlastec.2014.07.017 ↗
13. Developments in laser-based surface engineering processes: with particular reference to protection against cavitation erosion10.1016/j.surfcoat.2016.02.019 ↗
14. Morphologies, microstructures, and mechanical properties of samples produced using laser metal deposition with 316 L stainless steel wire10.1016/j.optlaseng.2017.02.008 ↗
15. Microstructure and mechanical properties of 308L stainless steel fabricated by laminar plasma additive manufacturing10.1016/j.msea.2019.138523 ↗
16. Microstructure evolution and mechanical properties of multiple-layer laser cladding coating of 308L stainless steel10.1016/j.apsusc.2015.02.171 ↗
17. Laser hot-wire cladding of Co-Cr-W metal cored wire10.1016/j.optlaseng.2019.105998 ↗
18. Comparison of laser cladding with powder and hot and cold wire techniques
19. Wear and corrosion resistant laser coatings for hydraulic piston rods10.2351/1.4914503 ↗
20. Competitive failure analysis on tensile fracture of laser-deposited material for martensitic stainless steel10.1016/j.matdes.2017.01.014 ↗
21. Characterization of microstructure of A508III/309L/308L weld and oxide films formed in deaerated high-temperature water10.1016/j.jnucmat.2017.10.030 ↗
22. Microstructural characterization of an SA508–309L/308L–316L domestic dissimilar metal welded safe-end joint10.1016/j.matchar.2014.08.023 ↗
23. Repair of 304 stainless steel by laser cladding with 316L stainless steel powders followed by laser surface alloying with WC powders10.1016/j.jmapro.2016.08.004 ↗
24. Investigation on in-situ laser cladding coating of the 304 stainless steel in water environment10.1016/j.jmatprotec.2020.116949 ↗
25. Effects of process time interval and heat treatment on the mechanical and microstructural properties of direct laser deposited 316L stainless steel10.1016/j.msea.2015.07.056 ↗
26. Study on microstructure, mechanical properties and machinability of efficiently additive manufactured AISI 316L stainless steel by high-power direct laser deposition10.1016/j.jmatprotec.2016.09.005 ↗
27. Properties of a dissimilar friction stir weld between austenitic stainless steel and low carbon steel10.1016/j.jmst.2013.02.008 ↗
28. On the characterization procedure to quantify the contribution of microstructure on mechanical properties in intercritically deformed low carbon HSLA steels10.1016/j.msea.2020.139800 ↗
29. Effect of scanning speed on the microstructure and mechanical behavior of 316L stainless steel fabricated by selective laser melting10.1016/j.matdes.2019.108355 ↗
30. Kou · 2003 · 431
31. Lippold · 2005 · 376
32. Improved weldability diagram for pulsed laser welded austenitic stainless steels10.1179/136217103225008847 ↗
33. Microstructure evolution and EBSD analysis of a graded steel fabricated by laser additive manufacturing10.1016/j.vacuum.2017.03.021 ↗