Abstract In this study, selective laser melting (SLM) of Ti–15Mo alloy was systematically investigated, especially in its densification, microstructure and mechanical properties. At low scanning speed, the formation of spherical holes are mainly due to gas porosity brought about by residual gases. At high scanning speed, the lack of fusion (LOF) defects are presented because of the insufficient energy density, which is very detrimental to the ductility. Owing to the difference of the temperature gradient, the transition from the cellular crystals to equiaxed crystals has been observed in XY plane while the XZ plane are mainly consist of columnar crystals which are radiating along the edge of the molten pool. As a result of the retention of a reasonable level of ω phase, high dislocation density, finer grains, the twinning-induced plasticity (TWIP) and the changes of texture orientation, the Ti–15Mo samples processed by the SLM achieve a greater combination of high tensile strength of 840.41 MPa and a high elongation of 32.37%, which are higher than those reported so far. The twins become denser and thicker with increasing strain, and the average of twin widths with various strains were calculated to 7 μm at strain of 10%, 4 μm at strain of 15% and 2 μm at strain of 20%.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. Ti based biomaterials, the ultimate choice for orthopaedic implants - a review10.1016/j.pmatsci.2008.06.004 ↗
2. Experiment study on fracture fixation with low rigidity titanium alloy: plate fixation of tibia fracture model in rabbit10.1007/s10856-008-3372-y ↗
3. Effects of oxygen concentration and phase stability on nano-domain structure and thermal expansion behavior of Ti-Nb-Zr-Ta-O alloys10.1016/j.actamat.2015.08.054 ↗
4. Preparation and characterization of Ti-15Mo alloy used as biomaterial10.1590/S1516-14392011005000013 ↗
5. Laser powder bed fusion of Ti15Mo10.1016/j.rineng.2020.100155 ↗
6. Mechanism of twinning-induced plasticity in β-type Ti–15Mo alloy10.1016/j.scriptamat.2013.05.027 ↗
7. In-situ investigation of phase transformations in ultra-fine grained Ti15Mo alloy10.1016/j.jallcom.2021.159027 ↗
8. Microstructure evolution in solution treated Ti15Mo alloy processed by high pressure torsion10.1016/j.matchar.2014.10.024 ↗
9. Preparation of bulk Ti 15Mo alloy using cryogenic milling and spark plasma sintering10.1016/j.matchar.2020.110762 ↗
10. Microstructure and mechanical behaviour of Ti―6Al―7Nb alloy produced by selective laser melting10.1016/j.matchar.2011.03.006 ↗
11. Densification, microstructure evolution and fatigue behavior of Ti-13Nb-13Zr alloy processed by selective laser melting10.1016/j.powtec.2018.09.073 ↗
12. Manufacture by selective laser melting and mechanical behavior of a biomedical Ti-24Nb-4Zr-8Sn alloy10.1016/j.scriptamat.2011.03.024 ↗
13. Densification behavior, microstructure evolution, and wear performance of selective laser melting processed commercially pure titanium10.1016/j.actamat.2012.04.006 ↗
14. A study of the microstructural evolution during selective laser melting of Ti–6Al–4V10.1016/j.actamat.2010.02.004 ↗
15. Archimedes revisited: a faster, better, cheaper method of accurately measuring the volume of small objects10.1088/0031-9120/40/5/008 ↗
16. Direct energy deposition - laser additive manufacturing of titanium - molybdenum alloy: parametric studies, microstructure and mechanical properties10.1016/j.jallcom.2019.02.121 ↗
17. Thermal and stress modeling of multi-material laser processing10.1016/S1359-6454(01)00312-3 ↗
18. Study on shrinkage behaviour of direct laser sintering metallic powder10.1243/095440505X32995 ↗
19. Finite element analysis of the effect of volume shrinkage during laser densification10.1016/j.actamat.2005.06.014 ↗
20. Influence of processing parameters on the evolution of melt pool, porosity, and microstructures in Ti-6Al-4V alloy parts fabricated by selective laser melting10.1007/s40964-017-0030-2 ↗
21. Fatigue life of additively manufactured Ti–6Al–4V in the very high cycle fatigue regime10.1016/j.ijfatigue.2016.05.018 ↗
22. Effects of powders and process parameters on density and hardness of A357 aluminum alloy fabricated by selective laser melting10.1007/s00170-019-04641-x ↗
23. On direct laser deposited Hastelloy X: dimension, surface finish, microstructure and mechanical properties10.1179/026708309X12578491814591 ↗
24. Gradient microstructures and mechanical properties of Ti-6Al-4V/Zn composite prepared by friction stir processing10.3390/ma12172795 ↗
25. In situ X-ray analysis of mechanism of nonlinear super elastic behavior of Ti–Nb–Ta–Zr system beta-type titanium alloy for biomedical applications10.1016/j.msec.2007.04.028 ↗
26. Origin of ω-phase formation in metastable β-type Ti-Mo alloys: cluster structure and stacking fault
27. ω-Assisted refinement of α phase and its effect on the tensile properties of a near β titanium alloy10.1016/j.jmst.2019.10.031 ↗
28. The formation of omega phase in titanium and zirconium alloys: a review10.1007/BF00550217 ↗
29. Selective electron beam melting of Ti–48Al–2Nb–2Cr: microstructure and aluminium loss10.1016/j.intermet.2014.01.004 ↗
30. Microstructure and deformation behavior of Ti-6Al-4V alloy by high-power laser solid forming10.1016/j.actamat.2017.04.026 ↗
31. Anisotropic mechanical behavior of biomedical Ti-13Nb-13Zr alloy manufactured by selective laser melting10.1016/j.jallcom.2018.05.179 ↗
32. 316L stainless steel with gradient porosity fabricated by selective laser melting10.1007/s11665-009-9535-2 ↗
33. Selective laser melting of W-Ni-Cu composite powder: densification, microstructure evolution and nano-crystalline formation10.1016/j.ijrmhm.2017.09.004 ↗
34. Crystallographic texture control of beta-type Ti–15Mo–5Zr–3Al alloy by selective laser melting for the development of novel implants with a biocompatible low Young's modulus10.1016/j.scriptamat.2016.12.038 ↗
35. Selective laser melting of pure tantalum: Densification, microstructure and mechanical behaviors10.1016/j.msea.2017.09.083 ↗
36. As-fabricated and heat-treated microstructures of the Ti-6Al-4V alloy processed by selective laser melting10.1007/s11661-011-0731-y ↗
37. Correlation between porosity and processing parameters in TiAl6V4 produced by selective laser melting10.1016/j.matdes.2016.05.070 ↗
38. Defects in additive manufactured metals and their effect on fatigue performance: a state-of-the-art review
39. Direct energy deposition - laser additive manufacturing of titanium-molybdenum alloy: parametric studies, microstructure and mechanical properties10.1016/j.jallcom.2019.02.121 ↗
40. Beta type Ti-Mo alloys with changeable Young's modulus for spinal fixation applications10.1016/j.actbio.2012.02.004 ↗
41. Effects of Mo contents on the microstructure, properties and cytocompatibility of the microwave sintered porous Ti-Mo alloys10.1016/j.msec.2018.12.028 ↗
42. Relationship between texture development and deformation twinning activity in Ti-15Mo alloy10.1016/j.msea.2018.04.050 ↗
43. Effects of α phase precipitation on crevice corrosion and tensile strength in Ti-15Mo alloy10.1016/j.msea.2009.10.033 ↗
44. Precipitation behavior of Ti15Mo alloy and effects on microstructure and mechanical performance10.1007/s11665-019-04456-7 ↗
45. The origin of high-density dislocations in additively manufactured metals10.1080/21663831.2020.1751739 ↗
46. Strengthening strategy for a ductile metastable β-titanium alloy using low-temperature aging10.1080/21663831.2017.1350211 ↗
47. Significant contribution of stacking faults to the strain hardening behavior of Cu-15%Al alloy with different grain sizes10.1038/srep16707 ↗
48. Effect of β (110) texture intensity on α-variant selection and microstructure morphology during β→α phase transformation in near α titanium alloy10.1016/j.actamat.2016.12.069 ↗
49. A turn-on Schiff-base fluorescence sensor for Fe3+ ion10.1016/j.inoche.2013.10.004 ↗
50. Transition of multi-deformation modes in Ti-10Mo alloy with oxygen addition10.1016/j.msea.2013.10.010 ↗
51. Deformation twinning in high-nitrogen austenitic stainless steel10.1016/j.actamat.2007.02.023 ↗
52. Mechanism of twinning-induced plasticity in β-type Ti-15Mo alloy10.1016/j.scriptamat.2013.05.027 ↗
53. Ω phase Acts as a switch between dislocation channeling and joint twinning- and transformation-induced plasticity in a metastable Β titanium alloy10.1016/j.actamat.2018.03.053 ↗
54. Grain size effect on strain hardening in twinning-induced plasticity steels10.1016/j.scriptamat.2012.01.037 ↗